Alloy Digest (1994) 43 (5): Ni-453.
Published: 01 May 1994
... NICROBELL alloys were developed to be compatible with and complimentary to the thermoelectric conductors used for thermocouples and other conducting cables. This datasheet provides information on composition and physical properties. Filing Code: Ni-453. Producer or source: Nicrobell Pty Ltd...