Alloy Digest (1976) 25 (11): Ni-236.
Published: 01 November 1976
... is derived from the presence of hard nickel borides (and to a lesser extent chromium carbides) tightly held in a tough nickel-rich matrix. Among its many uses are cylinder liners, glass plant applications and valve components for nuclear applications. This datasheet provides information on...
Journal Articles
Alloy Digest (1978) 27 (12): Cu-364.
Published: 01 December 1978
... MUELLER Alloy 6970 (formerly MBCo. alloy 804) is a wrought alloy having excellent corrosion resistance when used with water and steam. It has good mechanical properties, excellent wear resistance and good machinability. These properties make it an ideal material for valve components. This...
Journal Articles
Alloy Digest (1993) 42 (9): SS-550.
Published: 01 September 1993
..., bushings, valve components, cutlery and pump parts. Designers may also consider Type 440C vacuum are remelted (VAR) for aerospace and small precision bearings. In these applications improved cleanliness, superior fatigue properties, high strength and corrosion resistance are critical design considerations...
Journal Articles
Alloy Digest (1999) 48 (9): Al-361.
Published: 01 September 1999
... Kaiser Aluminum alloy 6262 (Tennalum alloy 6262) is an Al-Mg-Si-Cu-Cr-Pb-Bi alloy with characteristic good machinability and corrosion resistance and a good acceptance of coatings (anodize response). It is typically used in automotive parts, fittings, building hardware, and valve components. This...
Journal Articles
Alloy Digest (1977) 26 (3): SS-337.
Published: 01 March 1977
... Carpenter 430FR Solenoid Quality stainless steel is a ferritic chromium-iron alloy developed especially for A.C. and D.C. magnetic circuit applications such as solenoid valve core components and electromagnetic relay cores. The electrical resistivity of 430FR is approximately 25% higher than other...
Journal Articles
Alloy Digest (1966) 15 (5): TS-179.
Published: 01 May 1966
... Carpenter V.S.M. is a molybdenum, chromium steel which offers good resistance to heat checking, provides high hot hardness and good resistance to wear and abrasion at elevated temperatures. It is recommended for valve and bearing components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1966) 15 (8): SS-185.
Published: 01 August 1966
... ENDURO S-1 is a chromium type stainless steel providing high strength, toughness and resistance to impact when heat treated. It shows resistance to wet and dry corrosion. It is recommended for steam turbine parts, valves, cutlery, pump components, etc. This datasheet provides information on...
Journal Articles
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
... AISI No. 616 is a hardenable martensitic type stainless steel recommended for high temperature applications up to 1200 F. It is used for steam turbine blades and buckets, valves, jet engine components, and high temperature bolting. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1968) 17 (10): Co-56.
Published: 01 October 1968
... HOWMET No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. It is recommended for bushings, scrapers, valve parts, and other machinery components. This datasheet provides information on...
Journal Articles
Alloy Digest (1985) 34 (1): SS-457.
Published: 01 January 1985
... (nearly equal to AISI Type 304 stainless steel) and its high degree of resistance to stress-corrosion cracking, it is used in a variety of environments. Typical uses are aircraft structural components, shafts, valve parts and fittings. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1985) 34 (7): Cu-499.
Published: 01 July 1985
... uses are valve stems, moderate-duty gears and marine components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (1985) 34 (8): Al-259.
Published: 01 August 1985
... valves, aerospace components, gears, fittings and washing machine agitators. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing...
Journal Articles
Alloy Digest (1985) 34 (9): Al-260.
Published: 01 September 1985
... include aircraft and aerospace components, gears, machinery parts, manifolds, valves and fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating...
Journal Articles
Alloy Digest (1987) 36 (2): Al-277.
Published: 01 February 1987
... many uses include aircraft components, gears, machinery parts, fittings, valves and ornamental products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1976) 25 (10): Cu-320.
Published: 01 October 1976
... Copper Alloy No. 875 is a copper-base casting alloy for applications requiring a combination of high strength and good resistance to corrosion. It cannot be hardened or strengthened by heat treatment. Its many applications include valve parts, small propellers, gears and marine components. This...
Journal Articles
Alloy Digest (1977) 26 (9): Cu-340.
Published: 01 September 1977
...-resistant alloys elasticity fatigue properties fracture toughness hardenability hardness heat treatability joinability machinability physical properties plastic molds pump components tensile properties valves BELMONT ALLOY 4977 Filing Code: cu-340 Copper Alloy SEPTEMBER 1977 - DATA ON WORLD...
Journal Articles
Alloy Digest (1978) 27 (1): SS-346.
Published: 01 January 1978
... ductility plus a higher degree of forgeability. Its wide range of uses include valve parts, engine parts and aircraft components; it is especially useful where high transverse strength and toughness are required. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... properties. It has good castability, excellent machinability and high resistance to corrosion. TERNALLOY 7 has many uses including aircraft components, gears machinery parts, fittings, valves and ornamental products. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1988) 37 (3): Zn-42.
Published: 01 March 1988
... uses include hardware, valves, implement components and equipment for liquid fuel transfer because it is non-sparking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also...
Journal Articles
Alloy Digest (1982) 31 (9): Cu-444.
Published: 01 September 1982
... designated Ampco D-4HT. It is suited for service up to 750 F. Typical applications include aerospace components, marine hardware, valve seats, glands and stuffing box nuts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...