Journal Articles
Alloy Digest (2021) 70 (7): Al-478.
Published: 01 July 2021
... Alcoa 560 is a proprietary, non-heat-treatable, aluminum-magnesium-manganese alloy developed by Alcoa in the late 1990s for high pressure die cast structural components. This alloy develops the required strength and toughness in the as-cast condition, thus eliminating or minimizing numerous...
Journal Articles
Alloy Digest (1984) 33 (3): SA-398.
Published: 01 March 1984
... range of highly-stressed, fracture-critical applications such as airframe structural components, landing gear components and light armor plate. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2022) 71 (7): SS-1349.
Published: 01 July 2022
... sufficient ductility in conditions up to 1/2 Hard and allows it to be roll or brake formed into aircraft, architectural, and particularly rail car structural components. However, 3/4 Hard to Full Hard tempers should be used whenever high wear resistance and spring features are required in components...
Journal Articles
Alloy Digest (2012) 61 (2): SA-643.
Published: 01 February 2012
... RUUKKI RAEX 300 (typical yield strength 900 MPa) is part of the Raex family of high-strength and wear-resistant steels with favorable hardness and impact toughness to extend life and decrease wear in structural components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2012) 61 (3): SA-646.
Published: 01 March 2012
... RUUKKI RAEX 400 (typical yield strength 1000 MPa) is part of the Raex family of high-strength and wear-resistant steels with favorable hardness and impact toughness to extend life and decrease wear in structural components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2012) 61 (6): SA-656.
Published: 01 June 2012
... RUUKKI RAEX 450 (typical yield strength 1200 MPa) is part of the Raex family of high-strength and wear-resistant steels with favorable hardness and impact toughness to extend life and decrease wear in structural components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2012) 61 (7): SA-658.
Published: 01 July 2012
... RUUKKI RAEX 500 (typical yield strength 1250 MPa) is part of the Raex family of high-strength and wear-resistant steels with favorable hardness and impact toughness to extend life and decrease wear in structural components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1978) 27 (4): SA-345.
Published: 01 April 1978
... sizes produced by the manufacturer. It is an excellent choice for fabrication of structural components or for use in pressure tubing subjected to a low-temperature environment. *STROLOY is a registered trademark of Babcock and Wilcox. Composition: Physical Constants: (Approximate) Range Density, lb/cu...
Journal Articles
Alloy Digest (1992) 41 (7): SA-463.
Published: 01 July 1992
... LADISH D-11 is a low alloy steel of medium carbon content and a balanced alloy composition. The alloy was designed for structural components and hot work tool and die applications as it possesses better higher temperature strength than D-6-A and H-13. This datasheet provides information...
Journal Articles
Alloy Digest (1967) 16 (2): Mo-8.
Published: 01 February 1967
... of arc-cast TZM, which has the same composition. Suggested uses are dies for extrusion, hot pressing, and die casting and for a wide structural components that operate at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1968) 17 (4): SA-225.
Published: 01 April 1968
... for applications such as rocket motor cases and accessories, bolts and fasteners and aircraft structural components- particularly landing gear. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2007) 56 (5): Ni-649.
Published: 01 May 2007
... deg C (1800 deg F). It is typically used in aircraft turbine and structural components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well...
Journal Articles
Alloy Digest (2001) 50 (2): SS-818.
Published: 01 February 2001
... Lescalloy Jethete M-152 ESR is a martensitic stainless steel that is hardenable to product high strength for structural components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat...
Journal Articles
Alloy Digest (2014) 63 (10): Ni-719.
Published: 01 October 2014
... Alloy IN 939 was developed for turbine airfoils and has been used extensively in industrial gas turbines. However, the development of the alloy and the joining technology required for application to large structural components in aero engines includes risks. This datasheet covers a weldable...
Journal Articles
Alloy Digest (1981) 30 (5): SA-380.
Published: 01 May 1981
... ARMCO SSS 100A is a low-carbon, fine-grained, quenched-and-tempered alloy steel. It is strong, tough and readily fabricated with equipment and facilities suited to its high strength. It has a minimum yield strength of 100,000 psi. Among its many uses are structural components in heavy-duty...
Journal Articles
Alloy Digest (1964) 13 (10): TS-152.
Published: 01 October 1964
... Pyromet 882 is an air-hardening 5% chromium tool steel recommended for high temperature applications up to 1000 F. It has extremely high tensile and creep strength. It is used for such critical applications as structural components in aircraft and missiles which require either extremely high...
Journal Articles
Alloy Digest (1965) 14 (2): SA-173.
Published: 01 February 1965
... Cyclops BHT is a low-alloy martensitic high-speed steel of the molybdenum type recommended for high strength, high load structural components designed for elevated temperature service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1966) 15 (5): SA-194.
Published: 01 May 1966
... McLouth ML-50 is a high-strength low-alloy steel combining excellent formability, weldability with good atmospheric corrosion resistance. It is recommended for structural components where decreased weight is desired. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1961) 10 (6): TS-105.
Published: 01 June 1961
... Potomac A is a medium carbon, alloy steel that can maintain strength at elevated temperatures up to 1000 F. It is recommended for hot die applications and for structure components where strength at elevated temperatures is important. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1982) 31 (5): Cu-437.
Published: 01 May 1982
... have gradually become popular only since aliminum became commercially available about 85 years ago. Among its many uses are marine hardware, structural components and corrosion-resistant tanks and vessels. This datasheet provides information on composition, physical properties, hardness, elasticity...