Journal Articles
Alloy Digest (2005) 54 (1): TS-611.
Published: 01 January 2005
... CLC 1.2311 is a prehardened mold steel optimized for martensite and surface finish quality. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low...
Journal Articles
Alloy Digest (2012) 61 (3): SA-645.
Published: 01 March 2012
..., and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as forming, heat treating, and joining. Filing Code: SA-645. Producer or source: Dillinger Hütte GTS. Producer or Source: Dillinger Hütte GTS Copyright © ASM International® 2012 2012 ASM...
Journal Articles
Alloy Digest (2005) 54 (2): SS-918.
Published: 01 February 2005
... resistance and surface qualities as well as heat treating and surface treatment. Filing Code: SS-918. Producer or source: Böhler-Uddeholm North America. Producer or Source: Böhler-Uddeholm North America Copyright © ASM International® 2005 2005 ASM International chemical composition corrosion...
Journal Articles
Alloy Digest (2008) 57 (7): Ni-664.
Published: 01 July 2008
... on corrosion resistance and surface qualities as well as heat treating and surface treatment. Filing Code: Ni-664. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 2008 2008 ASM International abrasion resistance chemical...
Journal Articles
Alloy Digest (2017) 66 (12): SA-807.
Published: 01 December 2017
... temperatures of up to approximately 500–550 deg C (932–1022 deg F). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as casting and forming. Filing Code: SA-807. Producer or source...
Journal Articles
Alloy Digest (2017) 66 (5): SA-785.
Published: 01 May 2017
... temperatures of up to approximately 500-550 deg C (932-1022 deg F). This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as casting. Filing Code: SA-785. Producer or source: Schmolz + Bickenbach Group...
Journal Articles
Alloy Digest (2017) 66 (6): SA-787.
Published: 01 June 2017
... temperatures of up to approximately 500–550 deg C (932–1022 deg F). This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on surface qualities as well as casting and forming. Filing Code: SA-787. Producer or source: Schmolz + Bickenbach...
Journal Articles
Alloy Digest (2017) 66 (7): SA-791.
Published: 01 July 2017
... temperatures of up to approximately 500–550 deg C (932–1022 deg F). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as casting and forming. Filing Code: SA-791. Producer or source...
Journal Articles
Alloy Digest (2017) 66 (8): SA-795.
Published: 01 August 2017
... of up to approximately 500–550 deg C (932–1022 deg F). This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as casting and forming. Filing Code: SA-795. Producer or source: Schmolz + Bickenbach...
Journal Articles
Alloy Digest (2017) 66 (9): SA-797.
Published: 01 September 2017
... of up to approximately 500–550 deg C (932–1022 deg F). This datasheet provides information on composition and tensile properties. It also includes information on surface qualities as well as casting and forming. Filing Code: SA-797. Producer or source: Schmolz + Bickenbach Group. Producer or Source...
Journal Articles
Alloy Digest (2017) 66 (10): SA-802.
Published: 01 October 2017
... temperatures of up to approximately 500–550 deg C (932–1022 deg F). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as casting and forming. Filing Code: SA-802. Producer or source...
Journal Articles
Alloy Digest (2017) 66 (11): SA-806.
Published: 01 November 2017
... temperatures of up to approximately 500–550 deg C (932–1022 deg F). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on surface qualities as well as casting. Filing Code: SA-806. Producer or source: Schmolz...
Journal Articles
Alloy Digest (2011) 60 (8): CS-166.
Published: 01 August 2011
... on surface qualities as well as forming, joining, and surface treatment. Filing Code: CS-166. Producer or source: SSAB Hardox Corporation. Producer or Source: SSAB Hardox Corporation Copyright © ASM International® 2011 2011 ASM International bend strength chemical composition DOGAL 600 CP...
Journal Articles
Alloy Digest (2011) 60 (10): CS-167.
Published: 01 October 2011
..., and tensile properties. It also includes information on surface qualities as well as forming, heat treating, joining, and surface treatment. Filing Code: CS-167. Producer or source: SSAB Swedish Steel Inc.. Producer or Source: SSAB Swedish Steel Inc. Copyright © ASM International® 2011 2011 ASM...
Journal Articles
Alloy Digest (2012) 61 (1): SA-641.
Published: 01 January 2012
... provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on wear resistance and surface qualities as well as forming, heat treating, machining, and joining. Filing Code: SA-641. Producer or source: Dillinger Hütte...
Journal Articles
Alloy Digest (2020) 69 (7): TS-796.
Published: 01 July 2020
...) with brief exposures up to 595 °C (1100 °F). This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance and surface qualities as well as heat treating, machining, joining, and surface treatment. Filing Code...
Journal Articles
Alloy Digest (2009) 58 (6): Ni-670.
Published: 01 June 2009
... Colmonoy 455L is a nickel-base hard-surfacing composite powder for high abrasion and moderate impact resistance. This datasheet provides information on composition, physical properties, and hardness. It also includes information on surface qualities as well as powder metal forms. Filing Code: Ni...
Journal Articles
Alloy Digest (2002) 51 (1): SS-843.
Published: 01 January 2002
... be ground. This datasheet provides information on composition, physical properties, and hardness. It also includes information on surface qualities as well as joining. Filing Code: SS-843. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM...
Journal Articles
Alloy Digest (2010) 59 (4): TS-689.
Published: 01 April 2010
... Nimax is a low-carbon plastic mold steel delivered at a hardness of ~40 HRC. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on surface qualities...
Journal Articles
Alloy Digest (2010) 59 (10): TS-693.
Published: 01 October 2010
... CPM REX M3-1 is a modification of M3-2 with lower carbon and vanadium. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on surface qualities as well as forming, heat treating, and machining. Filing Code: TS-693...