Skip Nav Destination
Close Modal
Search Results for
thermal cracking resistance
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 2190 Search Results for
thermal cracking resistance
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1959) 8 (4): SA-82.
Published: 01 April 1959
... Timken 17-22-AV is a silicon-chromium-molybdenum-vanadium alloy steel having high resistance to thermal cracking and heat checking, even in a highly hardened condition, and also has good shock resistance at high hardeness levels. This datasheet provides information on composition, hardness...
Abstract
View article
PDF
Timken 17-22-AV is a silicon-chromium-molybdenum-vanadium alloy steel having high resistance to thermal cracking and heat checking, even in a highly hardened condition, and also has good shock resistance at high hardeness levels. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-82. Producer or source: Timken Roller Bearing Company.
Journal Articles
Alloy Digest (1952) 1 (1): SA-1.
Published: 01 September 1952
... Timken 17-22A is a silicon-chromium-molybdenum-vanadium alloy steel having high resistance to thermal cracking and heat checking, even in a highly hardened condition, and also has good shock resistance at high hardness levels. It is available in two carbon grades. This datasheet provides...
Abstract
View article
PDF
Timken 17-22A is a silicon-chromium-molybdenum-vanadium alloy steel having high resistance to thermal cracking and heat checking, even in a highly hardened condition, and also has good shock resistance at high hardness levels. It is available in two carbon grades. This datasheet provides information on composition, hardness, and tensile properties. Filing Code: SA-1. Producer or source: Timken Roller Bearing Company.
Journal Articles
Alloy Digest (1996) 45 (8): SS-649.
Published: 01 August 1996
... resistance to chloride stress-corrosion cracking and good resistance to pitting, crevice, and general corrosion. It has higher thermal conductivity and a lower coefficient of thermal expansion than austenitic stainless steel. SAF2304isa mdemark of Sandvik AB. Chemical Composition, wt M cabon 0.020 23.0...
Abstract
View article
PDF
Avesta Sheffield SAF 2304 is an austenitic/ferritic duplex stainless steel with high tensile strength, impact toughness with good workability and weldability. The alloy has high resistance to chloride stress-corrosion cracking and good resistance to pitting, crevice, and general corrosion. It has higher thermal conductivity and a lower coefficient of thermal expansion than austenitic stainless steel. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-649. Producer or source: Avesta Sheffield Inc.
Journal Articles
Alloy Digest (1996) 45 (9): SS-652.
Published: 01 September 1996
..., excellent resistance to chloride stress-corrosion cracking, high thermal conductivity, and a low coefficient of thermal expansion. The impact strength is also high. In addition. Avesta Sheffield SAF 2507 s high chromium, molybdenum. and nitrogen levels provide excellent resistance to pitting, crevice...
Abstract
View article
PDF
Avesta Sheffield SAF 2507 is an austenitic/ferritic duplex stainless steel with very high strength. The alloy has a lower coefficient of thermal expansion and a higher thermal conductivity than austenitic stainless steels. The alloy has a high resistance to pitting, crevice, and general corrosion; it has a very high resistance to chloride stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-652. Producer or source: Avesta Sheffield Inc.
Journal Articles
Alloy Digest (1996) 45 (9): Ni-516.
Published: 01 September 1996
... The alloy has outstanding localized corrosion resistance, excellent stress~otrosion cracking resistance, and good thermal stability. Hastelloy and C-2000 are trademarks of Haynes huernational. Inc. Chemical Composition, wt (Nominai) Chromilllll Molybdenum Coppar Carbon Silicon Nickel 23 16 1.6 0.01 max...
Abstract
View article
PDF
Hastelloy C-2000 has a broad capability range for handling corrosive environments. The alloy has high resistance to reagent grade sulfuric acid, hydrochloric acid to high concentrations, and nitric acid. The alloy has outstanding localized corrosion resistance, excellent stress-corrosion cracking resistance, and good thermal stability. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance. Filing Code: Ni-516. Producer or source: Haynes International Inc.
Journal Articles
Alloy Digest (2023) 72 (1): SS-1355.
Published: 01 January 2023
... corrosion environments and has a lower coefficient of expansion and better thermal conductivity. Cleveland- Cliffs 444 has superior chloride stress-corrosion cracking resistance to Type 304 and Type 316 austenitic stainless steels. It is oxidation and creep resistant at elevated temperatures, making...
Abstract
View article
PDF
Cleveland-Cliffs 444 is a low carbon, low nitrogen, dual stabilized ferritic stainless steel that provides pitting and crevice corrosion resistance superior to most ferritic stainless steels and some austenitic stainless steels. It is equivalent to Type 304 austenitic stainless steel in many corrosion environments and has a lower coefficient of expansion and better thermal conductivity. Cleveland- Cliffs 444 has superior chloride stress-corrosion cracking resistance to Type 304 and Type 316 austenitic stainless steels. It is oxidation and creep resistant at elevated temperatures, making it a preferred material for the most demanding applications in automotive exhaust. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-1355. Producer or source: Cleveland-Cliffs Inc.
Journal Articles
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... resistance compared to the standard 5Yc chromium hot work steels. Firedie 9 has excellent resistance to thermal shock, and dies can be water cooled during operation without fear of cracking. The advantages in using Firedie 9 are (I) Very high toughness, (2) High hardenability. (3) Good wear resistance and (4...
Abstract
View article
PDF
FIREDIE 9 is a chromium-molybdenum-cobalt hot-work steel. It has outstanding resistance to softening in elevated-temperature service; the cobalt gives this steel its superior heat resistance. Firedie 9 has excellent resistance to thermal shock; in fact, dies can be water cooled durin operation without fear of cracking. Among its many applications are forging dies, hot-extrusion mandrels, hot-shear blades, die-casting dies and hot punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-450. Producer or source: Columbia Tool Steel Company.
Journal Articles
Alloy Digest (1994) 43 (8): Ni-459.
Published: 01 August 1994
... and higher AWE boiler and pressure-vessel design stress allowables than C800 H. The alloy resists stress-corrosion cracking, resists sulfur attack, internal oxidation, scaling and corrosion in thermal processing and heat-transfer applications. The strength is obtained by a selective chemistry range within...
Abstract
View article
PDF
Carlson Alloy C800 AT has superior creep and rupture strengths over long-term exposure to high temperatures and higher ASME boiler and pressure-vessel design stress allowables than C800 H. The alloy resists stress-corrosion cracking, resists sulfur attack, internal oxidation, scaling and corrosion in thermal processing and heat-transfer applications. The strength is obtained by a selective chemistry range within that of Alloy C800 H. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. Filing Code: Ni-459. Producer or source: G.O. Carlson Inc.
Journal Articles
Alloy Digest (1960) 9 (11): SA-106.
Published: 01 November 1960
... UNITEMP-14MV is a silicon-chromium-molybdenum-vanadium alloy steel having high resistance to thermal cracking and heat checking, even in a highly hardened condition, and also has good shock resistance at high hardness levels. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
UNITEMP-14MV is a silicon-chromium-molybdenum-vanadium alloy steel having high resistance to thermal cracking and heat checking, even in a highly hardened condition, and also has good shock resistance at high hardness levels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-106. Producer or source: Cyclops Corporation.
Journal Articles
Alloy Digest (2018) 67 (8): Cu-877.
Published: 01 August 2018
... Alloy CuSn10 is a high-performance copper alloy. The alloy is characterized by good electrical and thermal conductivity and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength...
Abstract
View article
PDF
Alloy CuSn10 is a high-performance copper alloy. The alloy is characterized by good electrical and thermal conductivity and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion and wear resistance as well as forming and joining. Filing Code: Cu-877. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Alloy Digest (2005) 54 (4): SS-922.
Published: 01 April 2005
... improved blending characteristics and reduced cracking potential in welded areas. The material is supplied in the solution-treated condition with a hardness of approximately 321 HB (34 HRC). It may be age hardened with a simple thermal treatment to a hardness of 40+ HRC. This datasheet provides information...
Abstract
View article
PDF
Mar-X is a precipitation-hardening, stainless steel with excellent corrosion resistance for both atmospheric and chemical attack. The heat response characteristics of this grade provide especially good welding characteristics. Absence of hardening in the weld heat-affected zone (HAZ) offers improved blending characteristics and reduced cracking potential in welded areas. The material is supplied in the solution-treated condition with a hardness of approximately 321 HB (34 HRC). It may be age hardened with a simple thermal treatment to a hardness of 40+ HRC. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating, machining, joining, and surface treatment. Filing Code: SS-922. Producer or source: A. Finkl & Sons Company.
Journal Articles
Alloy Digest (2018) 67 (9): Cu-879.
Published: 01 September 2018
... Alloy Cu-ETP (UNS C11000) is a high conductivity pure copper alloy. The alloy is characterized by good electrical and thermal conductivity, and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, and bend strength. It also...
Abstract
View article
PDF
Alloy Cu-ETP (UNS C11000) is a high conductivity pure copper alloy. The alloy is characterized by good electrical and thermal conductivity, and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, and bend strength. It also includes information on forming. Filing Code: Cu-879. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.
Journal Articles
Alloy Digest (1989) 38 (1): Ni-366.
Published: 01 January 1989
... Allegheny Ludlum AL 825 alloy is a nickel-iron-chromium-molybdenum-copper alloy with superior corrosion resistance including stress-corrosion cracking resistance. It is highly ductile from cryogenic to well over 1000 F(538 C) temperatures. It is readily weldable. This datasheet provides...
Abstract
View article
PDF
Allegheny Ludlum AL 825 alloy is a nickel-iron-chromium-molybdenum-copper alloy with superior corrosion resistance including stress-corrosion cracking resistance. It is highly ductile from cryogenic to well over 1000 F(538 C) temperatures. It is readily weldable. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-366. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1995) 44 (7): Ni-483.
Published: 01 July 1995
... SANDVIK SANICRO 70 is an austenitic alloy with good high temperature resistance to carburization and nitridation. The alloy is also very resistant to chloride-ion stress-corrosion cracking and to hydrogen chloride. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
SANDVIK SANICRO 70 is an austenitic alloy with good high temperature resistance to carburization and nitridation. The alloy is also very resistant to chloride-ion stress-corrosion cracking and to hydrogen chloride. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: Ni-483. Producer or source: Sandvik.
Journal Articles
Alloy Digest (2009) 58 (2): TS-677.
Published: 01 February 2009
... machinability physical properties wear resistance thermal properties LSS H11 (Hot-Work Tool Steel) LSS H11 is a hot-work tool steel with excellent impact toughness. It is used where resistance to cracking is needed. LSS is a trademark of Latrobe Specialty Steel Co. Chemical Composition, wt (Typical...
Abstract
View article
PDF
LSS H11 is a hot-work tool steel with excellent impact toughness. It is used where resistance to cracking is needed. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on wear resistance as well as heat treating and machining. Filing Code: TS-677. Producer or source: Latrobe Specialty Steel Company.
Journal Articles
Alloy Digest (1994) 43 (8): Ni-461.
Published: 01 August 1994
... HASTELLOY B-3 ALLOY is a nickel-molybdenum alloy with thermal stability to reduce the deleterious intermetallic precipitates which cause loss of ductility and corrosion resistance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...
Abstract
View article
PDF
HASTELLOY B-3 ALLOY is a nickel-molybdenum alloy with thermal stability to reduce the deleterious intermetallic precipitates which cause loss of ductility and corrosion resistance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance. Filing Code: Ni-461. Producer or source: Haynes International Inc.
Journal Articles
Alloy Digest (2013) 62 (1): SS-1131.
Published: 01 January 2013
... of corrosive media. Stress Corrosion Cracking Resistance. The ATI 444 alloy is practically immune to chloride stress corrosion cracking. The following table compares the cracking resistance of the ATI 444 alloy to conventional austenitic stainless steels in standard boiling test solutions. This testing...
Abstract
View article
PDF
ATI 444 is a low-carbon and low-nitrogen ferritic stainless steel with 18Cr and 2Mo and is often referred to as "18-2". This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-1131. Producer or source: Allegheny Technologies Inc..
Journal Articles
Alloy Digest (2006) 55 (9): SS-975.
Published: 01 September 2006
... corrosion resistance and ductility. The alloy has good resistance to carburization, oxidation, and nitridation and is used in furnace applications. Table 1 Thermal and Electrical Properties Temperature Thermal conductivity Electrical resistivity °C °F W/m . K Btu/(ft . h . °F) . m circular-mil/ft 24 75...
Abstract
View article
PDF
Sandmeyer alloy 330 is a stainless steel with high nickel and chromium content, and with good corrosion resistance and ductility. The alloy has good resistance to carburization, oxidation, and nitridation and is used in furnace applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-975. Producer or source: Sandmeyer Steel Company.
Journal Articles
Alloy Digest (2011) 60 (2): Ni-687.
Published: 01 February 2011
... Sandmeyer alloy 825 is a nickel alloy high in chromium and molybdenum with good corrosion resistance and ductility. The alloy has enough nickel (42%) to be relatively free from chloride-ion stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
Sandmeyer alloy 825 is a nickel alloy high in chromium and molybdenum with good corrosion resistance and ductility. The alloy has enough nickel (42%) to be relatively free from chloride-ion stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-687. Producer or source: Sandmeyer Steel Company.
Journal Articles
Alloy Digest (1972) 21 (7): SS-276.
Published: 01 July 1972
... SANDVIK 3RE60 is an extra-low-carbon stainless steel with a duplex structure consisting of ferrite and austenite. It has high resistance to stress-corrosion cracking, good formability and good weldability. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
SANDVIK 3RE60 is an extra-low-carbon stainless steel with a duplex structure consisting of ferrite and austenite. It has high resistance to stress-corrosion cracking, good formability and good weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-276. Producer or source: Sandvik.
1