Alloy Digest (1963) 12 (8): SA-152.
Published: 01 August 1963
... Carpenter SIL No. 1 is a hardenable silicon-chromium alloy steel that is used in applications where the operating temperatures are below 1000 F. It is widely used for intake valves and for exhaust valve stems in internal combustion engines. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1967) 16 (12): Cu-183.
Published: 01 December 1967
... EVERDUR-637 is a high-strength, corrosion resistant copper alloy containing silicon and aluminum. It is also characterized by its good forging and machining qualities. It is recommended for fasteners, valve stems, marine hardware, cable connectors, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1995) 44 (6): Cu-601.
Published: 01 June 1995
... HIDURON alloy 191 was developed for marine applications where both a combination of strength and good corrosion/ impingement resistance is needed. It finds applications in shafts, fasteners and valve stems. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1996) 45 (4): Ni-339.
Published: 01 April 1996
... Nimonic alloy 901 is a nickel-base alloy strengthened by additions of molybdenum, titanium, and aluminum. It possesses high creep and rupture strength from 1000 to 1400 deg F. Applications include components for gas turbines, bolting, and valve stems for power applications. This datasheet provides...
Journal Articles
Alloy Digest (1979) 28 (9): Cu-379.
Published: 01 September 1979
.... Among its many applications are valve stems, gears, rivets and threaded connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1979) 28 (11): Cu-384.
Published: 01 November 1979
.... Its many uses include automotive clutch disks, shafting and valve stems and bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1980) 29 (4): Cu-393.
Published: 01 April 1980
... properties. Typical applications include valve stems, threaded connectors and flare fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1979) 28 (1): Cu-365.
Published: 01 January 1979
... to corrosion. Its numerous applications include cams, valve stems and marine hardware. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1979) 28 (6): Cu-375.
Published: 01 June 1979
... are desired. Typical applications are valve stems, gears and flare fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1980) 29 (7): Cu-398.
Published: 01 July 1980
... MUELLER Alloy 3530 (formerly MBCo. Alloy 254) is a high-leaded brass noted for its excellent thread-rolling and knurling properties; it has a machinability rating approaching that of free-cutting brass. Typical applications include adapters, gears and valve stems. This datasheet provides...
Journal Articles
Alloy Digest (1981) 30 (3): Cu-414.
Published: 01 March 1981
... elasticity hardness heat treatability joinability machinability marine hardware nuts physical properties propeller shafts shear strength tensile properties valve stems workability wrought brass UNS C46400 Copper Alloy No. C46400 Filing Code: Cu414 Copper Alloy MARCH 1981 - DATA ON WORLD WIDE...
Journal Articles
Alloy Digest (1965) 14 (5): Cu-151.
Published: 01 May 1965
... LAVIN NDZ-S BRONZE is a copper-base alloy recommended as a high-strength dezincification and dealuminization resistant valve stem material in water supply systems. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1970) 19 (3): Cu-212.
Published: 01 March 1970
... MUELLER 6162 is a general purpose alloy for use where high strength and corrosion resistance are necessary, but where high hardness is not a factor. It is recommended for fasteners, bearings, valve stems, gears and pole line hardware. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1962) 11 (2): Cu-113.
Published: 01 February 1962
... NDZ-BRONZE is a copper-base alloy recommended as a high-strength dezincification and dealuminization resistant valve stem material in water supply systems. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1983) 32 (1): Cu-452.
Published: 01 January 1983
... ANACONDA Alloy 482 is a variation of the basic Naval Brass composition; it contains a small amount of lead (nominally 0.70%) to improve its machinability. It has good mechanical properties and high resistance to corrosion by seawater. It is used for marine hardware, valve stems and other machined...
Journal Articles
Alloy Digest (1986) 35 (2): Cu-506.
Published: 01 February 1986
... for numerous applications such as bearings, gears, impellers and valve stems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1985) 34 (3): SS-459.
Published: 01 March 1985
... particularly for automatic screw-machine operations where the longer tool life results in more productive machine time. Among its many uses are fittings, gears, shafts and valve stems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1985) 34 (8): Cu-453.
Published: 01 August 1985
... copper-zinc (yellow brass) alloy. Typical uses are marine fittings, valve stems, lever arms and light-duty gears. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1985) 34 (7): Cu-499.
Published: 01 July 1985
... uses are valve stems, moderate-duty gears and marine components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (1975) 24 (8): Cu-300.
Published: 01 August 1975
... or shock loads. Its anti-galling characteristics make it an excellent slow-speed, heavy load-bearing material for service against steel. Its applications include valve stems, gears, shafts and marine hardware. Composition: Physical Constants: (Approximate) Copper Iron Aluminum Manganese zinc Nominal 64.0...