Alloy Digest (1974) 23 (8): Al-58.
Published: 01 August 1974
... ALUMINUM 2017 is an age-hardenable wrought alloy of medium strength and ductility. Its service temperature is below 212 F. It is used for general engineering applications, such as transportation equipment, machine parts and fittings. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1977) 26 (6): SA-334.
Published: 01 June 1977
... AISI 5147 is a low-chromium (nominally 1% chromium), intermediate-hardenability alloy steel for medium-duty applications. It is normally hardened by quenching in oil. It has a wide range of applications for transportation equipment, farm implements, tools and industrial machinery. This datasheet...
Journal Articles
Alloy Digest (1995) 44 (11): SS-623.
Published: 01 November 1995
... REMANIT 4310 is one of the lowest alloyed austenitic stainless steels and has lower Cr and Ni for more work hardening. It is used in conveying materials and for lightweight high strength transportation equipment. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1978) 27 (5): SA-346.
Published: 01 May 1978
... from 40,000 to 80,000 psi. They are used widely in the transportation and mobile-equipment industries. See also Ispat Inland Cal Hi-Form 80Y100T, Alloy Digest CS-136, May 2003. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1982) 31 (7): SS-411.
Published: 01 July 1982
.... Cronifer 2328 is used widely in the chemical industry for equipment and for the storage and transportation of various acids and solutions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1968) 17 (7): SA-228.
Published: 01 July 1968
... CREUSOT-9D6 is a weldable 9% nickel steel recommended for low temperature applications such as storage and transportation tanks, liquified gas equipment, and cryogenic structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1996) 45 (12): SS-663.
Published: 01 December 1996
... Armco 409 Ni is a fine-grain stainless steel developed for applications more than 0.120 in. thick needing an alloy superior to Type 409 stainless steels in weld formability and toughness. Applications include coal-handling equipment, transportation containers, mixers, liners, exhaust flanges, heat...
Journal Articles
Alloy Digest (2013) 62 (1): Al-440.
Published: 01 January 2013
... 4 (0.2) 8 (0.3) 980 (39) 2200 (87)(a) 800 (32) 15000 (591) (a) Wider than 2200 mm (87 in.) sheets may be supplied upon request Applications: Transportation equipment, particularly in tipper trailers Producer: Alcoa Europe SA European Mill Products CH-1202 Geneva, Switzerland Tel: +41-22-919-60-00...
Journal Articles
Alloy Digest (1958) 7 (8): SA-74.
Published: 01 August 1958
...-uctural carbon steel by using this grade of steel. Yoloy s provides substantial savings in weight to the transportation industty and can be safely used because of its high corrosion resistance. It is furnished with lower mechanical properties and es&lent ductility for easy fabrication. After fabrication...
Journal Articles
Alloy Digest (1966) 15 (7): SA-198.
Published: 01 July 1966
.... Applications: Bridges, transportation equipment including marine, railway and highway, buildings and general constructional use. Particularly advantageous where high strength for thick sections is required arid als 0 when exposed unpainted exterior structures are contemplated. Manufacturer: The Steel Company...
Journal Articles
Alloy Digest (1962) 11 (1): SA-123.
Published: 01 January 1962
... Strength No. 2 gives the same excellent corrosion resistance found in other high strength low alloy steels. This grade has been very well received by manufacturers of all types of transportation equipment where the combination of formability, corrosion resistance, and elevated mechanical proper- ties...
Journal Articles
Alloy Digest (2019) 68 (6): Sa-846.
Published: 01 June 2019
... reduction in section thickness without loss of structural integrity. Forms Available Plate, thickness from 5 30 mm (0.24 1.18 in Applications Typical applications include: transport equipment such as low loaders; high-rise buildings (columns and beams); columns for low- and high-rise buildings; transfer...
Journal Articles
Alloy Digest (2007) 56 (10): SS-1000.
Published: 01 October 2007
..., and other bulk transport equipment where there is a need for a good combination of corrosion resistance, strength, toughness, and ease of fabrication. Producer: Allegheny Ludlum An Allegheny Technologies Company Pittsburgh, PA (800) 289-7528 ISSN: 002-614X SS-1000B ...
Journal Articles
Alloy Digest (2019) 68 (4): SA-842.
Published: 01 April 2019
... of Bisplate are able to be drilled, countersunk, and tapped. In all cases, suitable high-powered and rigid drill equipment should be used. When drilling the Bisalloy structural steel grades, the use of cobalt-type high-speed drills is recommended. Drills equipped with replaceable carbide inserts can also...
Journal Articles
Alloy Digest (2019) 68 (3): SA-840.
Published: 01 March 2019
..., thickness from 5 500 mm (0.20 20 in.) Applications This material offers advantages in many structural applications, including transport equipment such as trays, low loaders, and trailer outriggers; storage tanks of water oil and gas; columns for low- and high-rise building; transfer beams for low- and high...
Journal Articles
Alloy Digest (1956) 5 (7): SA-45.
Published: 01 July 1956
..., spindles, shafts and pinions. Transportation equipment such as drive shafts, motor gears and sruds. di8erential and uansmkion gears, jack shafrs and connecting rod bolts. Exavating and road machinery such as ditch digger teeth, shafts, gears and acerpillar treads. Cement mill equipment, logging toob, mine...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1042.
Published: 01 August 2009
... and hot rolled, according to thickness Applications Applications are the classic construction, transport equipment, and industrial equipment arenas where a better performance is needed when moderately corrosive environments exist. Producer: Arcelor Stainless Processing LLC Sterling Heights, MI 48312...
Journal Articles
Alloy Digest (2003) 52 (11): SA-524.
Published: 01 November 2003
... reduction in gross design weight because smaller cross sections can be specified provided suitable design and fabrication prac- tices are followed. The grades are also used in tower and building members, components for earthmoving or transport equipment, booms, dippersticks, bucket parts for power shovels...
Journal Articles
Alloy Digest (2020) 69 (9): Al-468.
Published: 01 September 2020
...) for a plate or sheet thickness (t) of Temper 0.4 mm 0.8 mm 1.6 mm 3.2 mm 4.8 mm 6.0 mm 10 mm 12 mm O 0.5t 1t 1t 1t 1.5t 1.5t H321 1.5t 1.5t 2t 2.5t (a) The minimum bend radius will depend on the type of bending equipment, and on the tooling and its condition. (b) Bending edge transverse to rolling...
Journal Articles
Alloy Digest (2022) 71 (5): SS-1347.
Published: 01 May 2022
... equipment, and other bulk transport equipment where there is a need for a good combination of corrosion resistance, strength, toughness, and ease of fabrication. Supplier ATI 1000 Six PPG Place Pittsburgh, Pennsylvania 15222, USA Tel: +1 800 289 7454 Web: www.atimetals.com Consult ATI 201LN, ATI, 2014...