Alloy Digest (1958) 7 (8): SS-77.
Published: 01 August 1958
... TYPE HD is a heat resistant 28% chromium alloy recommended for high oxidation resistance in sulfur atmospheres. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (1959) 8 (8): SS-92.
Published: 01 August 1959
... TYPE HC is a heat resistant 28% chromium alloy steel containing up to 4% nickel. It is recommended for oxidation resistance in high sulfur atmospheres. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also...
Journal Articles
Alloy Digest (2015) 64 (2): SA-718.
Published: 01 February 2015
... 0.025 Sulfur 0.020 Aluminum 0.02 Copper 0.25 0.50 Nickel 0.50 Chromium 0.40 0.70 Niobium 0.040 Iron bal CEV, plate thickness 30 mm (1.2 in % 0.29 CEV, plate thickness 60 mm (2.4 in % 0.31 CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15; CET = C + (Mn+Mo)/10 + (Cr+Cu)/20 + Ni/40 In addition, the...
Journal Articles
Alloy Digest (2015) 64 (3): SA-721.
Published: 01 March 2015
... 0.50 1.25 Phosphorus 0.025 Sulfur 0.010 Aluminum 0.020 Copper 0.30 0.50 Nickel 0.50 Chromium 0.40 0.70 Niobium 0.015 0.05 Molybdenum 0.10 Zirconium 0.05 Iron bal CEV, % Plate thickness, 30 mm (1.2 in.) 0.46 Plate thickness, 60 mm (2.4 in.) 0.48 CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15...
Journal Articles
Alloy Digest (2015) 64 (4): SA-724.
Published: 01 April 2015
... 0.50 Manganese 1.40 Phosphorus 0.020 Sulfur 0.003 Aluminum 0.020 Copper 0.25 0.40 Nickel 0.50 Chromium 0.40 0.80 Niobium 0.05 Molybdenum 0.08 Vanadium 0.08 Titanium 0.02 Nitrogen 0.01 Iron bal CEV, typical, % 0.47 CEV, maximum, % 0.49 CET, typical, % 0.28 CEV = C + Mn/6 + (Cr+Mo+V...
Journal Articles
Alloy Digest (1986) 35 (8): Ni-338.
Published: 01 August 1986
... steel and it has good toughness. It can be used from sub-zero to as high 800 F (1000 F in sulfur-free oxidizing environments). Its corrosion resistance (including virtual immunity to stress-corrosion cracking in chloride environments) is very good in reducing conditions but not in oxidizing atmosphere...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1039.
Published: 01 August 2009
... Nikrothal 30 is one of a family of austenitic alloys used in resistance wires for electric heating. It has good ductility after use, good corrosion resistance except in sulfur-containing atmospheres and certain controlled atmospheres, and excellent weldability. This datasheet provides information...
Journal Articles
Alloy Digest (1995) 44 (1): Ni-474.
Published: 01 January 1995
... CARLSON ALLOYS C 800/800H have good strength plus excellent resistance to oxidation and carburization at elevated temperatures. Fair degree of resistance to stress-corrosion cracking. They resist sulfur attack, internal oxidation, scaling and corrosion in industrial atmospheres. This datasheet...
Journal Articles
Alloy Digest (2001) 50 (11): Ti-122.
Published: 01 November 2001
... marine atmospheres. It is also resistant to attack by hot metallic chloride solutions, sodium and potassium hypochlorite, and chlorine dioxide. The metal is resistant to attack by hot nitric acid at concentrations up to 80% and is not attacked by sulfuric acid. TIMETAL is a registered trademark of TIMET...
Journal Articles
Alloy Digest (1997) 46 (2): Ni-521.
Published: 01 February 1997
... Nicrofer 6023 is a nickel-chromium-iron alloy containing small quantities of aluminum. It has excellent resistance to oxidation at high temperatures, good resistance in oxidizing sulfur-bearing atmospheres, and good resistance to carburizing conditions. The alloy has good mechanical properties at...
Journal Articles
Alloy Digest (1985) 34 (5): Ni-314.
Published: 01 May 1985
... NICROFER 6023 is a nickel-chromium-iron alloy containing small quantities of aluminum. It has excellent resistance to oxidation at high temperatures, good resistance in oxidizing sulfur-bearing atmospheres and good resistance to carburizing conditions. The alloy has good mechanical properties at...
Journal Articles
Alloy Digest (1985) 34 (8): Ni-319.
Published: 01 August 1985
... temperatures; also, it can be used at temperatures to 800 F(427 C) and as high as 1000 F(538 C) in sulfur-free oxidizing atmospheres. Alloy 400 is used widely in many fields, particularly marine and chemical processing. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1963) 12 (9): Ni-86.
Published: 01 September 1963
... Corronel 230 is a nickel-chromium alloy having high resistance to corrosion by hot nitric acid and excellent resistance to attack at elevated temperatures from oxidizing and reducing atmospheres high in sulfur. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1965) 14 (7): SS-171.
Published: 01 July 1965
... Type CC-50 is an iron-chromium casting alloy having high corrosion resistance. It is recommended for furnace equipment, valve bodies and for extremely corrosive sulfur-bearing atmospheres. This datasheet provides information on composition, physical properties, hardness, and tensile properties as...
Journal Articles
Alloy Digest (1988) 37 (11): Co-84.
Published: 01 November 1988
... HAYNES ALLOY No. 150 is a cobalt-base alloy with excellent thermal shock resistance. It has a higher melting point than other cobalt-and nickel-base high-temperature alloys and resists high-temperature corrosion in air and air-sulfur dioxide atmospheres. This datasheet provides information on...
Journal Articles
Alloy Digest (1981) 30 (3): Ni-266.
Published: 01 March 1981
... pat yea. DOI: 10.31399/asm.ad.ni0266 Copyright © ASM International® 1996 Heat Treatment: INCONEL alloy 690, like other nickel alloys, should be clean before it is heated and should be heated in a low-sulfur atmos- phere. Furnace atmospheres for open heating should also be slightly reducing to prevent...
Journal Articles
Alloy Digest (1982) 31 (8): Cu-443.
Published: 01 August 1982
... Copper Alloy No. C60800 is a medium-strength aluminum bronze containing nominally 95% copper and 5% aluminum. It has good resistance to atmospheric corrosion and its resists attack by nonoxidizing mineral acids such as sulfuric, hydrochloric and phosphoric. It is used widely for tubing in such...
Journal Articles
Alloy Digest (2017) 66 (2): TS-739.
Published: 01 February 2017
... Böhler (or Boehler) S692 Microclean is a high sulfur, high carbon PM M4, with higher manganese and 0.22 sulfur for improved machining characteristics, and is available in rounds greater than or equal to 64.16 mm (2.562 in.) diameter. S693 Microclean is the low sulfur version of high carbon PM M4...
Journal Articles
Alloy Digest (1957) 6 (8): TS-61.
Published: 01 August 1957
... MOTUNG 652 is an intermediate molybdenum-tungsten type of high-speed steel conforming to the M-2 analysis. It is available with normal sulfur content or with high sulfur for free machining properties. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (1994) 43 (4): SS-565.
Published: 01 April 1994
... URANUS B6 is a high-alloy austenitic stainless steel with low carbon content. It was originally developed and used for many years to resist corrosion in dilute sulfuric acid. It is one of the best stainless steels for very aggressive chemical environments, in particular sulfuric and phosphoric...