1-9 of 9 Search Results for

tin babbit

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (4): Sn-3.
Published: 01 April 1973
... Tin Babbit comprises a family of essentially tin-antimony-copper alloys used to minimize friction in moving parts of machines. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (7): Pb-11.
Published: 01 July 1973
... temperatures. * G Babbit is a trademark of American Smelting and Refining Company. Ca4nposition: Lead Antimony AXWliC Tin Copper Nominal 83.50 12.75 3.00 0.75 Range Remainder 12.0-l 3.5 2.5-3.0 0.6-l .O 0.1 max. Physical Constants: Density, lb/cu in. Specific gravity Melting point, oF Solidus Liquidus Modulus...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (7): Pb-10.
Published: 01 July 1973
... Lead Babbit comprises a family of alloys used to cut down on friction in moving parts of machines. Alloys 7, 8 and 13 are essentially lead-antimony-tin alloys. Alloy 15 is an arsenical (about 1% arsenic) lead-base alloy. This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (12): Cu-324.
Published: 01 December 1976
... Prrblisbed by EIlgneerine AlIoys Dii Inc. Upper Mont&r, New Jersey FEDERAL+ BRONZE 822 (High-Leaded Tin Bronze) FEDERAL BRONZE 822 is a copper-base, high-lead bearing bronze with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (6): Cu-439.
Published: 01 June 1982
... Copper Alloy No. C93500 is a cast bronze containing nominally 9% lead and 5% tin. It has excellent machinability, low strength and good resistance to corrosion. It is used for corrosion-resistant castings, small bearings and bushings. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (6): Cu-819.
Published: 01 June 2013
... 2CX Chemical Composition, wt (Nominal) Nickel 9 Tin 6 Copper bal Physical Properties: Density, kg/m3 (lb/in.3) 8910 (0.322) Thermal conductivity, W/m·K (Btu/(h·ft·ºF)) 52 (30) Magnetic permeability < 1.001 Coefficient of linear thermal expansion, 21 102 ºC (70 215 ºF), 10 6/K (10 6/ºF) 16.2 (9.0...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (9): Cu-258.
Published: 01 September 1972
... possessing unusually good frictional properties. It will not, even under extreme conditions, melt like a babbit or freeze on the shaft like a bronze. Microexamination shows that the lead is in fine, globular form and uniformly distributed. Also, there is no lead between the copper-tin grain boundaries...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (5): Cu-724.
Published: 01 May 2013
... performance and high thermal stability to plain bearing applications. Parts are easily formed and they can be machined either before or after heat treatment. TOUGHMET 2 (Spinodal Cu-Ni-Sn Alloy) TOUGHMET 2 Chemical Composition, wt (Nominal) Nickel 9 Tin 6 Copper bal Physical Properties: Density, kg/m3 (lbs...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (3): Al-250.
Published: 01 March 1984
.... Composition: Tin Silicon Copper Nickel Iron Titanium Magnesium Manganese Others, total Aluminum 5.5-7.0 2.0-3-O 0.7-l .3 o-30-0.7 0.7 max. 0.20 max. 0.10 max. 0.10 max. 0.30 max. Remainder Physical Constants: (Approximate) Density, lb/cu in. 0.102 Specific gravity 2.83 Thermal coef. expansion/ F (-58...