1-15 of 15 Search Results for

transducers

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1977) 26 (6): Ni-246.
Published: 01 June 1977
..., electrical components, transducers and nickel-cadmium batteries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-246...
Journal Articles
Alloy Digest (1984) 33 (5): Fe-70.
Published: 01 May 1984
... MAGNIFER 50 is a soft magnetic iron-nickel alloy containing about 48% nickel. It has a saturation induction of 1.55T and a high permeability. It exhibits the highest saturation induction obtainable with iron-nickel alloys. Typical applications are (1) Low-frequency power transducers, (2) Chokes...
Journal Articles
Alloy Digest (1967) 16 (1): Co-50.
Published: 01 January 1967
.... Material in this condirion is currently being used in self-biasing magnetostriction transducers operating at remanence. Hiperco 50 will also respond to magnetic annealing in the same manner as Supermendur, although it is recom- mended that Supermendur be purchased for the special applications in which...
Journal Articles
Alloy Digest (1967) 16 (7): Ni-125.
Published: 01 July 1967
... and elecrrical proper- ties which allow its use in magneric and electrical devices. Its magnetostrictive capabilities make it useful in transducers. The bight shiny lustre and good corrosion resistance make it an excellent choice for appltcations where decorative appearance is important. Availability: 1. Reroll...
Journal Articles
Alloy Digest (1992) 41 (1): Co-85.
Published: 01 January 1992
... or coil (strip). Strip ranges upward from 0.002 thick: maximum width is 16 . Applications: Motor, generator, transformer and head laminations; torque mechanisms; cordless power tools; poles and cores; transducers. Producer: Spang Specialty Metals Butler, Pennsylvania 16003 ...
Journal Articles
Alloy Digest (1967) 16 (9): Co-52.
Published: 01 September 1967
... magnetic saturation at high magnetic levels is essential. It is also useful for its high value of positive magnetostriction for sonar applications, ultrasonic transducers and commercial equipment. Foms Available: Bars - hot rolled to centerless ground. Applications: Electrical equipment, sonar, ultrasonic...
Journal Articles
Alloy Digest (1982) 31 (2): Fe-64.
Published: 01 February 1982
... nominal thickness and of almost any length. Several standard widths up to 2 inches are available and other widths can be obtained by slitting or special casting. Applications. METGLAS alloy 2605SC finds applications in pulse transformers, magnetic amplifiers. power transformers, current transducers...
Journal Articles
Alloy Digest (1996) 45 (6): Fe-110.
Published: 01 June 1996
...-wound cores. core sheets. and relay parts. The producer can also undertake job-annealing of Par=. Applications: Producer: KRUPP VDM GmbH D-58778 WerdohVGerman) (2392) 55-O In USA: VDM Technologies Corp. Parsippany. NJ 07051 (201) 167-8515 Typical applications of Magnifer 36 are: l LF transducers l...
Journal Articles
Alloy Digest (2004) 53 (5): Fe-129.
Published: 01 May 2004
.... Contact the producer for sizes available. Applications: Rotelloy 5 is used for maximum savings in weight and space in aircraft generators, fuel pump motors, torpedo motors, motors for active magnet- ic bearings, racing car generators, and transducers for underwater detec- tion. Producer: Carpenter...
Journal Articles
Alloy Digest (1971) 20 (11): Co-4.
Published: 01 November 1971
..., oceanographic cable, heart springs, helical springs, corrosion-resistant springs, pressure transducers and diaphragms. Manufacturer: Elgiloy Company Elgin, Illinois 60120. ...
Journal Articles
Alloy Digest (2004) 53 (4): Fe-128.
Published: 01 April 2004
... available. Applications: Rotelloy 3 is used for savings in weight and space in aircraft generators, fuel pump motors, torpedo motors, motors for active magnetic bearings, racing car generators, and transducers for underwater detection. Producer: Carpenter Technology Ltd. Napier Way Crawley, West Sussex...
Journal Articles
Alloy Digest (2004) 53 (6): Fe-130.
Published: 01 June 2004
... squares as hot worked. Contact the producer for sizes available. Applications: HS 50 is used for savings in weight and space in aircraft generators, fuel pump motors, torpedo motors, motors for active magnetic bearings, rac- ing car generators, and transducers for underwater detection. Producer: Carpenter...
Journal Articles
Alloy Digest (1976) 25 (3): Ni-224.
Published: 01 March 1976
... for such parts. Nimag 100 has unusual magnetostriction characteristics and is used extensively in equipment employing the use of magneto- striction effects, viz, sonar, fathometer, ultrasonic soldering de- vices transducers, and others. Forms Available: Rod, plate, strip and foil. Applications: Electrical...
Journal Articles
Alloy Digest (1970) 19 (10): Mo-10.
Published: 01 October 1970
... and fluorescent lamps, electronic tube components, electric furnace elements, electrical contacts and electrodes, slip-ring brushes, supports in transducers and rectifiers, structural parts for rockets and missiles. Manufacturer: Climax Molybdenum Company of Michigan, a Subsidiary of American Metal Climax, Inc...
Journal Articles
Alloy Digest (1962) 11 (10): Ni-75.
Published: 01 October 1962
... of magner- ostriction effects, viz., sonar, farhometer, ultrasonic soldering devices transducers, and others. Forms Available: Rod, bar, pipe, tubing, plate, sheet, strip, clad place. Applications: Caustic alkalies handling equipment and piping. Production storage, producrion and handling of fluorine...