Alloy Digest (1994) 43 (11): SS-575.
Published: 01 November 1994
... SANDVIK 3R69 is a nitrogen-alloyed, high-strength variant of AISI 316L, used predominantly in the urea industry. The steel has guaranteed maximum ferrite content of 0.6%. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1995) 44 (5): SS-593.
Published: 01 May 1995
... Sandvik 3R60 is an austenitic stainless steel, a highly purity variant of AISI Type 316L for the urea industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high...
Journal Articles
Alloy Digest (1997) 46 (2): SS-671.
Published: 01 February 1997
... Sandvik Safurex is a high alloy duplex (austenitic-ferritic) stainless steel primarily developed to withstand the corrosive environments present in the urea industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1989) 38 (4): SS-504.
Published: 01 April 1989
... SANDVIK 2RE69 is a fully austenitic stainless steel with extra low carbon and impurity levels. It was developed primarily to cope with severe corrosive conditions existing in the urea industry. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1998) 47 (1): SS-705.
Published: 01 January 1998
... to ASTM A 262 Practice E. Both OOCr25Ni6Mo2N and OCr25Ni6Mo3CuN steels are serviceable in ammonium carbamate liquor used in the urea industry. Results from the Huey test (Stamicarbon 53961 B Standard) are given in Table 7 and show a good resistance intergranular corrosion. Corrosion Fatigue. Duplex...
Journal Articles
Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
... and 317L stainless steels. Its many uses include marine scrubbers, desalination equipment, sulfuric acid production, wet phosphoric acid production, mild sour gas wells, urea production and pulp and paper industry. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
... 304, 316, and 317L stainless steels. Its many uses include marine scrubbers, desalination equipment, sulfuric acid production, wet phosphoric acid production, mild sour gas wells, urea production, and applications in the pulp and paper industry. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1998) 47 (2): SS-706.
Published: 01 February 1998
... type 316. Type OCr25Ni6Mo3CuN has good resistance to wear and erosion corrosion in ammonium carbamate liquor from the urea industry and to handling solutions containing chlorides. In addition, du- plex stainless steels are characterixed by high mechanical strength as well as good weldability. Table 4...
Journal Articles
Alloy Digest (1979) 28 (1): SS-360.
Published: 01 January 1979
... for handling caustic, organic acids, nitric acid, bleach sdutions, urea and chloride-containing cooling waters. *ALLEGHENY LUDLUM and E-BRITE 26-1 are registered trademarks of AlIegheny Ludlum Industries, Inc. (Data shown are typicaL Do not use for specification or final design.) Composition: Physical...
Journal Articles
Alloy Digest (2012) 61 (12): SS-1129.
Published: 01 December 2012
... utilization of this alloy is for fasteners and actuators in the following industrial applications: Chemical process industry sulfuric acid production, nitric acid processes, polythionic acid resistance, urea production, equipment handling organic and fatty acids Marine industry and shipbuilding pumps...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1198.
Published: 01 January 2015
... to 12,000 mm (472 in.) Applications: Typical applications occur in the oil and gas industry including sour gas applications, pulp and paper industry, chemical industry, acetic acid distillation towers, urea production, phosphoric acid plants, sulfuric acid processes, pollution control equipment, truck...
Journal Articles
Alloy Digest (1994) 43 (4): SS-565.
Published: 01 April 1994
... type steels (activation pH: 0 at 70°C). Stress Corrosion: Due to its higher nickel content, UR B6 is more resistant to stress-corrosion cracking than other austen- itic steels, and has proven to be safe inmany industrial media. Dilute Chloride Solutions: Laboratory tests carried out in an autoclave...
Journal Articles
Alloy Digest (1997) 46 (3): SS-675.
Published: 01 March 1997
... is intergranular amosion resistant, even in the welded state when under continu- ous operating conditions up to 400°C. This steel is widely used in the chemical industry, in the production of urea, in the manufac- ture of synthetic fibers. in the cellulose industry, and in textile finishing. The molybdenum content...
Journal Articles
Alloy Digest (2015) 64 (3): SS-1204.
Published: 01 March 2015
... industry; acetic acid distillation towers; urea production; phosphoric acid plants; sulfuric acid processes; pollution control equipment; truck lorries; and chemical tankers. Producer: In USA: Industeel USA, LLC Coatesville, PA 19320, USA Tel: (610) 383-3000 Fax: (610) 383-3007 www.industeel.info...
Journal Articles
Alloy Digest (1996) 45 (9): SS-653.
Published: 01 September 1996
...-Loire Industrie. Composition(a), wt (Non) carbon 0.020 Chromium 22 Nickel 5.3 Molybdenum 3 Nitrogen 0.16 sulfur a.002 (a) PREN = Cr% + 3.3mo%] + 16 [N%] 2 33 (or 34) Physical Properties: Density, g/cm3 (lb/in3) Thermal fzxpansion Resistivity Thermal conductivity specificheat Modulus Tensile Properties...
Journal Articles
Alloy Digest (1999) 48 (8): SS-758.
Published: 01 August 1999
... industry, sour gas applications, pulp and paper industry, digesters, chemical industry reactor vessels, acetic acid distillation towers, urea production, phosphoric acid plant reactors, sulfuric acid processes, hydrometallurgy, pollution control equipment, trucks, lorries, chemical tankers Producer...
Journal Articles
Alloy Digest (2014) 63 (11): SS-1192.
Published: 01 November 2014
...: Typical applications include sea water pumps, propeller shafts, cables, and guy lines; urea synthesis, pumps, valves, bolts, exchanger tubes in the chemical industry; nuclear fuel recycling; offshore drilling, filters, perforated casings, and petrochemicals in the oil industry; and in paper manufacturing...
Journal Articles
Alloy Digest (2023) 72 (9): Ni-786.
Published: 01 September 2023
... 33 is a material that can be used for many applications in the chemical processing industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1994) 43 (5): SS-566.
Published: 01 May 1994
... and paper environments and urea. It is also suc- cessful in wet scrubbing systems. Manufacturer: Creusot-Loire Industrie. France Creusot-Mane1 Inc., Wayne. PA, 19087 215-254-9900 ...
Journal Articles
Alloy Digest (2020) 69 (9): Ti-170.
Published: 01 September 2020
... and the jewelry industry. Formability CP titanium grades have good hot and cold formability. Their capability for forming increases with decreasing content of interstitials, especially oxygen. Materials cold worked more than 5% need to be soft annealed to obtain the specified mechanical properties and optimum...