Alloy Digest (2021) 70 (3): SS-1332.
Published: 01 March 2021
... plus good mechanical properties and corrosion resistance, it has been used in a wide variety of consumer and transportation applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (2022) 71 (4): SS-1346.
Published: 01 April 2022
... plus good mechanical properties and corrosion resistance, it has been used in a wide variety of consumer and transportation applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (2002) 51 (9): SS-861.
Published: 01 September 2002
... strengths to be achieved by rolling with a lower loss of ductility than with Type 302. The high-strength properties of Type 301 make it ideally suited to structural and transportation applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... cryogenic components die applications dimensional stability laser components liquefied natural gas production physical properties SANDMEYER SSC INVAR 36 tensile properties thermal expansion transportation application workability UNS K93603 DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2012...
Journal Articles
Alloy Digest (1996) 45 (12): SS-663.
Published: 01 December 1996
... Armco 409 Ni is a fine-grain stainless steel developed for applications more than 0.120 in. thick needing an alloy superior to Type 409 stainless steels in weld formability and toughness. Applications include coal-handling equipment, transportation containers, mixers, liners, exhaust flanges, heat...
Journal Articles
Alloy Digest (2013) 62 (1): Al-440.
Published: 01 January 2013
... that was originally developed to withstand the extreme rigors of maritime applications. Drawing on the experience of freight transport applications, exhaustive testing in the lab and in the field proved its performance characteristics to be uniquely suited to tipper trailer sides and floors. The characteristics can...
Journal Articles
Alloy Digest (2018) 67 (2): SS-1278.
Published: 01 February 2018
... strength with a good formability result on a very high lightweight construction potential. This lightweight potential, as well as its excellent CO2 footprint, make the grade ideal for a wide range of transportation (e.g., truck, bus, railway vehicles) but mainly automotive applications as an alternative...
Journal Articles
Alloy Digest (1977) 26 (6): SA-334.
Published: 01 June 1977
... AISI 5147 is a low-chromium (nominally 1% chromium), intermediate-hardenability alloy steel for medium-duty applications. It is normally hardened by quenching in oil. It has a wide range of applications for transportation equipment, farm implements, tools and industrial machinery. This datasheet...
Journal Articles
Alloy Digest (1991) 40 (10): Cp-19.
Published: 01 October 1991
... Refractory Sheet Type 100 is an engineered ceramic, fiber reinforced structural alumina composite with useful properties in thermal, structural and electrical insulation applications; as well as the transport of molten nonferrous metals to 1260 C (2300 F). This datasheet provides information...
Journal Articles
Alloy Digest (1974) 23 (8): Al-58.
Published: 01 August 1974
... ALUMINUM 2017 is an age-hardenable wrought alloy of medium strength and ductility. Its service temperature is below 212 F. It is used for general engineering applications, such as transportation equipment, machine parts and fittings. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1968) 17 (7): SA-228.
Published: 01 July 1968
... CREUSOT-9D6 is a weldable 9% nickel steel recommended for low temperature applications such as storage and transportation tanks, liquified gas equipment, and cryogenic structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2005) 54 (2): SA-546.
Published: 01 February 2005
... Docol 450 Wear is an ultra-high strength steel that is used for many wear application in transportation and construction products. This datasheet provides information on composition, physical properties, microstructure, hardness, tensile properties, and bend strength. It also includes information...
Journal Articles
Alloy Digest (1996) 45 (8): SS-651.
Published: 01 August 1996
... Remainit 4318, similar to type 301LN, is in the family of lowest-alloyed austenitic stainless steels. This type has the highest rate of work hardening. Typical applications include the transportation industry and conveyor belts for food processing. This datasheet provides information...
Journal Articles
Alloy Digest (2000) 49 (10): Al-373.
Published: 01 October 2000
...-hardenable high-strength version of alloy 2024 (see Alloy Digest Al-23 and Al-346). The 2324-T39 alloy is used where higher strength, toughness, and good resistance to fatigue-crack propagation are needed. A typical application is the lower wing skin of commercial transport aircraft. Chemical Composition, wt...
Journal Articles
Alloy Digest (1998) 47 (11): Al-355.
Published: 01 November 1998
... Kaiser Aluminum alloy 2017 has good machinability and good mechanical properties. It is used in rivets. General structural applications, and transportation. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue...
Journal Articles
Alloy Digest (1978) 27 (5): SA-346.
Published: 01 May 1978
... corrosion-resistant alloys elasticity heat treatability INLAND HI-FORM joinability machinability mobile equipment industries physical properties tensile properties transportation application workability An INLAND HI-FORM Filing Code: SA-346 Steel-Alloy MAY 1976 EUI - DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (1985) 34 (8): SA-411.
Published: 01 August 1985
... properties temper embrittlement tensile properties transportation application workability UNS G40320 H40320 AIS1 4032 Filing Code: SA-411 Steel-Alloy AUGUST 1985 - DATA ON WORLD WIDE METALS AND ALLOYS Puhlrshrd hr Alloy Dlgesr. Inc. 17 Canfield Street Orange. Ne\c Jerse!, 07050 (201) 761-1090 AISI...
Journal Articles
Alloy Digest (2002) 51 (7): Al-379.
Published: 01 July 2002
.../32 in Applications: Transportation applications include chemical tankers for strength and corrosion resistance and to weld 5254 to 5254. Container applications include the chemical storage of hydrogen peroxide for corrosion resistance and strength and to weld 5254 to 5254 Producer: AlcoTec Wire...
Journal Articles
Alloy Digest (1982) 31 (7): SS-411.
Published: 01 July 1982
... International® 1996 1996 ASM International chemical application chemical composition corrosion-resistant alloys corrosivity CRONIFER 2328 elasticity fracture toughness hardness heat treatability joinability machinability physical properties tensile properties transportation application...
Journal Articles
Alloy Digest (2002) 51 (5): Al-377.
Published: 01 May 2002
... to 5454. Transportation applications include line heaters and steam lines for strength and high temperature welding 5454 to 5454. Producer: AlcoTec Wire Corporation Traverse City, MI 49686-9263 (231) 941-4111 (231) 941-9154 (fax) ISSN: 002-614X Al-377B Fig. 1 Typical shear strength, longitudinal fillet...