Alloy Digest (1987) 36 (9): CS-114.
Published: 01 September 1987
... construction applications corrosion-resistant alloys elasticity forgings fracture toughness hardness heat treatability joinability machinability physical properties pressure vessels SAE 1025 spinning tools tensile properties torque transmission components workability Producer or Source...
Journal Articles
Alloy Digest (1967) 16 (2): SA-206.
Published: 01 February 1967