Journal Articles
Alloy Digest (1996) 45 (12): SS-664.
Published: 01 December 1996
... for uses involving severe corrosive conditions. The alloy has high strength and good resistance to creep at elevated temperatures. Its many applications include the nuclear, chemical, food, paper, and textile industries. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1983) 32 (2): SS-420.
Published: 01 February 1983
... involving severed corrosive conditions. In addition, Type 316 has high strength and high resistance to creep at elevated temperatures. Its many applications include the nuclear, chemical, food, paper and textile industries. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1981) 30 (2): Cu-412.
Published: 01 February 1981
... Copper Alloy No. C51100 is a copper-tin-phosphorus alloy with relatively high tensile and yield strengths, good ductility and good resistance to corrosion. It can be fabricated by a number of conventional processes. Its many applications include bridge bearing plates, numerous hardware uses...
Journal Articles
Alloy Digest (1984) 33 (12): Al-254.
Published: 01 December 1984
... ALUMINUM 535.0 is a high-purity aluminum alloy of the aluminum-magnesium type. It possesses a high and stable combination of strength, shock resistance and ductility in the cast condition. Among its many applications are armament, hardware, cooking utensils, highway trailers, textile machinery...
Journal Articles
Alloy Digest (1971) 20 (3): SS-252.
Published: 01 March 1971
... ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmagnetic even after severe cold work. Common applications are in the petrochemical, chemical, pulp and paper, textile, food processing, and marine industries...
Journal Articles
Alloy Digest (1979) 28 (11): SS-369.
Published: 01 November 1979
... joinability machinability nuclear applications petrochemical applications physical properties tensile properties textile applications AU 08 ACI Type M-81111 Filing Code: ss-389 Stainless Steel NOVEMBER 1979 BIGISTd - DATA ON WORLD WIDE METALS AND ALLOYS E%&wKdbu -gAtlayr&vNxlr PoatofficeBa823 Uppa Ma...
Journal Articles
Alloy Digest (2001) 50 (12): SS-838.
Published: 01 December 2001
... in flat-rolled products such as sheet, strip, or plate, both hot rolled and cold rolled. Applications: Applications include offshore modules, equipment for the phar- maceutical, synthetic fiber, pulp, paper, and textile industries; tanks and piping of chemical tankers; production, storage, and landbase...
Journal Articles
Alloy Digest (2002) 51 (10): SS-865.
Published: 01 October 2002
... valuable property is high creep strength at elevated temperatures. The alloy has extensive use in marine exterior trim, chemical- and food-process equipment, pharmaceutical and textile-finishing equipment, and in the pulp and paper industry. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1984) 33 (2): SS-439.
Published: 01 February 1984
... to intergranular corrosion. Type 316L is used widely in many industries such as chemical, food, paper, textile, nuclear and oil. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2003) 52 (1): SS-872.
Published: 01 January 2003
... that contribute to intergranular corrosion. Type 316L is used widely in many industries such as chemical, food, paper, textile, nuclear, and oil. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature...
Journal Articles
Alloy Digest (1968) 17 (10): SS-214.
Published: 01 October 1968
... FAGERSTA-R350 is a low-carbon 18-9 type of austenitic stainless steel recommended for welded equipment in the food, chemical, textile and plastic industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1968) 17 (11): SS-216.
Published: 01 November 1968
... FAGERSTA-R320 is a low-carbon 18-9 type of austenitic stainless steel recommended for welded equipment in the food, chemical, textile and plastic industries. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1965) 14 (12): Ni-108.
Published: 01 December 1965
... or cold drawn tubes, welded or welded and cold drawn cubes and strip. Applications: Aircraft exhaust manifolds, cabin heaters, locking wire, parts in turbo-jet engines. Nuclear power reacror heat exchanger tubes, equipment for the plastic, paper and pulp, textile and chemical industries. Furnace parts...
Journal Articles
Alloy Digest (2010) 59 (2): SS-1055.
Published: 01 February 2010
.... Consider CTS alloys for many blade applications including commercial food processing, paper processing, textile, packaging, recycling/refuse, kitchen knives, hand tools, scissors/shears, shaving razors, sport/hunting knives, ice skates, military/defense, law enforcement, salon blades, and various surgical...
Journal Articles
Alloy Digest (1971) 20 (12): Cu-246.
Published: 01 December 1971
... running fits. They are widely used in automotive applications. They are also used in household appliances, paper and textile machinery, printing presses, and laundry machines where the prevention of oil splashing is essential. Forms Available: Bearings. Applications: Fractional horsepower motors...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1324.
Published: 01 August 2020
... conditions. In many cases it eliminates the necessity of annealing weldments except for applications specifying stress relief. Type 304L has slightly lower mechanical properties than Type 304. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2013) 62 (8): SS-1154.
Published: 01 August 2013
... food processing, paper processing, textile, packaging, recycling/refuse, kitchen knives, hand tools, scissors/shears, shaving razors, sport/hunting knives, ice skates, military/defense, law enforcement, salon blades, and various surgical/medical applications. CTS-BD30P ALLOY (Martensitic Stainless...
Journal Articles
Alloy Digest (1991) 40 (8): SA-461.
Published: 01 August 1991
... hour at 1020-1200°F (550- 65O C), furnace cool to 930°F (500°C) then air cool to room temperature. Hot rolled strip, hardened and tempered cold rolled strip. Applications: Quench hardening: Austenitize at 1560°F (SSO C), oil quench. Martempering: Austenitize at 1560°F (85O C), quench into hot bath...
Journal Articles
Alloy Digest (2002) 51 (9): Cu-689.
Published: 01 September 2002
... Wieland-K12 and K14 are copper alloys used for applications needing good electrical conductivity. Weldability of the two alloys is slightly different. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2020) 69 (5): SS-1317.
Published: 01 May 2020
.... Applications Architectural moldings and trim; kitchen equipment; processing equipment for the textile, paper, pharmaceutical, and chemical industries Supplier AK Steel Corporation 9227 Centre Pointe Drive West Chester, Ohio 45069, USA Tel: +1 844 783 3599 (Sales) Web: www.aksteel.com ISSN: 002-614X SS-1317B ...