1-20 of 3193 Search Results for

tough resistance

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (8): TS-368.
Published: 01 August 1980
... toughness and resistance to splitting stresses. It has found a number of other uses requiring resistance to shock loading and splitting stresses, such as clutch parts, vise jaws and expander punches. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (11): Cu-530.
Published: 01 November 1987
... Copper No. C11100 is commonly known as anneal-resistant electrolytic copper. It is produced mainly as wire for electrical power transmission where resistance to softening under overloads is desired. This datasheet provides information on composition, physical properties, and elasticity. It also...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (11): SS-510.
Published: 01 November 1989
... GALL-TOUGH Stainless is an austenitic stainless steel which possesses superior self-mated galling and metal-to-metal wear resistance. It is stronger and has better high-temperature oxidation resistance than AISI Type 304 stainless. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (3): SS-541.
Published: 01 March 1993
... ESCOLOY 45D is a duplex stainless steel casting with a combination of high strength, toughness and corrosion resistance. Pumps or valves handling sea water is one application area. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (10): Cu-590.
Published: 01 October 1993
... properties UNS C11100 Filing Code: cu-590 COPPER ALLOY NO. Cl1100 CopperA oy OCTOBER 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS COPPER ALLOY NO. Cl 1100 P-by: Alby Digest. Inc. 1201%77%161 27 Car&Id Stmel. Orange. N.J. 07050 I USA (Electric Tough Pitch, Anneal Resistant) COPPER ALLOY NO. Cl 1100...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (2): SS-986.
Published: 01 February 2007
... Gall-Tough Plus Stainless is a modification and improvement of Gall-Tough (Alloy Digest SS-510, November 1989). Gall-Tough Plus stainless is an austenitic stainless steel that possesses superior self-mated galling and metal-to-metal wear resistance. It is stronger and has better high-temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (10): TS-291.
Published: 01 October 1975
... UHB Regin 3 is a chromium-tungsten-vanadium tool steel characterized by good toughness (especially when exposed to impact stresses), high red hardness, good wear resistance and good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (8): SA-214.
Published: 01 August 1967
... FAGERSTA K825 is a tough, shock resistant alloy steel having high tensile strength and endurance limit in the heat treated condition. It is recommended for shafts, bolts, countershafts, etc. in moderately stressed applications. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (4): TS-6.
Published: 01 April 1953
... VAIRLOY is a manganese-chromium-molybdenum tool and die steel capable of being air-hardened at low temperatures with minimum distortion and deformation. It is strong, tough and wear resistant. This datasheet provides information on composition and hardness. It also includes information on forming...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (7): TS-48.
Published: 01 July 1956
... BETHLEHEM 67 CHISEL is the general-purpose, tungsten-type of shock-resisting tool steel. It has excellent properties for cold battering tools and hot-work shock applications. It is characterized by unusual toughness, resistance to fatigue and relative ease of heat treatment. This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (3): Cu-24.
Published: 01 March 1955
... toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-24. Producer or source: Revere Copper and Brass Inc.. Producer or Source: Revere Copper and Brass Inc. Copyright © ASM International® 1996 1996...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (1): SA-189.
Published: 01 January 1966
... to one. Specification Equivalents ASTM A-242-63T ASTM A-441-63T General Characteri sties: Tri-Steel is a low alloy high strength structural steel capable of providing greater load capacity with no corresponding increase in weight. It has good notch-toughness, resists abrasion and de- formation...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (5): Al-403.
Published: 01 May 2007
... Compressive Plane-strain Tensile strength, Yield strength, yield strength, fracture toughness, Resistance to Thickness L direction L direction Elongation L direction L-T direction SCC(b), min Alloy, temper mm in. MPa ksi MPa ksi L direction, % MPa ksi MPa m ksi in. EXCO rating(a) MPa ksi 7449, T79511 12 50...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (10): Al-373.
Published: 01 October 2000
... Alcoa 2324-T39 plate is an age-hardenable high-strength version of alloy 2024 (Alloy Digest Al-23, August 1973, and Al-346, March 1998). The 2324-T39 alloy is used where higher strength; toughness, and good resistance to fatigue-crack propagation are needed. A typical application is the lower wing...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (8): TS-654.
Published: 01 August 2007
... Thyrodur 2826 is a shock-resistant tool steel of average hardenability and intermediate alloy content compared with other tool steels with high toughness and resistance to shock. Shock-resistant steels are used primarily for chisels, rivet sets, punches, driver bits, and other applications...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (4): TS-663.
Published: 01 April 2008
... DuraTech Xtreme has very high impact toughness, high hot hardness, and good wear resistance. As indicated in the name, the alloy is intended for use in extreme” conditions. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (7): TS-320.
Published: 01 July 1977
... VASCO WEAR is an air-hardening, cold-work die steel developed to provide high resistance to wear at exceptionally good levels of toughness. It also has the high compressive strength necessary for maximum resistance to upsetting. Its many uses include such applications as thread-rolling dies...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (2): SS-876.
Published: 01 February 2003
.... These properties supplement the superior fracture toughness and Charpy impact energies. This martensitic precipitation-hardening stainless steel has very good resistance to general corrosion and stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1963) 12 (12): SA-158.
Published: 01 December 1963
... Jessop No. 9 is a non-magnetic super high tensile steel having exceptionally high toughness and wear resistance. It is recommended for heavy earth moving equipment subject to severe battering. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (3): TS-584.
Published: 01 March 2001
... Timken Latrobe Steel TLP A11 is a powder metallurgically produced A11 type of tool steel that is air hardening. It provides high wear resistance and a relatively high impact toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity as well...