1-20 of 1565 Search Results for

sulfur content

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1957) 6 (8): TS-61.
Published: 01 August 1957
... MOTUNG 652 is an intermediate molybdenum-tungsten type of high-speed steel conforming to the M-2 analysis. It is available with normal sulfur content or with high sulfur for free machining properties. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2022) 71 (9): SS-1351.
Published: 01 September 2022
... to below that of type 304 austenitic stainless steel. Compared with the other austenitic grades, Atlas 303 has excellent toughness, although its sulfur content reduces its toughness slightly. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2003) 52 (4): SS-881.
Published: 01 April 2003
... Nirosta 4427 is a molybdenum, 18-11-3 type austenitic stainless steel with molybdenum content at the high end of the standard range for type 316 stainless steel. With a higher sulfur content, this grade is specifically aimed at machining. The alloy is often referred to as Type 316F in the United...
Journal Articles
Alloy Digest (2017) 66 (4): SS-1261.
Published: 01 April 2017
... Superplast is a plastic mold steel with a high chromium content for corrosion resistance and a high sulfur content for good machinability. This datasheet provides information on composition, microstructure, hardness, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2002) 51 (5): SS-854.
Published: 01 May 2002
... NIROSTA 4305 is an austenitic alloy with a high sulfur content. The alloy is typically used for machined parts. As with other austenitic steels, it is necessary to machine with good-quality high-speed steel or tungsten carbide tools. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1974) 23 (2): SA-301.
Published: 01 February 1974
... CRUCIBLE HOLDER BLOCK is a medium-carbon chromium-molybdenum steel which affords superior machinability because of its sulfur content. It is used in such applications as holders or backers for forging dies and frames for plastic molds. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2007) 56 (9): SA-573.
Published: 01 September 2007
... Ovako 42CrMo4 is a quenched-and-tempered steel with high strength and good toughness. The alloy is also available with increased sulfur content to improve machinability. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1979) 28 (9): SA-364.
Published: 01 September 1979
... CABOT ESR 4330 Mod is a modified 4330 alloy steel produced by electric-furnace, melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility...
Journal Articles
Alloy Digest (1983) 32 (9): SA-393.
Published: 01 September 1983
... INGERSOLL-RAND ESR HY 140 is a 5Ni-Cr-Mo-V alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility...
Journal Articles
Alloy Digest (1979) 28 (4): SA-358.
Published: 01 April 1979
... Cabot ESR HY 140 is a 5Ni-Cr-Mo-V alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness...
Journal Articles
Alloy Digest (1980) 29 (4): SA-371.
Published: 01 April 1980
... CABOT ESR 4140 is a chromium-molybdenum alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness...
Journal Articles
Alloy Digest (1983) 32 (4): SA-388.
Published: 01 April 1983
... INGERSOLL-RAND OILFIELD PRODUCTS ESR 4330 MOD is a modified 4330 alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting with the use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved...
Journal Articles
Alloy Digest (1983) 32 (6): SA-391.
Published: 01 June 1983
... INGERSOLL-RAND OILFIELD PRODUCTS ESR 4140 is a chromium-molybdenum alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness. ESR 4140...
Journal Articles
Alloy Digest (1987) 36 (4): TS-474.
Published: 01 April 1987
... CPM REX M3HCHS is produced by the Crucible Particle Metallurgy process. Structurally it is characterized by its fine and uniform carbide and sulfide particle size. The control of manganese sulfide particle size and distribution permits increasing the sulfur content to at least double that found...
Journal Articles
Alloy Digest (2011) 60 (7): SS-1098.
Published: 01 July 2011
..., % 50 Reduction in area, % 55 Hardness, max, HB (HRB) 160 (92) Heat Treatment: Heat Carlson Alloy 303 to 1038 to 1121 ºC (1900 to 2050 ºF) and water quench. Workability: Hot Working. The high sulfur content, added for machinability, is detrimental to hot workability. If hot forming is necessary, AISI...
Journal Articles
Alloy Digest (2009) 58 (10): SA-609.
Published: 01 October 2009
... hardenability and strength control. Can be delivered as rolled, annealed normalized, or quenched and tempered. Ovako Designations: 253A. Standard variant with high hardenability and controlled sulfur content for improved machinability. 253F. Variant with reduced carbon range for reduced core hardness after...
Journal Articles
Alloy Digest (2020) 69 (6): SS-1320.
Published: 01 June 2020
..., and the relevant semifinished products, a maximum content of 0.030% sulfur applies. Particular ranges of sulfur content may provide improvement of particular properties. For machinability a controlled sulfur content of 0.015% to 0.030% is recommended and permitted. For weldability, a controlled sulfur content...
Journal Articles
Alloy Digest (2000) 49 (2): SS-776.
Published: 01 February 2000
... produce buckling and residual stresses in the weld. As a result, it is essential to properly brace the structures during welding. In arc welding use the shielded-arc type elec- trodes of the same composition. The higher sulfur content of MINIMISER 316/316L increases the susceptibility of the al- loy...
Journal Articles
Alloy Digest (2000) 49 (8): SS-800.
Published: 01 August 2000
...: Annealing. RAM 303 should be heated to a minimum of 1038 Hardening. RAM 303 cannot be hardened by heat treatment. Workability: Hot Working. The high sulfur content, added for machinability, is detrimental to hot workability. If hot forming is necessary, RAM 304 or an intermediate sulfur level alloy should...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1326.
Published: 01 August 2020
..., and the relevant semi-finished products, a maximum content of 0.030% sulfur applies. Particular ranges of sulfur content may provide improvement of particular properties. For machinability a controlled sulfur content of 0.015 0.030% is recommended. For weldability, a controlled sulfur content of 0.008 0.030...