Alloy Digest (1952) 1 (3): TS-3.
Published: 01 November 1952
... BETHLEHEM HOT WORK 8 alloy is a hot-work tool steel having high wear resistance in the higher range of operating temperatures. It also has high resistance to surface wash and heat-checking. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1986) 35 (10): TS-15.
Published: 01 October 1986
... CASCADE is a precipitation-hardening steel which is very popular as a mold steel for injection molding of thermoplastics. It is also an excellent choice for many zinc die-casting dies because of its resistance to heat checking and wash. A further wide usage for Cascade is as a holding-block...
Journal Articles
Alloy Digest (1995) 44 (12): SS-628.
Published: 01 December 1995
... resistance making the alloy useful in washing machines and hot water boilers. @REMANIT is a trademark of Thyssen Stahl AG. Chemical Composition, Wt. Min. Carbon - Chromium 16.0 Titanium 7x%C , %: Max. 0.05 18.0 1.2 Physical Properties: Density, kg/dm3 Thermal conductivity at 20°C, W/m-K Specific heat...
Journal Articles
Alloy Digest (1964) 13 (3): Cu-139.
Published: 01 March 1964
..., elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: Cu-139. Producer or source: Mallory Metallurgical Company. Producer or Source: Mallory Metallurgical Company Copyright © ASM...
Journal Articles
Alloy Digest (2000) 49 (10): Cu-29.
Published: 01 October 2000
.... This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CU-29. Producer or source: CMW Inc...
Journal Articles
Alloy Digest (1999) 48 (11): TS-569.
Published: 01 November 1999
... wear or washing will result. One means of guarding against this possibility is to mark the die surface with a Tempilstik designed to melt a particular temperature before starting the preheating process. Any means of die preheating that develops temperatures on the surface that exceed the tempering...
Journal Articles
Alloy Digest (1958) 7 (2): Cu-59.
Published: 01 February 1958
... of sulphuric acid and water at 135-165 deg F. for lo-30 minutes, rinse in cold water, wash in hot neutralizing bath of t&odium-phosphare heated to approximately 150 deg F. Cleaning and Brightening: If a bright clean surface is desired after hardening in an air furnace, the following steps should be observed...
Journal Articles
Alloy Digest (1964) 13 (3): SS-153.
Published: 01 March 1964
.... It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-153. Producer or source: Armco Inc., Eastern Steel Division. Producer or Source: Armco Inc., Eastern Steel Division Copyright © ASM International® 1996...
Journal Articles
Alloy Digest (2000) 49 (3): TS-574.
Published: 01 March 2000
... treating techniques provide outstanding qualities and exceptionally uniform hard- ness throughout. Cuprodie resists abrasion and heat checking and washing and offers excellent machinability. No oil should be used to lubricate Cuprodie dies, since this usually results in poor performance. When broken...
Journal Articles
Alloy Digest (2007) 56 (1): SS-984.
Published: 01 January 2007
... stainless and Types 410, 420, and 440 in 5% neutral salt spray for 200 h (test method ASTM B 117). For maximum corrosion resistance, parts must be free of scale, foreign particles, free iron, and surface imperfections than can trap foreign material and contribute to pitting and crevice corrosion, especially...
Journal Articles
Alloy Digest (1959) 8 (3): SS-85.
Published: 01 March 1959
... as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-85. Producer or source: Samuel Fox & Company Ltd, Stocksbridge Works. Producer or Source: Samuel Fox & Company Ltd, Stocksbridge Works...
Journal Articles
Alloy Digest (1956) 5 (8): SS-46.
Published: 01 August 1956
... information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-46. Producer or source: Republic Steel Corporation. Producer or Source: Republic Steel Corporation Copyright © ASM International® 1996 1996...
Journal Articles
Alloy Digest (2020) 69 (9): SS-1327.
Published: 01 September 2020
... the surface to prevent superficial stains. Stress-Corrosion Cracking. Like most stainless steels, ACX 490 exhibits good resistance to stress-corrosion cracking. Oxidation Resistance The relatively high chromium content of ACX 490 contributes to its good oxidation resistance. ACX 490 exhibits good oxidation...
Journal Articles
Alloy Digest (1965) 14 (6): SS-170.
Published: 01 June 1965
..., elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-170. Producer or source: Carpenter. Producer or Source: Carpenter Copyright © ASM...
Journal Articles
Alloy Digest (1976) 25 (9): SA-324.
Published: 01 September 1976
... are being handled. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-324. Producer or source...
Journal Articles
Alloy Digest (1978) 27 (2): Zn-33.
Published: 01 February 1978
... provides information on composition, physical properties, hardness, tensile properties, and shear and bend strength It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zn-33. Producer or source: Ball Corporation...
Journal Articles
Alloy Digest (1996) 45 (11): SS-659.
Published: 01 November 1996
... Remanit 4511 was developed as a modification of Type 430 to improve its aqueous corrosion resistance. Due to its composition, that is, an addition of niobium (columbium), the alloy maintains better corrosion resistance in welds and heat-affected zone areas than does Type 430. This datasheet...
Journal Articles
Alloy Digest (1961) 10 (8): Al-106.
Published: 01 August 1961
... properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-106. Producer or source: Aluminum Company of Canada Ltd. Producer or Source: Aluminum Company of Canada Ltd...
Journal Articles
Alloy Digest (1964) 13 (11): SS-162.
Published: 01 November 1964
..., and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-162. Producer or source: Stainless steel mills...
Journal Articles
Alloy Digest (1955) 4 (6): SS-31.
Published: 01 June 1955
... on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-31. Producer or source: Cyclops Corporation. Producer or Source: Cyclops Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion...