1-20 of 240 Search Results for

trucks

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2014) 63 (2): CS-179.
Published: 01 February 2014
... Swebor 450 (hardness 450 HBW) is a high-strength steel with good wear resistant qualities. It is used in applications where demands on wear resistance are high. These include loader buckets, mining truck bodies, wearing parts of agricultural machines, wearing parts of mining machines, waste...
Journal Articles
Alloy Digest (2011) 60 (9): SA-634.
Published: 01 September 2011
... as dump truck bodies. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-634. Producer or source...
Journal Articles
Alloy Digest (2011) 60 (11): SA-636.
Published: 01 November 2011
... Dillidur 400V is a wear-resistant steel with surface hardness at room temperature of 370–430 HB. The steel is easy to weld, bend, and machine. Because of its high wear resistance and good welding performance, 400V is used in the production of agricultural machinery and industrial truck systems...
Journal Articles
Alloy Digest (1977) 26 (11): CS-69.
Published: 01 November 1977
... suited to the automotive, farm and construction equipment, and appliance industries for such applications as truck bodies, light poles, bumper support members and parts for agricultural implements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1977) 26 (12): Ni-252.
Published: 01 December 1977
... PYROMET 31 is a nickel-base superalloy that exhibits an unusual combination of corrosion resistance and strength to temperatures as high as 1500 F (816 C). It has excellent resistance to hot sulfidation attack such as could occur in truck and locomotive diesel valve service. This datasheet...
Journal Articles
Alloy Digest (2011) 60 (4): SA-624.
Published: 01 April 2011
... FORA 450 is a wear resistant steel with a minimum HB hardness of 450. This water quenched martensitic steel is used in truck bodies. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on wear resistance as well as forming, machining...
Journal Articles
Alloy Digest (1968) 17 (5): SA-226.
Published: 01 May 1968
... JLX-50CC is a high-strength columbium steel designed for ease of fabrication. It has good formability, weldability, and toughness. It is recommended for mining equipment, automobile and truck bodies, trailers and similar construction. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2009) 58 (2): SA-592.
Published: 01 February 2009
..., including truck chassis and crane booms. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-592. Producer or source: SSAB Swedish...
Journal Articles
Alloy Digest (2009) 58 (3): SA-594.
Published: 01 March 2009
..., including truck chassis, crane booms, and earthmoving machines. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fatigue. It also includes information on forming, heat treating, and joining. Filing Code: SA-594. Producer or source...
Journal Articles
Alloy Digest (2009) 58 (4): SA-598.
Published: 01 April 2009
... Domex 600MC is a hot-rolled, extra high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-10.00 mm. The alloy meets or exceeds the requirements of S600MC in EN 10149-2. Applications include truck chassis, crane booms, and earthmoving machines...
Journal Articles
Alloy Digest (1994) 43 (5): SA-475.
Published: 01 May 1994
... LUKENS HARDWARE 400F steel was developed from armor steel production technology to have as low a carbon equivalent as possible, consistent with meeting both surface and through-thickness hardness. Uses include truck body liners, bucket lips and conveyor troughs. This datasheet provides information...
Journal Articles
Alloy Digest (1994) 43 (6): SA-476.
Published: 01 June 1994
... LUKENS HARDWEAR 500F steel was developed from armor steel production technology to have as low a carbon equivalent as possible, consistent with meeting both surface and through-thickness hardness. Uses include truck body liners, bucket lips and conveyor troughs. This datasheet provides information...
Journal Articles
Alloy Digest (1979) 28 (5): SA-359.
Published: 01 May 1979
... of a fully killed, low-carbon, vacuum-degassed, columbium-alloyed steel. This special composition and processing practice minimize harmful nonmetallic inclusions that hamper formability. Typical applications include automotive reinforcements, truck parts and construction components. This datasheet provides...
Journal Articles
Alloy Digest (1964) 13 (8): CS-21.
Published: 01 August 1964
... JLX-W is a columbium-bearing carbon steel produced in four grades according to the minimum yield point. It has good forming characteristics and excellent weldability. It is recommended where high strength and weight saving are required, such as freight cars, trucks, storage tanks, etc...
Journal Articles
Alloy Digest (1965) 14 (11): SA-186.
Published: 01 November 1965
... Allegheny Metal AM-363 is a low-cost maraging, stainless, structural alloy steel. It is recommended for structural framework in railroad cars and truck bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1970) 19 (3): Mg-68.
Published: 01 March 1970
... DOMAL AZ21X is a readily extrudable magnesium alloy used where moderate strength requirements will suffice. It does not respond to an age-hardening heat treatment. It is recommended for structural members, truck bodies and paneling. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1998) 47 (2): Ni-536.
Published: 01 February 1998
... Pyromet 31V is a sulfidation resistant, precipitation hardenable superalloy with unusual combination of corrosion resistance and strength to 816 C (1500 F). It has excellent resistance to hot sulfidation attack and has been used in truck and locomotive diesel valve service. This datasheet provides...
Journal Articles
Alloy Digest (1998) 47 (5): SA-496.
Published: 01 May 1998
... Inland DuraSpring is a high-strength microalloyed spring steel for use in high stress coil springs for automobile and light truck suspension systems. This bar product offers significant improvements in tensile strength, fatigue properties, and fracture toughness compared to conventional spring...
Journal Articles
Alloy Digest (1984) 33 (9): Ni-303.
Published: 01 September 1984
... of application is brazing turbine blades in truck engines where high strength at high temperatures is required. This datasheet provides information on composition, physical properties, and microstructure. It also includes information on forming, heat treating, and joining. Filing Code: Ni-303. Producer or source...
Journal Articles
Alloy Digest (1966) 15 (8): SA-199.
Published: 01 August 1966
... AW-TEN is a high-strength structural steel offering 50,000 psi minimum yield strength, good formability and weldability, and superior corrosion resistance. It is intended primarily for weight reduction and longer service life. It is recommended for automobile and truck bodies, buildings, bridges...