Alloy Digest (2001) 50 (7): SS-826.
Published: 01 July 2001
... TLS 420 MQ os a mold-quality stainless steel that meets requirements in polishability, corrosion resistance, and wear resistance by special melting and forging practices. Is is used in plastic mold cavities and surgical instruments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2005) 54 (11): Ti-137.
Published: 01 November 2005
... Allvac Titanium 6Al-4V ELI is an alloy with extra-low interstitials to produce cleanliness and consistency in properties. It is used in surgical instruments and implants. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2000) 49 (5): SS-783.
Published: 01 May 2000
... Armco 440A is a martensitic hardenable, high-carbon, high-chromium stainless steel recommended for cutlery, valve parts, and surgical instruments. It is always used in the hardened condition. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1968) 17 (10): SS-215.
Published: 01 October 1968
... AISI Type 440A is a martensitic hardenable high-carbon high chromium stainless steel recommended for cutlery, valve parts, surgical instruments, etc. It is always used in the hardened condition. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1981) 30 (10): SS-394.
Published: 01 October 1981
... CRUCIBLE 420 is a hardenable chromium steel designed particularly for cutlery applications. It is the general-purpose cutlery grade of stainless steel. It is magnetic at all times. Among its many applications are bushings, cutlery, valve trim and dental and surgical instruments. This datasheet...
Journal Articles
Alloy Digest (1982) 31 (10): Ni-279.
Published: 01 October 1982
..., corrosion and oxidation. The applications for Berylco Alloy 42C include cast-to-shape jewelry, surgical instruments, valves, pumps and dental alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1984) 33 (10): SS-452.
Published: 01 October 1984
... be austenitized and quenched to a hardness of Rockwell C56. Its applications include dental and surgical instruments, cutlery and valve parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2017) 66 (4): Ti-159.
Published: 01 April 2017
... ATI 6-4 ELI, also known as Grade 23, is a higher purity grade of ATI Ti-6Al-4V for use in surgical and medical applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1996) 45 (10): SS-657.
Published: 01 October 1996
...: Remanit 4021 is used for parts prone to wear. for example, cutting blades. surgical instruments. die sheets, and brake discs. Producer: Thyssen Stahl AG Krefeld, Germany (02151) 83-01 In USA: Thyssen Specialty Steels, Inc. Carol stream, IL 60188 (708) 682-3900 SS-657B ...
Journal Articles
Alloy Digest (1997) 46 (1): SS-669.
Published: 01 January 1997
... Applications: Producer: Cutlery, kitchen knives, pocket knife blades. meat knives, vemia callipm. surgical instruments, brake discs, and die sheets. Tbyssen StabI AG Krefeld. Germany (02151) 83-01 ISSN: 002-614X In USA: Thyssen specialty steels. Inc. carol strtam. IL 60188 (708) 682-3900 SS-669B ...
Journal Articles
Alloy Digest (1995) 44 (6): SS-596.
Published: 01 June 1995
... fixation devices such as bone plates, screws, and intramedullary nails. This alloy has been used for produc- ing surgical implant devices. The alloy has also been used in surgical instruments where high hardness is not a te- quirement. Producer: Carpenter Technology Corp. Reading, PA 196124662 USA 610-208...
Journal Articles
Alloy Digest (2020) 69 (7): SS-1323.
Published: 01 July 2020
..., scissors; dental instruments, e.g. burrs, curettes, and cutters; medical screwdrivers; surgical instruments Supplier Zapp AG Zapp-Platz 1 40880 Ratingen, Germany Tel: +49 2102 710-0 Web: www.zapp.com All data from Zapp AG except where noted. ISSN: 002-614X SS-1323B ...
Journal Articles
Alloy Digest (2020) 69 (6): SS-1320.
Published: 01 June 2020
..., and curettes; medical screwdrivers; surgical instruments. Supplier Zapp AG Zapp-Platz 1 40880 Ratingen, Germany Tel: +49 2102 710-0 Web: www.zapp.com All data from Zapp AG except where noted. ISSN: 002-614X SS-1320B ...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1326.
Published: 01 August 2020
... % 850 1000 123 145 650 94 10 Hardness of Surgical Instruments Conforming to ISO 71531:2016: 49 55 HRC. Modulus of Elasticity Property Unit Modulus of elasticity GPa (106 psi) At 20 °C (68 °F) Value 215 (31.2) Hot Forming Preheat slowly to 800 °C (1470 °F). Wait for equalization of the temperature. Raise...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-309.
Published: 01 January 1985
.... This alloy also has found uses in industrial instrumentation. jet and rocket engines, surgical instruments and in nuclear reactor vessels and piping. Manufacturer: Nickel alloy producers. ...
Journal Articles
Alloy Digest (2005) 54 (4): SS-925.
Published: 01 April 2005
... are in components that are subject to wear. This includes the entire range of blades for the table and kitchen. Other applications include penknives and surgical instruments, valve parts, seats for oil well pumps, other shears, and wear sur- faces. Producer: Krupp Thyssen Nirosta North America, Inc. Bannockburn, IL...
Journal Articles
Alloy Digest (1973) 22 (4): Sn-3.
Published: 01 April 1973
... castings for dairy machinery, dental appliances, surgical instruments, soda fountain equipment. Alloy 2: Bearings, most widely used tin-base bearing alloy in the automotive field. AJloy 3: Bearings for high-load applications, hardest of standard Tin- Babbit alloys and has greatest load-carrying capacity...
Journal Articles
Alloy Digest (1955) 4 (12): SS-38.
Published: 01 December 1955
..., hot rolled bars and forgings, ground bars, wire and wire rods, cold drawn bars, annealed or tempered suip. Applications: Pivot pins, dental and surgical instruments, cutlery, valve parts, ball bearings, general applications where both strength and ductility are required. Manufacturer: Allegheny Ludlum...
Journal Articles
Alloy Digest (1988) 37 (6): SS-101.
Published: 01 June 1988
..., ground bars. wire and wire rods. annealed strip. Applications: Pivot pins. dental and surgical instruments. cutlery. valve pans, ball bearings. nozzles, hardened steel balls and seats for oil well pumps, wear-resistant textile machlne pans. Manufacturer: Stamless steel mills. ...
Journal Articles
Alloy Digest (1969) 18 (4): SS-223.
Published: 01 April 1969
... and forgings, ground bars, wire and wire rods. Applications Pivot pins, dental and surgical instruments, cutlery, valve parts, baII beatings, molds, pump parts. shear blades, gage blocks, bushings, nozzles, wear resisting parts. Manufacturer: Practically all stainless steel mills. ...