Alloy Digest (1970) 19 (11): Cu-222.
Published: 01 November 1970
... Copper No. 110, generally known as electrolytic tough pitch copper or ETP, is cathode copper remelted and cast with a controlled oxygen content. It is the most important type of copper commercially available and is used by the electrical industry as wire for electrical conductors, bars for bus...
Journal Articles
Alloy Digest (1970) 19 (11): Cu-221.
Published: 01 November 1970
... COPPER Nos. 113, 114, 115 and 116 are tough pitch coppers containing varying quantities of silver. At ambient temperatures, their properties are the same as those of tough pitch copper. Silver is added to increase the resistance to softening at elevated temperatures. This datasheet provides...
Journal Articles
Alloy Digest (1983) 32 (8): Cu-461.
Published: 01 August 1983
.... Copper Alloy No. C 11000. ASTM: B 49 and B 133. ASME SB 12. Federal: QQC-502. Military: MIL-C-12166. SAE: 5461 and 5463. General Characteristics: Mueller Copper 1100, commonly known as electrolytic tough pitch copper, is a copper containing nominally 0.04Yc oxygen. It has excellent electrical and thermal...
Journal Articles
Alloy Digest (2005) 54 (1): Cu-728.
Published: 01 January 2005
... Wieland-K32 is a nondeoxidized copper with acceptable electrical and thermal conductivities. It is often called electrolytic tough pitch copper. Typical applications include wrapping strip for power cables and for coaxial telephone cables in electrical engineering. This datasheet provides...
Journal Articles
Alloy Digest (2021) 70 (7): Cu-922.
Published: 01 July 2021
... Aurubis Cu-ETP (electrolytic tough pitch copper) is an electrolytically refined, high conductivity copper that contains a minimum of 99.90% Cu and a controlled amount of oxygen (generally 0.02–0.04%). It has a minimum electrical conductivity of 100% IACS. Special precautions are necessary when...
Journal Articles
Alloy Digest (2022) 71 (5): Cu-931.
Published: 01 May 2022
... Mueller Brass C11000 (electrolytic tough pitch copper) is an electrolytically refined, high conductivity copper that contains a minimum of 99.90% copper and a controlled amount of oxygen in the form of Cu2O. It has a minimum electrical conductivity of 100% IACS. Electrolytic tough pitch copper...
Journal Articles
Alloy Digest (2020) 69 (10): Cu-913.
Published: 01 October 2020
... KME Cu-ETP (electrolytic tough pitch copper) is an electrolytically refined, high conductivity copper that contains a minimum of 99.90% Cu and a controlled amount of oxygen in the form of Cu2O. It has a minimum electrical conductivity of 100% IACS. Cu-ETP is the most widely used grade of copper...
Journal Articles
Alloy Digest (1990) 39 (11): Cu-554.
Published: 01 November 1990
... Copper Nos. C12500, C12700, C12800, C12900 and C13000 fire refined tough pitch coppers differ only in silver content. All have electrical conductivity of 98% IACS, volume basis. Minimum copper + silver content of these grades is 99.88%. Silver confers anneal resistance to the materials...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-590.
Published: 01 October 1993
... properties UNS C11100 Filing Code: cu-590 COPPER ALLOY NO. Cl1100 CopperA oy OCTOBER 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS COPPER ALLOY NO. Cl 1100 P-by: Alby Digest. Inc. 1201%77%161 27 Car&Id Stmel. Orange. N.J. 07050 I USA (Electric Tough Pitch, Anneal Resistant) COPPER ALLOY NO. Cl 1100...
Journal Articles
Alloy Digest (1987) 36 (11): Cu-530.
Published: 01 November 1987
... DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: Cu-530 Copper Alloy NOVEMBER 1987 Published by: Alloy Dipa. imc 17cmtiKldslrcn onnp. Newkmq070SO (201) 677-9161 Copper No. Cl 1100 (Electrolytic lough Pitch, Anneal Resistant) Copper No. Cl 1100is commonly known as anneal-resistant electrolytic copper...
Journal Articles
Alloy Digest (1982) 31 (7): Cu-441.
Published: 01 July 1982
... Copper Alloy No. C18700 is a copper-base alloy containing lead (nominally 1.0%). The lead is added to impact free-cutting properties to the metal. Although the lead lowers the electrical conductivity of Alloy No. C18700 slightly below that of tough-pitch copper, it still has high electrical...
Journal Articles
Alloy Digest (1988) 37 (1): Cu-533.
Published: 01 January 1988
... CDA C18700 is a copper-base alloy containing lead (nominally 1.0%). The lead is added to impart free-cutting properties to the metal. Although the lead lowers the electrical conductivity of CDA C18700 slightly below that of tough-pitch copper, it still has high electrical conductivity well within...
Journal Articles
Alloy Digest (2003) 52 (9): Cu-709.
Published: 01 September 2003
... Wieland-K30 is a nondeoxidized copper with acceptable electrical and thermal conductivities. It is often called electrolytic tough pitch copper. Typical applications include lead frames and automotive connectors. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1980) 29 (8): Cu-400.
Published: 01 August 1980
...) Its pipes and tubes have the highest thermal conductivity of any standard heat-exchanger material, (2) It provides greater ductility than tough pitch copper, (3) It permits excellent silver-alloy brazing, carbon-arc welding, inert-gas arc and oxyacetylene welding and (4) It con- tains no oxygen...
Journal Articles
Alloy Digest (2007) 56 (7): Cu-749.
Published: 01 July 2007
... sulfate, sodium carbonate, sodium nitrate, sodium sulfate, and zinc sulfate. Water. All types of potable water, any industrial and mine waters, seawater, and brackish water. Tough pitch copper is considered to be immune to stress-corrosion DOI: 10.31399/asm.ad.cu0749 cracking in ammonia and the other...
Journal Articles
Alloy Digest (1985) 34 (4): Cu-495.
Published: 01 April 1985
... and mechanical properties are similar to those of electrolytic tough pitch copper, the most widely used of the coppers. Mueller Copper 1220, however, has certain fabvricat- ing advantages over tough pitch copper. It can be more severely cold worked and is more readily joined by welding. In consequence...
Journal Articles
Alloy Digest (1972) 21 (3): Cu-253.
Published: 01 March 1972
... pitch copper, the most widely used of the coppers. However, Copper No. 122 has certain fabricating advantages over tough pitch copper. It can be more severely cold worked and is more readily joined by welding. In consequence, it is used widely for the fabrication of equipment for such applications...
Journal Articles
Alloy Digest (1971) 20 (10): Cu-243.
Published: 01 October 1971
... is involved. Specification Equivalents: ASTM B301. CDA No. 145. General Characteristics: COPPER No. 145 is a deoxidized copper-tellurium alloy which combines good machinability with high conductivity. it can be machined at speeds from two to five times those used with electrolytic tough pitch copper. Surface...
Journal Articles
Alloy Digest (1964) 13 (8): Cu-144.
Published: 01 August 1964
...: Oxygen-Free, High-Conductivity Copper combines most of the advantages of Electrolytic Tough Pitch Copper and Deoxidized Copper. Ic is excellent for deep draw- ing, has high electrical and thermal conductivity, and resists the embrirrling effect of reducing gases (hydrogen) on equipment operated...
Journal Articles
Alloy Digest (2022) 71 (1): Cu-928.
Published: 01 January 2022
.... Information on resistance to softening sourced from Electrolytic Tough Pitch Copper, Copper Development Association, 2018. Table 1 Mechanical properties at room temperature Material condition(a) R220 R240 R290 R360 Tensile strength MPa ksi 220 260 32 38 240 300 35 44 290 360 42 52 360 52 0.2% proof...