Alloy Digest (1994) 43 (6): SA-477.
Published: 01 June 1994
... SANDVIK 310/T22 is a composite tube consisting of Type 310 stainless steel for corrosion resistance on the outside diameter and having T22 (21/4 Cr-1Mo) to A213 on the inside diameter to act as the superheater tube and design load carrier. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (3): SA-509.
Published: 01 March 2001
... V and M T/P92 is a ferritic alloy with improved high-temperature strength and creep behaviors compared to those of other ferritic steel alloys. Applications include both superheater tubes and main steam piping in advanced boilers. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (12): SS-232.
Published: 01 December 1969
... SICROMO-5S is a low-carbon, 5% chromium alloy steel recommended for applications in which a high degree of surface stability under oxidizing conditions is required for temperatures up to 1500 F. It is used in air prehealer tubes, recuperater and superheater tubes. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (12): SS-248.
Published: 01 December 1970
... SANDVIK 12R72HV is an austenitic chromium-nickel-molybdenum-titanium stainless steel suitable for metal temperature up to about 308 in the power industry and the petrochemical industry. Typical applications are superheater tubes and hydrocarbon crackers. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (12): SA-220.
Published: 01 December 1967
... ESSHETE CRM2 is a low alloy corrosion and oxidation resistant steel suitable for moderately high 1100 F (593 C) temperature applications such as steam piping and superheater tubes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (7): SS-934.
Published: 01 July 2005
... for precipitation strengthening in order to improve the long-term creep rupture strength. Allowable stress for Tempaloy AA-1 at 650 °C (1200 °F) for 105 h is 1.5 times that of conventional TP321H and TP347H. Tempaloy AA-1 is suitable as a material for superheater tubes and reheater tubes in boilers. Because small...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (2): SA-95.
Published: 01 February 1960
... petroleum products. ASTM A 199.111 ASThf A 200.Tl1 ASTM A 213.111 AST M A 335.P11 General Characteristics: DM steel offers unusually high strength at elevated tempera- tures, good stability up to 1200°F, and fairly good corrosion and oxidation resistance. It is recommended for superheater tubing and steam...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (11): SS-1022.
Published: 01 November 2008
... DMV 347 HFG is produced as seamless tubing suitable as a replacement for old reheater and superheater boiler tubes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (8): Ni-572.
Published: 01 August 2001
... Sandvik Sanicro 63 was developed specifically for use as outer cladding of composite tubes in service as superheater materials for waste-derived fuel plants. It is a modification of UNS N06625. Typical inner components of the composite tubes are Sandvik 4L7 and Sandvik HT8. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (11): Ni-692.
Published: 01 November 2011
... DMV 617 Modified is a superheater boiler tubing grade with strength and corrosion resistance for ultra supercritical boilers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (10): SS-1019.
Published: 01 October 2008
... DMV 304 HCu is produced as seamless tubing and designed for application as superheaters. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (1): Ni-535.
Published: 01 January 1998
... Sandvik Sanicro 65 was developed specifically for use as outer cladding of composite tubes in service as superheater materials for waste derived fuel plants. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (7): SA-464.
Published: 01 July 1993
... HCM 12A is a ferritic steel with high strength that was developed for use in superheater and reheater tubes and is also used in large diameter thick wall pipe for headers in power generation boilers. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (9): SS-831.
Published: 01 September 2001
... Sandvik Sanicro 28 composite tube is used in services as superheater material for waste-derived fuel plants. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (9): Ni-544.
Published: 01 September 1998
... is readily weldable, and welding products are available with strength and corrosion-resistance properties comparable with those of the tubing. Cold-formed bends, such as those required for superheater pendants, have been produced in MCOCLAD 671/8OOHT. Press bending has yielded good results with sand-filled...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (10): Ni-180.
Published: 01 October 1972
... resistance, makes the alloy useful for a variety of high temperature applications. Forms Available: Plate, sheet, tubing, rod, bar. Applications: Superheater tube shields, soot-blower tubes, boiler splash plates, boiler tube separators and hangers, high-temperature recuperators, incinerators for waste fumes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (10): SS-766.
Published: 01 October 1999
..., steam superheaters, tube supports, hangers, and tube sheets. Producer: Kubota Metal Corporation, Fahramet Division 25 Commerce Road, P.O. Box 1700 Orillia, Ontario, Canada, L3V 6L6 (705) 325-2781 (705) 325-5887 (fax) ISSN: 002-614X SS-766B Table 4 Carburization Resistance Alloy grade Weight gain, mg/mm2...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (9): SA-799.
Published: 01 September 2017
... properties up to 650 °C (1202 °F) Maximum design temperature is 620 °C (1148 °F) Product Forms Available: Fitting, pipe, and tubing Applications: Power plant headers and superheater tubing Producer: Vallourec Tubes France 92660 Boulogne-Billancourt, France Tel: +33-1-4909-3640 www.vallourec.com ISSN: 002...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (1): SA-776.
Published: 01 January 2017
... are those from 20 °C (68 °F) to indicated temperature. DOI: 10.31399/asm.ad.sa0776 General Characteristics: The producer has developed a new creep enhanced ferritic steel (CEFS), Save 12AD for superheater tubes, reheater tubes, large diameter and thick-wall pipes and forgings, for conventional and advanced...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (6): Ni-663.
Published: 01 June 2008
... KHR45A 0.94 UCX 0.40 Oxidation resistance to cyclic oxidation at 1150 °C (2100 °F) Applications: Ethylene pyrolysis tubes and fittings, cracking furnace coils, superheater tubes, direct-reduction furnace assemblies. Producer: Kubota Metal Corporation, Fahramet Division Orillia, Ontario, Canada L3V 6L6...