Alloy Digest (2019) 68 (2): SS-1303.
Published: 01 February 2019
... Sandvik 13C26 Medical Strip is martensitic stainless strip steel that has very good wear resistance. One important use is surgical blades. This datasheet provides information on composition, physical properties, and hardness as well as fatigue. It also includes information on wear resistance...
Journal Articles
Alloy Digest (1991) 40 (8): SA-461.
Published: 01 August 1991
... UDDEHOLM AISI 52100 is an extremely versatile high-strength steel available in strip form. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating. Filing Code: SA-461. Producer or source: Uddeholm Corporation. Producer...
Journal Articles
Alloy Digest (1992) 41 (5): Ni-402.
Published: 01 May 1992
... BLENDALLOY 254025 Filing Code: Ni-402 Nickel Alloy - DIGEST- MAY 1992 DATA ON WORLD WIDE METALS AND ALLOYS PuMshedby: Alloy Digest. ln~1201-677-6161 27 CanIbId SIreel. Orange. N.J. 07060/ USA BLENDALLOY 255025 (Soft Magnetic Alloy Strip) BLENDALLOY 25-5025 is a soft magnetic nickel/ion alloy. It is produced...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-717.
Published: 01 June 2004
... that the material has been age hardened by the standard heat treatment. Material in these tem- pers has been cold rolled to a thickness reduction of 29 and 37%, respectively. Specification Equivalents: UNS C17460 ASTM B 768 (strip) General Characteristics: Brush 60 is a high-conductivity copper beryllium strip...
Journal Articles
Alloy Digest (2005) 54 (12): SS-948.
Published: 01 December 2005
... Sandvik 7C27Mo2 is martensitic stainless strip steel that also contains molybdenum for corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: SS-948...
Journal Articles
Alloy Digest (2006) 55 (1): SS-951.
Published: 01 January 2006
... Sandvik 13C26 is martensitic stainless strip steel that has very good wear resistance. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: SS-951. Producer or source: Sandvik Steel Company...
Journal Articles
Alloy Digest (2006) 55 (2): SS-954.
Published: 01 February 2006
... workability (Nominal) Carbon 0.60 Silicon 0.40 Manganese 0.40 Phosphorus 0.025 max Sulfur 0.010 max Chromium 13.5 Iron bal See Table 1. Hardening. The hardening temperature is 1080 °C (1975 °F), with a holding time of 5 min, and quenching in oil. Tempering. For strip thickness...
Journal Articles
Alloy Digest (2006) 55 (3): SS-956.
Published: 01 March 2006
... properties, the aging should be made at 475 °C (885 °F) for 4 h. Some examples of the aging effect are given in Table 4. SANDVIK NANOFLEX Filing Code: SS-956 Stainless Steel March 2006 SANDVIK NANOFLEX (Strip Steel) Sandvik Nanoflex is a corrosion-resistant precipitation-hardening austenitic stainless steel...
Journal Articles
Alloy Digest (2006) 55 (7): CS-146.
Published: 01 July 2006
... Sandvik 20C is a strip steel with high fatigue strength, supplied for pad printing or as a shock absorber steel. It has a high yield to tensile strength value. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also...
Journal Articles
Alloy Digest (1992) 41 (10): Ni-413.
Published: 01 October 1992
... BRUSH WELLMAN Alloy 360 beryllium nickel strip combines unique mechanical and physical properties required in electrical, electronic and electromechanical systems. Strength, stress-relaxation and fatigue are some of those properties. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1998) 47 (10): Ti-105.
Published: 01 October 1998
... TIMETAL 21S (Ti-15%Mo-3%Nb-3%Al-0.2Si) offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aerospace applications include engine exhaust plug and nozzle assemblies. This datasheet provides information...
Journal Articles
Alloy Digest (1999) 48 (4): Co-106.
Published: 01 April 1999
... AMETEK 595, 591, and 580 are ductile cobalt strip produced by the powder method. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: CO-106. Producer or source: AMETEK Specialty Metal Products. Producer or Source: AMETEK...
Journal Articles
Alloy Digest (1999) 48 (5): Ni-551.
Published: 01 May 1999
... N02200 AMETEK 899 NICKEL (High Purity Nickel Strip) High-purity nickel offers unique physical and mechanical properties used in both the metal forming and rechargeable battery markets. Chemical Composition, wt Physical and Magnetic Properties: Products Available: This product is available in strip...
Journal Articles
Alloy Digest (1999) 48 (12): CS-133.
Published: 01 December 1999
... SANDVIK 15LM is strip steel especially suited for automatic production of hand and bow saws. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: CS-133. Producer or source: Sandvik. Producer or Source: Sandvik Copyright ©...
Journal Articles
Alloy Digest (2000) 49 (1): CS-134.
Published: 01 January 2000
... SANDVIK 15N2 is strip steel for stonecutting saws and especially designed for the manufacture of diamond saw blades. This datasheet provides information on composition, physical properties, hardness, and tensile properties. Filing Code: CS-134. Producer or source: Sandvik. Producer or Source...
Journal Articles
Alloy Digest (1984) 33 (9): SA-401.
Published: 01 September 1984
... provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and bend strength. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-401. Producer or source: Uddeholm Strip Steel AB. Producer or Source...
Journal Articles
Alloy Digest (1967) 16 (4): Ni-123.
Published: 01 April 1967
... Carpenter Vacumet HyMu 800 is a vacuum melted nickel-molybdenum-iron alloy recommended as strip for laminations or torroids with a minimum permeability of 65,000 at 40 gauss in strip 0.010-0.001 inch thick. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1999) 48 (3): Ni-549.
Published: 01 March 1999
... AMETEK 820 alloy is a powder metallurgically produced strip that is used in hardfacing weld wire. The production process, however, can produce other special strip compositions such as the nickel-chromium alloys used as resistance alloys. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2022) 71 (10): Cu-934.
Published: 01 October 2022
... Aurubis C12200 (Cu-DHP) is a phosphorus-deoxidized copper, that contains a minimum of 99.9% copper and high residual phosphorus (0.015–0.040%). It is the most widely used copper for tube and pipe but also finds widespread use for sheet and strip items. Aurubis C12200 exhibits better ductility than...
Journal Articles
Alloy Digest (2022) 71 (2): Cu-929.
Published: 01 February 2022
... Austral Wright 5% Phosphor Bronze (UNS C51800) is a wrought copper-tin-phosphorus alloy. It is the most widely used grade of wrought phosphor bronze. It is harder, stronger and stiffer than the wrought brasses and, in strip and wire form, is produced with a combination of excellent cold...