Alloy Digest (2001) 50 (12): Ti-123.
Published: 01 December 2001
... TIMETAL 367 is a Ti-6Al-7Nb medium-strength alpha-beta alloy for surgical implants. The alloy is analogous to TIMETAL 367 6-4 (revised as Ti-6Al-4V, Alloy Digest Ti-66, September 1992), but with niobium as the more biocompatible alloying element. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2005) 54 (1): SS-915.
Published: 01 January 2005
... Equivalents: ASTM 1586 ISO 5832-9 General Characteristics: BioDur 734 is a specialty alloy candidate for fracture fixation devices and implanted orthopedic devices for hips, knees, and other joints that has been developed by the producer for consid- BIODUR® 734 Filing Code: SS-915 Stainless Steel January 2005...
Journal Articles
Alloy Digest (1995) 44 (6): SS-596.
Published: 01 June 1995
... BioDur 316LS stainless steel is a modified version of Type 316L stainless steel to improve corrosion resistance for surgical implant applications. The alloy is vacuum arc remelted. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (2014) 63 (10): SS-1186.
Published: 01 October 2014
... of cleanliness (according to ASTM E45/A or ISO 4967 /A). See Table 2. Products Available: All products in bars, wire, and billet. Applications: Ugipure 4441 can be used to manufacture any surgical implant designed to remain for a long period of time or permanently in the human body: prosthesis, screw, plate, etc...
Journal Articles
Alloy Digest (2005) 54 (11): Ti-137.
Published: 01 November 2005
... Allvac Titanium 6Al-4V ELI is an alloy with extra-low interstitials to produce cleanliness and consistency in properties. It is used in surgical instruments and implants. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2006) 55 (6): Co-111.
Published: 01 June 2006
... successfully in human implant applications in contact with soft tissue and bone for more than a decade. Long-term clinical experience of the use of this material has shown that an acceptable level of biological response can be expected if the alloy is used in appropriate applications. Surgical implants...
Journal Articles
Alloy Digest (2017) 66 (4): Ti-159.
Published: 01 April 2017
...: Billet ASTM F136: Surgical implants UNS R56407 General Characteristics: ATI Ti-6Al-4V-ELI, Grade 23 alloy (Extra Low Interstitials, UNS R56407) is a higher purity grade of ATI Ti-6Al-4V alloy. This grade has lower oxygen, carbon, and iron content. This titanium grade is produced by vacuum arc primary...
Journal Articles
Alloy Digest (2006) 55 (7): Ti-139.
Published: 01 July 2006
... sensitivity and forming characteristics. Product Forms Available: Bar and billet Applications: This alloy was developed for medical devices and surgical implants such as total hip replacement systems, fracture fixation plates, intermedullary rods and nails, spinal devices, screws, and wires. Producer: ATI...
Journal Articles
Alloy Digest (2002) 51 (7): Ti-129.
Published: 01 July 2002
... (powder), ASTM F 136 (wrought surgical implants), ASTM F 620 (forgings surgical implants), AWS A5.16-70 (weld filler wire rod) General Characteristics: Ti 6Al-4V ELI is a higher-purity (extra-low interstitial) version of Ti 6Al- 4V, with lower specified limits on iron and the interstitial elements car...
Journal Articles
Alloy Digest (2006) 55 (12): Co-115.
Published: 01 December 2006
... numerous applications in watch making, surgical implants, metrology, electronics, and aeronautical engineering. Other applications include springs for watch motors, shaped springs such as helical springs, flexible couplings, electrical and electronic apparatus, equipment for the chemical and oil and gas...
Journal Articles
Alloy Digest (1988) 37 (6): Ta-10.
Published: 01 June 1988
... chemicals Temperature Rate OC lO+Wyr 20 weight % HCl 190 2.29 200 3.30 220 22.90 37 weight B HCl 100 1.52 110 4.06 120 9.14 encountered in industry. It may be used as surgical implants without harm to the human body. It resists liquid metal attack. TANTALUM is attacked slowly by strong alkalies and more...
Journal Articles
Alloy Digest (2021) 70 (6): Co-137.
Published: 01 June 2021
.... Ugitech UGI Phynox is also characterized by excellent Chromium resistance to stress-corrosion cracking and hydrogen embrittle- Nickel 0.015 0.015 ment. Its perfect passivity with human tissues explains why it has Molybdenum been used for more than twenty five years in surgical implants. Beryllium 0.015...
Journal Articles
Alloy Digest (2005) 54 (7): Ti-136.
Published: 01 July 2005
.... Lemons, Ed., ASTM, 1966, p 64 2. J. Disegi, Wrought Titanium-15% Molybdenum Implant Material, Synthes (USA), Paoli, PA Oct 2003 3. IMI Titanium 205, Alloy Data Sheet, IMI Titanium Limited, Birmingham, England 4. S. Steinemann et al., Beta-Titanium Alloy for Surgical Implants, Seventh World Conference...
Journal Articles
Alloy Digest (2011) 60 (12): Co-24.
Published: 01 December 2011
... temperature and time, it perforated at the crevice site location. The alloy is acceptable for use in sour environments by qualifying with the NACE MR0175 sulfide cracking test; max hardness HRC is 35. The alloy also has been tested for pitting/crevice corrosion of surgical implants by the ASTM test F-746 (2...
Journal Articles
Alloy Digest (1991) 40 (2): Co-61.
Published: 01 February 1991
... (solution treated and cold drawn bars) AhIS 5845 (solution treated, cold drawn and aged bars) AMS 7468 (bolts and screws, forged head, roll threaded after aging) ANS/ASTM F562-78 (surgical implant applications) NACE Standard MR-01-75 (sulfide stress cracking resistant material for oil field equipment...
Journal Articles
Alloy Digest (2020) 69 (4): Ti-165.
Published: 01 April 2020
...) Grade 1 EN ISO 5832-2:2018(c) Grade 1 (a) For titanium and titanium alloy plate, sheet, and strip. (b) For titanium and tita- nium alloy wire. (c) For unalloyed titanium for surgical implant applications Table 1 Tensile properties at room temperature Tensile strength, min 0.2% proof strength Elongation...
Journal Articles
Alloy Digest (1972) 21 (11): Ta-2.
Published: 01 November 1972
..., foil, tubing (seamless and welded and redrawn), and powder (several grades available). Applications: Chemical process equipment including heating and cool- ing coils, heat exchangers, condensers, reaction vessels; electronic industry applications such as rectifiers, capac- itors and cathodes; surgical...
Journal Articles
Alloy Digest (1981) 30 (9): SS-392.
Published: 01 September 1981
... and scales at approximately 1650OF. Forms Available: Bar, rod, wire and forging billets. Applications: Typical applications for CRUCIBLE 316L comprise screw- machine products, food-processing equipment, photographic developing equipment, machined shafts, pulphandling equip ment, surgical implants, valves...
Journal Articles
Alloy Digest (2021) 70 (2): Co-133.
Published: 01 February 2021
..., springs, and surgical implants. A maximum service Hot forming information sourced from CarTech MP35N, temperature of 400 °C (750 °F) is suggested. ANSI/NACE Carpenter Technology Corporation. MR0175/ISO 15156-3:2015 (Tables A.38 and A.39) lists UNS R30035 as suitable for components without restriction...
Journal Articles
Alloy Digest (2020) 69 (12): Ti-173.
Published: 01 December 2020
..., sheet, forging, welding filler metal. Applications Aerospace applications, automotive applications, jewelry, offshore applications, sonotrodes, surgical implants. Supplier Zapp AG Zapp-Platz 1 40880 Ratingen, Germany Tel: +49 2102 710 0 Web: www.zapp.com All data from Zapp AG except where noted. ISSN...