Alloy Digest (1990) 39 (2): Ni-378.
Published: 01 February 1990
... CARPENTER VACUMET HYMU "800" ALLOY is a vacuum melted nickel-iron-molybdenum alloy available in strip form for the manufacture of laminations and tape toroids. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating...
Journal Articles
Alloy Digest (1969) 18 (4): Ni-144.
Published: 01 April 1969
... Allegheny Ludlum Moly Permalloy is a nickel-iron-molybdenum alloy having excellent permeability and core loss properties. It has high initial and maximum permeability, low coercive force, and low hysteresis loss. It is recommended for toroids, tape and lamination cores. This datasheet provides...
Journal Articles
Alloy Digest (1969) 18 (8): Fe-38.
Published: 01 August 1969
... Alfenol is an unoriented 12% to 16% aluminum-iron alloy which has high electrical resistivity and low eddy current losses. It is furnished in the 12% aluminum and in the 16% aluminum grades. The recommended uses are for relays, gyro mechanisms, servo-mechanisms and toroid tape cores...
Journal Articles
Alloy Digest (1970) 19 (6): Ni-158.
Published: 01 June 1970
... Carpenter Hy-Ra 80 is a nickel-iron-molybdenum alloy specially processed to exhibit square hystereris loop properties. It is recommended for tape wound toroids which will show specific magnetic characteristics after hydrogen annealing. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1983) 32 (11): Ni-294.
Published: 01 November 1983
... MAGNIFER 75 is a soft magnetic nickel-iron alloy containing about 5% copper and 2% chromium. It offers very high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound toroids, laminations, shielding and relay parts. This datasheet...
Journal Articles
Alloy Digest (1972) 21 (5): Ni-173.
Published: 01 May 1972
... Iron PROPERTIES Fig. 1 - Effect of annealing treatment on magnetic permeability. Tape toroid specimen. Copyright © ASM International® 1996DOI: 10.31399/asm.ad.ni0173 Exciting Field H &) Fig. 2 - Typical magnetization curves for 0.002-m. (0.005 cm) thick tape toroid l-in. (2.54 cm) ID by l k-in. (3.18...
Journal Articles
Alloy Digest (1967) 16 (4): Ni-123.
Published: 01 April 1967
... Elongation, % in 2 60 8.74 0.316 0.08 12.9 65 0.0011 460 0.118 2650 31.5-33.7 DOI: 10.31399/asm.ad.ni0123 Copyright © ASM International® 1996 Normal Magnetization Curves Carpenter HyMu 800 .OOY thick tape toroid 1 I.D. x 1% O.D. Normal Magnetization Curves Carpenter Hyh,lu 800 .004 thick tape toroid...
Journal Articles
Alloy Digest (1971) 20 (10): Ni-5.
Published: 01 October 1971
...: Transformer cores, tape-wound toroids and laminations for compactness and weight saving, and magnetic shields for protection of electrical components against stray magnetic tieids. Manufacturer: Carpenter Technology Corporation Reading, Pennsylvania 19603. lhrsted~ (Silberts per Centimeter)-Magnetizing Fonx...
Journal Articles
Alloy Digest (1984) 33 (2): Ni-291.
Published: 01 February 1984
... for transformers, tape-wound toroids, laminations, shielding and relay parts. Nore: This digest was revised to correct errors from several sources. l MAGNIFER is a registered trademark of Vereinigte Deutsche Metallwerke AG. Composition: Nickel 80 Molybdenum 5 Manganese 0.5 Silicon 0.3 Carbon 0.02 Iron Remainder...
Journal Articles
Alloy Digest (1989) 38 (10): Ni-375.
Published: 01 October 1989
..., gauss (split snip. split rod) 3500 Minimum 6OHz AC permeability @ 40 gauss 200 gauss 2000 gauss 0.025 in. thick* 35300 40000 55000 0.006 in. thick* 65ooo 85000 135000 0.002 in. thick** 7oOOo 9oooo 220000 *l l/2 in. OD x 1 in. ID ring lamination specimens. **Tape toroid specimen. Condition Table 3...
Journal Articles
Alloy Digest (2021) 70 (1): Co-132.
Published: 01 January 2021
... toroidal bars 200 3 × 3/8 × 3/16 in. 4000 cpm (67 Hz) Room temperature, air 100 0 1,0E+0,5 1,0E+0,6 1,0E+0,7 1,0E+0,8 1,0E+0,4 Cycles RBF S/N diagram in ksi units Fig. 2 As-built microstructure, etched cross-section along the Z-direction, 50× 120,00 100,00 Load (ksi) 80,00 Interrupted at 60,00 20 M cycles...
Journal Articles
Alloy Digest (1966) 15 (7): Fe-28.
Published: 01 July 1966
... Division HamiIton Watch Company Lancaster, Pennsylvania DOI: 10.31399/asm.ad.fe0028 Copyright © ASM International® 1996 FIGURE 3 INITIAL PERMEMIlmY vs REolJENcY lhe initial p.rm.abilitie, o, a fwktion of fnqumcy 0.. ,howvn FIGURE 4 AC MAGNETIC PROPERTIES: The magnetic properties were obtained on toroidal...
Journal Articles
Alloy Digest (1976) 25 (11): Ni-235.
Published: 01 November 1976
... or 207-l 380 hfPa Saturation magnetization, 4 7rMs 7.8 K gauss 0.78 T B,/B,, unstressed 0.4 0.4 Br/Bs, applied stress of 0.95 0.95 30,000-200.000 psi or 207-l 380 MPa Toroid Annealed in Vacuum for 2 Hours at 3250C Permeability at lOOHz, AB = 100 Gauss 12000 12000 Coercive force, Hc 0.02 Oe 1.57 A/m B...
Journal Articles
Alloy Digest (1996) 45 (7): Ni-514.
Published: 01 July 1996
... thickness 0.1 mm) PlopnkmT Ma&al 8.q Ba. h w MagnifaS3F so >350 SilO >120 100 a700 A00 >240 Available Forms: Ship and toroidal tape-wound cores. Applications: Typical applications of Magnifer 53 are: . LFtransducem l htegrating current transformers for earth-leakage circuit- breakers Producer: KRUPP VDM...
Journal Articles
Alloy Digest (2006) 55 (7): Fe-139.
Published: 01 July 2006
... data are given in Fig. 1 2; all data were taken on standard toroids at room temperature after suitable annealing cycles. Details of testing procedure are available from the manufacturer. General Characteristics: This alloy and other Metglas alloys are produced by cooling at about a million degrees...
Journal Articles
Alloy Digest (1960) 9 (11): Ni-62.
Published: 01 November 1960
... in the purchaser s plant, Westinghouse canoot be respoosible for the final quality of the product. Sheet, strip, sections and cores. Cold rolled and hot rolled sheets. Heat treated laminations. Applications: High Q choke coils, toroidal cores, filter reactors, laminations in special traosformers. Manufacturer...
Journal Articles
Alloy Digest (1996) 45 (8): Fe-111.
Published: 01 August 1996
... is relatively 10~. Available Forms: Semis. Strip, ribbon. sheet. bar. and wire are available. Sizes and tolerances are available from the producer Fabricated. Toroidal tape-wound cores, core sheets. and relay parts. The producer can also undertake job-annealing of parts. DOI: 10.31399/asm.ad.fe0111 Table 2...
Journal Articles
Alloy Digest (1996) 45 (6): Fe-110.
Published: 01 June 1996
...= Gxebxs *Y cl-a& ~IODIK DMD PI6 ccnn. &.Ivm 1fxtInuuLmT WIN MagniferMK MDI DI 0.10-0.35 XCOZ ?OOfC, V,o=I.l MD la D la 0.104.35 23co~xc4c~ DIN41301 Available Forms: Semis. Strip. ribbon. sheet. bar. and wire are available. Contact the producer for sizes and tolerances. Fabricated Parts. Toroidal tape...
Journal Articles
Alloy Digest (1982) 31 (2): Fe-64.
Published: 01 February 1982
... magnetic properties of METGLAS alloy 2605SC in the as- cast and annealed conditions are given in Table 1. Other mag- netic data are given in Figures 1 to 4; all data were taken on standard toroids at room temperature after suitable annealing cycles. Details of testing procedure are available from the manu...
Journal Articles
Alloy Digest (1982) 31 (4): Fe-65.
Published: 01 April 1982
... during 1982. Magnetic Properties: Some magnetic properties of METGLAS alloy 2605S-2 in the as- cast and annealed conditions are given in Table 1. Other magnetic data are given in Figures I to 5; all data were taken on standard toroids at room temperature after suitable annealing cycles. Details...