Publisher: Journals Gateway
Alloy Digest (1965) 14 (6): Ti-44.
Published: 01 June 1965
... treatability joinability machinability physical properties tensile properties titanium-Aluminum-vanadium-tin alloys workability I Filing Code: Ti-44 -I mm. Titanium Alloy I JUNE 1965 -DATA ON WORLD WIDE METALS AND ALLOY2 Pdlishd 6y . . Engmemg Alloys Digest, Inc. Ti-6AL6V-2Sn Uppa Moaadrir. New Jay...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (1): Ti-61.
Published: 01 January 1971
.... As a neutral stabilizer. the 2% tin strengthens both the alpha and beta phases, and, with the aluminum, provides better room and elevated temperature strength properties than CARPENTER TITANIUM 64 (6% A1-4% Vanadium) alloy and other lower-alloyed alpha-beta compositions. Beta stabilization is accomplished...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (4): Ti-57.
Published: 01 April 1969
... by Engineering Alloys Digest, Inc Uppa Montclair, New Jew HARVEY HA 5158 (High Temperature Alloy) HARVEY HA 5 158 is an alpha-beta, heat treatable titanium alloy recommended for elevated temperature applications. Composition: Physical Constants: (at 70°F) Aluminum 5.0-6.0 Density, lb/cu.in. 0.164 Vanadium 5.0...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (7): Ti-180.
Published: 01 July 2021
... is necessary in pickling to minimize hydrogen absorp- Stress-Corrosion Cracking. Due to its high vanadium content tion. Information on welding sourced from M.J. Donachie, and lower aluminum content, CarTech Ti 15V-3Cr-3Sn-3Al is Titanium: A Technical Guide, 2nd ed, ASM International, expected to be less...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (9): Al-190.
Published: 01 September 1969
... max. Iron 0.30 max. Magnesium 0.02 max. zinc 0.10 max. Copper 5.8-6.8 Manganese 0.2GO.40 Titanium 0.02-0.10 Zirconium 0.10-0.25 Vanadium 0.05-O. 15 Cadmium 0.05-0.20 Tin 0.03-0.08 Others, each 0.05 max. , total 0.15 max. Aluminum Remainder Physical Constants: (-T81 Temper) (Typical) Specific gravity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (12): SA-774.
Published: 01 December 2016
... 0.75 Phosphorus 0.020 max Sulfur 0.020 max Aluminum, total 0.015 0.080 Boron 0.001 0.010 Chromium 0.90 1.20 Molybdenum 0.90 1.10 Nickel 0.20 max Vanadium 0.60 0.80 Titanium 0.07 0.15 Arsenic 0.020 max Tin 0.020 max Copper 0.20 max Antimony report R* 0.1 max *R = P + 2.43As + 3.57Sn + 8.16Sb + 0.13Cu...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (11): Cb-25.
Published: 01 November 2000
... Inc. Chemical Composition, wt%: Element Composition, wt.% Hafnium 10.0 Titanium 0.7 1.3 Zirconium 0.7 Tantalum 0.5 Tungsten 0.5 Element Guaranteed impurity, ppm Carbon <150 Hydrogen <10 Iron <50 Copper <40 Chromium <20 Manganese <20 Nickel <20 Vanadium <20 Tin <10 Oxygen <225 Nitrogen <150 Silicon <50...