1-20 of 148 Search Results for

valve bodies

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1997) 46 (6): SS-409.
Published: 01 June 1997
... operations where longer tool life results in more productive machining time. Applications include shafts, valve bodies, valves, valve trim, and fittings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1955) 4 (10): CI-12.
Published: 01 October 1955
... MEEHANITE GE is a medium strength iron having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, pump bodies, valve bodies, steam cylinders, cylinder...
Journal Articles
Alloy Digest (1980) 29 (10): Cu-404.
Published: 01 October 1980
... uses include valve bodies, putters and hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1998) 47 (11): SS-724.
Published: 01 November 1998
... Type CG6MMN is a 22Cr-12.5Ni-5Mn-2.25Mo alloy that is the cast equivalent of Nitronic 50 (see Alloy Digest SS-304, revised April 1990). The alloy is used as castings for pump and valve bodies to resist a wide variety of environments that corrode type 316 (CF8M). This datasheet provides information...
Journal Articles
Alloy Digest (1999) 48 (1): Al-357.
Published: 01 January 1999
... Kaiser Aluminum Alloy 2024 has good machinability and good mechanical properties. The alloy is typically used in aircraft structures, rivets, connectors, hydraulic valve bodies, and miscellaneous structural applications. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (6): SS-225.
Published: 01 June 1969
... Duraloy CB 30 is a cast chromium steel having good corrosion resistance. It cannot be hardened by heat treatment. It is recommended for food processing and oil services at high temperatures, valve bodies, impellers and heat treating equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1965) 14 (7): SS-171.
Published: 01 July 1965
... Type CC-50 is an iron-chromium casting alloy having high corrosion resistance. It is recommended for furnace equipment, valve bodies and for extremely corrosive sulfur-bearing atmospheres. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1968) 17 (8): Zn-11.
Published: 01 August 1968
... ILZRO-14 is a zinc-base die casting alloy developed with superior creep resistance at both ambient and elevated temperatures. It is recommended for carburetors, fuel pumps, valve bodies, etc. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1962) 11 (2): Cu-113.
Published: 01 February 1962
...: NDZ is a bronze alloy combining corrosion resistance (including resistance to dezinci- fication and dealuminization) with high tensile strength, unusually high yield strength, good elongation, good electrical conductivity and fair machinability. Forms Avoilable: Applications: Valve stems, valve bodies...
Journal Articles
Alloy Digest (1979) 28 (11): Cu-384.
Published: 01 November 1979
.... Its many uses include automotive clutch disks, shafting and valve stems and bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1980) 29 (12): Cu-408.
Published: 01 December 1980
... AMPCOLOY 521 is a cast copper-nickel alloy with excellent resistance to many highly active corrosives, particularly saline waters and sulfuric and phosphoric acids. It has high strength and good ductility and can be welded readily. Its many applications include valves, pump bodies, steam fittings...
Journal Articles
Alloy Digest (1976) 25 (9): Cu-319.
Published: 01 September 1976
... industries. It is used in the as-cast condition without further heat treatment, except that stress relieving is optional after heavy machining. Forms Available: Castings and ingots. Applications: Parts that must resist corrosion by seawater, such parts comprise valves, pump bodies, flanges and elbows...
Journal Articles
Alloy Digest (1963) 12 (8): Cu-132.
Published: 01 August 1963
... OUNCE Metal, also known as Composition Metal, is a cast 5% leaded bronze recommended for bearings, valves and pump bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1970) 19 (7): SS-241.
Published: 01 July 1970
... chip. Standard drill machinability tests were performed on Yz in. hot rolled and annealed bar product. The results indicate that Uniloy 326 machines comparably to non-free-machining austenitic stainless grades. It is particularly adaptable for pressure valves, valve bodies, the paper pulp industry...
Journal Articles
Alloy Digest (1965) 14 (5): Cu-151.
Published: 01 May 1965
... and dealuminization)with high tensile strength, unusually high yield strength, good elongation, good electrical conductivity and fair machinability. Forms Available: Sand castings and ingots. Applications: Valve stems, valve bodies, valve bonnets, propeller whee Is, marine and other corrosive uses, electrical parts...
Journal Articles
Alloy Digest (1978) 27 (12): Cu-364.
Published: 01 December 1978
... is not recommended. Forms Available: Rod and screw-machine products. Applications: Valve stems. gate stems, valve bodies and valve com- ponents for potable water systems,steam systems, sewage treatment plants, selected chemical plant systems and other applications where corrosion is a problem. Manufacturer: Mueller...
Journal Articles
Alloy Digest (2013) 62 (6): Cu-820.
Published: 01 June 2013
... capability, and the scrap is completely recyclable with C36000, C37700, and other conventional alloys. DOI: 10.31399/asm.ad.cu0820 Products Available Rounds and hexagons from 6.350 to 76.200 mm (0.250 3.000 in Applications: Applications include: drinking water fixtures and fittings, forged valves and valve...
Journal Articles
Alloy Digest (1965) 14 (11): Cu-157.
Published: 01 November 1965
..., bolts, fasteners, faucet handles, plumbing fixtures, stop-cocks, valve bodies. Manufacturer: Noranda Copper Mills, Ltd. Montreal, Quebec, Canada ...
Journal Articles
Alloy Digest (2019) 68 (10): Cu-898.
Published: 01 October 2019
... connectors. Typical fastener uses include stripped nuts. Marine uses include covers for marine hardware, marine equipment. Typical industrial uses include welding jaws, pickling hooks, high-strength clamps, valve bodies, pickling baskets, bearing segment for the steel industry, large hold down screws...
Journal Articles
Alloy Digest (2016) 65 (8): Cu-849.
Published: 01 August 2016
...: Applications include: drinking water fixtures and fittings, forged valves and valve bodies, PEX plumbing applications and systems, products requiring AB1953 compliance, and products requiring dezincification characteristics. Producer: Mueller Brass Co. Port Huron, MI 48060, USA Tel: (810) 987-7770 Fax: (810...