Alloy Digest (1966) 15 (1): Al-151.
Published: 01 January 1966
... Aluminum X7005 is an age-hardenable aluminum alloy having high mechanical properties, good fracture toughness, good corrosion and stress-corrosion resistance, and good weldability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1970) 19 (1): Cu-210.
Published: 01 January 1970
... International Alronze bend strength chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability physical properties stress-corrosion-resistant alloys tensile properties workability ALRONZE Filing Code: cu-210 Copper Alloy JANUARY 1970...
Journal Articles
Alloy Digest (2002) 51 (2): SS-844.
Published: 01 February 2002
... Carlson Alloy 904L is a 21Cr-24Ni-4.5Mo-1.5Cu low-carbon austenitic alloy that resists corrosion in a wide range of both oxidizing and reducing environments. It has good pitting and crevice-corrosion resistance and eliminates stress-corrosion cracking in most common chloride environments...
Journal Articles
Alloy Digest (1987) 36 (2): Ni-344.
Published: 01 February 1987
... UNITEMP 625 is a nickel-base, austenitic, solution-strengthened high-performance alloy that provides excellent resistance to both high-temperature gaseous corrosion and aqueous corrosion coupled with good strength and stress-rupture properties to 1800 F. The alloy has good resistance to stress...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-459.
Published: 01 August 1994
... Carlson Alloy C800 AT has superior creep and rupture strengths over long-term exposure to high temperatures and higher ASME boiler and pressure-vessel design stress allowables than C800 H. The alloy resists stress-corrosion cracking, resists sulfur attack, internal oxidation, scaling and corrosion...
Journal Articles
Alloy Digest (1977) 26 (9): Ni-249.
Published: 01 September 1977
... the formation of grain-boundry carbide precipitates in the weld heat-affected zone, thus making it suitable for most chemical process applications in the as-welded condition. This alloy also has excellent resistance to pitting and stress-corrosion cracking. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2021) 70 (8): Ni-774.
Published: 01 August 2021
... to oxidizing chemicals and atmospheres. It is also resistant to reducing chemicals because of its nickel and copper contents. The nickel content also provides the alloy with exceptional stress-corrosion-cracking resistance in chloride-containing environments. The high molybdenum content provides very good...
Journal Articles
Alloy Digest (1998) 47 (7): Al-350.
Published: 01 July 1998
... Alcoa 7075 alloy has very high strength and is used for highly stressed structural parts. The T7351 temper offers improved stress-corrosion cracking resistance. The alloy’s strength level equals or exceeds mild steels. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1988) 37 (12): Ni-365.
Published: 01 December 1988
... HASTELLOY alloy H-9M is especially designed for enhanced resistance to pitting and crevice corrosion attack. It is resistant to failure by stress-corrosion cracking in general and to hydrogen/hydrogen sulfide stress cracking in particular. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2007) 56 (7): Ni-653.
Published: 01 July 2007
... Langalloy K-500 is a nickel-copper alloy with both aluminum and titanium additions for age hardening. The additions give the alloy high strength and hardness. The alloy has excellent corrosion resistance along with resistance to chloride stress corrosion, high fatigue resistance in sea water...
Journal Articles
Alloy Digest (1988) 37 (12): SS-498.
Published: 01 December 1988
... INCO alloy 020 is an austenitic nickel-iron-chromium alloy. Its relatively high nickel content provides resistance to stress-corrosion cracking. Molybdenum gives the alloy good resistance to pitting and crevice corrosion; chromium makes it resistant to oxidation and niobium confers resistance...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... HASTELLOY Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated...
Journal Articles
Alloy Digest (1985) 34 (10): Cu-502.
Published: 01 October 1985
... Copper Alloy No. C69000 is a copper-zinc-aluminum-nickel alloy with a good combination of strength and ductility. Its capacity is excellent for hot work or cold work. It has fairly good resistance to general corrosion and stress-corrosion cracking; its corrosion resistance is superior...
Journal Articles
Alloy Digest (1983) 32 (8): Ni-289.
Published: 01 August 1983
... JESSOP JS Alloy G is a nickel-chromium-iron-molybdenum-copper alloy that exhibits excellent resistance to a wide variety of corrosive conditions. It resists corrosion in both oxidizing and reducing environments, and can handle both acid and alkaline solutions. JS Alloy G resists pitting and stress...
Journal Articles
Alloy Digest (1983) 32 (12): Ni-295.
Published: 01 December 1983
... and sulfuric acids. It is used for flue-gas scrubbers. In various acidic and alkaline environments, alloy G is used for its high level of resistance to pitting and stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1980) 29 (8): SS-374.
Published: 01 August 1980
.... This excellent corrosion resistance and its excellent combination of high-temperature strength, resistance to thermal fatigue and resistance to carburization make this alloy especially suited for severe service conditions involving high stress and rapid thermal cycling. This datasheet provides information...
Journal Articles
Alloy Digest (1987) 36 (5): Ni-348.
Published: 01 May 1987
... JESSOP JS Alloy G-3 is a nickel-base alloy having excellent resistance to a variety of corrosive conditions including stress corrosion. Its low carbon content and stabilization by columbium permit welding without deterioration of corrosion resistance in the heat-affected zone. The alloy is well...
Journal Articles
Alloy Digest (1981) 30 (3): Ni-266.
Published: 01 March 1981
... INCONEL Alloy 690 is a wrought nickel-base alloy with excellent resistance to many corrosive aqueous media and high-temperature atmospheres. It also has high strength, good metallurgical stability, and favorable fabrication characteristics. It has excellent resistance to stress-corrosion cracking...
Journal Articles
Alloy Digest (1986) 35 (10): Ni-341.
Published: 01 October 1986
... INCO Alloy G-3 is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to provide increased resistance to weld heat-affected zone corrosion. The alloy has exceptional stress-corrosion cracking resistance in chloride-containing environments...
Journal Articles
Alloy Digest (2011) 60 (5): Ni-690.
Published: 01 May 2011
... ATI 59 alloy is a nickel-chromium-molybdenum alloy with excellent corrosion resistance and high mechanical strength. The alloy has excellent resistance to both oxidizing and reducing media, and possesses superior resistance to chloride pitting and stress-corrosion cracking. This datasheet provides...