Alloy Digest (2008) 57 (8): SA-583.
Published: 01 August 2008
... Ovako 157 is a case-hardened steel in three versions for bearing and transmission applications. This datasheet provides information on composition and hardness. It also includes information on casting, forming, and heat treating. Filing Code: SA-583. Producer or source: Ovako North America Inc...
Journal Articles
Alloy Digest (2009) 58 (4): SA-596.
Published: 01 April 2009
... OvaX 800 is a through-hardening steel for bearing and transmission applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on casting, forming, and machining. Filing Code: SA...
Journal Articles
Alloy Digest (1980) 29 (3): Al-181.
Published: 01 March 1980
... ALUMINUM 6070 is a high-strength, heat-treatable extrusion alloy. It was developed for structural applications. It has high resistance to general corrosion and stress-corrosion cracking. Its many applications include marine hardware, electric-transmission towers and bridges. This datasheet...
Journal Articles
Alloy Digest (2009) 58 (7): SA-604.
Published: 01 July 2009
... hardness heat treatability isotropic properties OVAX 600 tensile properties workability OVAX 600 (Through-Hardening and Bearing Steel) OvaX 600 is a through-hardening steel for bearing and transmission applications. Chemical Composition, wt Nominal composition Bearing composition Carbon 0.63 0.70...
Journal Articles
Alloy Digest (1985) 34 (5): CS-106.
Published: 01 May 1985
... for structural shapes and carburized parts. Among its many applications are bushings. clutch discs, flanges, thrust washers. tinplate. nails. rivets. automobile bodies and fenders. pans and transmission covers. Composition: Carbon Manganese Phosphorus Sulfur Silicon Iron 0.08-o. I3 0.30-0.60 0.040 max. 0.050 max...
Journal Articles
Alloy Digest (2005) 54 (12): SA-553.
Published: 01 December 2005
... levels up to 69 HRC, promoting high wear and contact fatigue life. It has a U.S. Patent. Ferrium C69 is designed to reduce the weight of an aerospace gearbox by as much as 50% with application primarily in high power-density transmission systems. Laboratory scale tests have demonstrated the performance...
Journal Articles
Alloy Digest (1987) 36 (11): Cu-530.
Published: 01 November 1987
.... It also is suitable for architectural and industrial applications. Forms Available: Mainly wire; also bar, rod, plate, shapes,tube, sheet and strip. Applications: Copper No. C 11100is used mainly for electrical power transmission where resistance to softening under overloads is desirable. Manufacturers...
Journal Articles
Alloy Digest (1999) 48 (11): Fe-121.
Published: 01 November 1999
...-106 for more detail on NK Super E-Core. Applications: Power Distribution. NK Super BR-Core is used in transform- ers to suppress exciting inrush current. ©Copyright 1999, ASM International. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM...
Journal Articles
Alloy Digest (2010) 59 (1): SA-612.
Published: 01 January 2010
... size and distribution of nonmetallic inclusions. See Fig. 4 on steel cleanliness. Product Forms Available: Bar with diameter 25 160 mm (0.10 6.3 in.) Applications: The alloy is used for all applications requiring carburized steels, especially bearing and transmission components. Fig. 1 Hardenability...
Journal Articles
Alloy Digest (1968) 17 (7): Cu-189.
Published: 01 July 1968
... in a reducing atmosphere. HI-TENS0 1622 has good tensile strength and conducciviry to make irs use advantageous for trolley wire. Forms Avoi loble: Sheet, strip, plate, wire, rods and bars. Applications: Electrical equipment, spring contacts, trolley wire, signal and automotive relays, low load transmission...
Journal Articles
Alloy Digest (2005) 54 (8): SA-549.
Published: 01 August 2005
... alloys, advantages include higher surface hardness, shorter nitriding times, better weldability, better load-carrying capacity, better machinability, and a tougher nitrided layer. Product Forms Available: Bars and hollow bars Applications: Typical applications are in transmissions or hydraulic compo...
Journal Articles
Alloy Digest (2012) 61 (4): Cu-805.
Published: 01 April 2012
..., and spring quality. Products Available: The standard forms available are rod, bar, wire, and flatwire. For other forms, please contact the producer. Applications: Because of its good strength and wear resistance, ACB Hitenso C16200 was used for low-load transmission lines in rural areas for its earliest...
Journal Articles
Alloy Digest (1992) 41 (4): P-34.
Published: 01 April 1992
... - o.ooo2 Seconds 60-135 Table 3 -TYPICAL ROOM-TEMPERATURE GAS PERME- ABILITY AND WATER VAPOR TRANSMISSION DATA (VARIOUS TYPES OF MOLDED POLYSTYRENE) Gas Permeability, Water Vapor Transmission, cc/mi1/100 in2JatmJday gm/mil/100in2/day (75100°F) 02 N2 co2 300-400 40-50 looo-1500 2-10 - Corrosion Resistance...
Journal Articles
Alloy Digest (1957) 6 (9): Al-56.
Published: 01 September 1957
.... Forms Available: Die castings Applications: Structural parts for transmission valve bodies, trans- mission cases, transmission extensions, fittings, motor housings, meter cases, switch boxes, typewriter frames, outboard motor parts, household and office appliances. Manufacturers: Doebler-Jarvis Division...
Journal Articles
Alloy Digest (1954) 3 (8): Mn-2.
Published: 01 August 1954
... in applications which cannot incorporate rubber or plastics to reduce vibration. Forms Available: Hot or cold rolled bars or forgings, and special heat treated parts. Produced in sheer and strip to order. Applications: Power transmission equipment, vibration conttols. Manufacturer: Chicago Development Corporation...
Journal Articles
Alloy Digest (1967) 16 (2): Al-163.
Published: 01 February 1967
... Aluminum A357 is a high strength, pressure tight sand and permanent mold aluminum casting alloy. It is age-hardenable. It is recommended for cast gear cases, cylinder heads, transmission cases and strong structural castings. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1967) 16 (6): Mg-63.
Published: 01 June 1967
.... Forms Available: Sand castings, Applications: Transmission cases, missile components, aircraft nose wheels, rockets, racing auromobile pistons, components of hydraulic units. Manufacturer: J. Stone 8~ Co. (Charlron) Ltd. London, England Magnesium Elektron Lrd. Manchester, England ...
Journal Articles
Alloy Digest (1960) 9 (2): Mn-1.
Published: 01 February 1960
..., special shapes. Applications: Low temperature resistor ap lications - rheostats, auxiliary heaters for circuit i makers - electricallv heated ex ansion elements, thermostatic bimetal, ele& trical P app iances, low thermal transmission couplings. ,&nneal: Heat in neutral or reducing atmosphere (S-free...
Journal Articles
Alloy Digest (2003) 52 (10): Al-385.
Published: 01 October 2003
..., and artificially aged. General Characteristics: This aluminum-silicon alloy is used when high strength with wear and/or galling resistance is required, particularly sliding friction. Other alloy families generally require hard coat anodiz- ing for wear applications. The alloy has good machining charac- teristics...
Journal Articles
Alloy Digest (2006) 55 (7): Fe-139.
Published: 01 July 2006
... Metglas 2605 SA1 is an amorphous iron-base soft magnetic alloy designed for extremely low core loss at distribution and power transformer frequencies and inductions. Applications include high-frequency inductors and current transformers. This datasheet provides information on composition, physical...