Alloy Digest (1999) 48 (9): SS-761.
Published: 01 September 1999
... Kubota alloy KRH35CL is similar to KHR35C but contains lower carbon for applications requiring good thermal fatigue and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (1988) 37 (11): Co-84.
Published: 01 November 1988
... HAYNES ALLOY No. 150 is a cobalt-base alloy with excellent thermal shock resistance. It has a higher melting point than other cobalt-and nickel-base high-temperature alloys and resists high-temperature corrosion in air and air-sulfur dioxide atmospheres. This datasheet provides information...
Journal Articles
Alloy Digest (1960) 9 (11): TS-99.
Published: 01 November 1960
... Mohawk is a 14% tungsten hot work steel having good red hardness and good abrasion resistance, but lower thermal shock resistance than the 5% chromium hot work die steels. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1962) 11 (5): Co-14.
Published: 01 May 1962
... Haynes Stellite Alloy No. 6 is a cobalt-base high-carbon alloy having high heat and thermal shock resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1962) 11 (6): Co-32.
Published: 01 June 1962
... SM 302 is a cast cobalt-base alloy having superior oxidation and thermal shock resistance. It was designed primarily for use as a first stage turbine vane to operate in the temperature range of 1500-2000 F. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1965) 14 (3): Co-43.
Published: 01 March 1965
... MAR-M 302 is a cast cobalt-base alloy having superior oxidation and thermal shock resistance. It was designed primarily for use as a first stage turbine vane to operate in the temperature range of 1500-2000 F. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1966) 15 (5): Co-48.
Published: 01 May 1966
... ESCO Alloy 72 is a cobalt-base alloy having high corrosion, heat and thermal shock resistance. It is recommended for applications requiring good mechanical properties at elevated temperatures and/or in corrosive media. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1957) 6 (6): Ni-35.
Published: 01 June 1957
... JESSOP G.39 is an austenitic nickel-base alloy having low coefficient of expansion and good thermal shock resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (1995) 44 (11): SS-621.
Published: 01 November 1995
... CENTRALLOY 4859 is a cast austenitic iron base alloy with 32% nickel and 20% chromium plus niobium. Despite a low carbon content it has a very stable austenitic structure, sufficient stress rupture strength, excellent thermal shock resistance, and is not susceptible to embrittlement. CENTRALLOY...
Journal Articles
Alloy Digest (2019) 68 (4): SS-1305.
Published: 01 April 2019
... MANAURITE 900X is a casting alloy with good creep strength and high thermal shock resistance. This alloy is evolution from Manaurite 900 (Alloy Digest SS-1304, March 2019). This datasheet provides information on composition and physical properties as well as creep. It also includes information...
Journal Articles
Alloy Digest (1990) 39 (7): Cer-4.
Published: 01 July 1990
... SILICON NITRIDE SN-220 has found its niche in industrial applications in engine and gas turbine components. It has excellent high-temperature strength and thermal shock resistance. This datasheet provides information on composition, physical properties, elasticity, and bend strength as well...
Journal Articles
Alloy Digest (1993) 42 (5): SS-543.
Published: 01 May 1993
... Märker G4859 is a cast austenitic iron-base alloy with good additions of chromium and nickel to develop good stress-rupture properties with good thermal shock resistance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1964) 13 (7): Ti-40.
Published: 01 July 1964
... recommended is 1800-22000F. It is recommended for severe and prolonged oxidation conditions, and where strength and thermal shock resistance are required. A low specific gravity, plus other physical properties such as high Young s modulus of elasticity, excellent compressive and tensile strength , combine...
Journal Articles
Alloy Digest (1961) 10 (1): Ti-29.
Published: 01 January 1961
...~ Oxidation Resistance at 18OOOF Hours Weight Gain, mg/cm2 50 21.2 100 31.5 200 47.6 Gewml Cbamctoristicr: The most outstanding properties of FS-26 are high temperature strength snd thermal shock resistance. In the temperature range from 1500 to MOOoF its stress to rupture and tensile strengths are equal...
Journal Articles
Alloy Digest (1997) 46 (3): TS-553.
Published: 01 March 1997
... Finkl PRESS-DIE is a precipitation-hardening die steel designed to resist thermal shock while providing wear resistance at elevated temperatures. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating. Filing Code: TS-553...
Journal Articles
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... FIREDIE 9 is a chromium-molybdenum-cobalt hot-work steel. It has outstanding resistance to softening in elevated-temperature service; the cobalt gives this steel its superior heat resistance. Firedie 9 has excellent resistance to thermal shock; in fact, dies can be water cooled durin operation...
Journal Articles
Alloy Digest (1965) 14 (5): Co-44.
Published: 01 May 1965
... Deloro-Stellite-7 is a cobalt base casting alloy possessing excellent corrosion resistance and high temperature strength together with good ductility and excellent resistance to thermal shock. It is recommended for gas turbine blades, brass casting dies and extrusion dies. This datasheet provides...
Journal Articles
Alloy Digest (1967) 16 (11): Co-54.
Published: 01 November 1967
... MAR-M Alloy 509 is a vacuum melted, cobalt-base alloy having high strength, low creep rates, and resistance to oxidation and thermal shock. It is recommended for aircraft and industrial gas turbine applications. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1961) 10 (3): CI-29.
Published: 01 March 1961
... MEEHANITE HE is recommended for use in applications where resistance to extreme thermal shock is the primary consideration, and physical property requirements are of a low order. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1967) 16 (3): Co-51.
Published: 01 March 1967
... UMCo-51 is a cobalt-base alloy having high stress-rupture strength. It is recommended for high temperature applications where the mechanical stresses are high, and where resistance to abrasion, thermal shock and oxidation are required. This datasheet provides information on composition, physical...