1-20 of 1654 Search Results for

stress-corrosion cracking resistance

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1971) 20 (4): SS-253.
Published: 01 April 1971
... USS 18-18-2 Stainless Steel (18% chromium-18% nickel-2% silicon) was developed specifically for superior resistance to stress-corrosion cracking in hot aqueous chloride solutions. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1998) 47 (7): Al-350.
Published: 01 July 1998
... Alcoa 7075 alloy has very high strength and is used for highly stressed structural parts. The T7351 temper offers improved stress-corrosion cracking resistance. The alloy’s strength level equals or exceeds mild steels. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-459.
Published: 01 August 1994
... Carlson Alloy C800 AT has superior creep and rupture strengths over long-term exposure to high temperatures and higher ASME boiler and pressure-vessel design stress allowables than C800 H. The alloy resists stress-corrosion cracking, resists sulfur attack, internal oxidation, scaling and corrosion...
Journal Articles
Alloy Digest (2021) 70 (8): Ni-774.
Published: 01 August 2021
... to oxidizing chemicals and atmospheres. It is also resistant to reducing chemicals because of its nickel and copper contents. The nickel content also provides the alloy with exceptional stress-corrosion-cracking resistance in chloride-containing environments. The high molybdenum content provides very good...
Journal Articles
Alloy Digest (1996) 45 (9): Ni-516.
Published: 01 September 1996
... Hastelloy C-2000 has a broad capability range for handling corrosive environments. The alloy has high resistance to reagent grade sulfuric acid, hydrochloric acid to high concentrations, and nitric acid. The alloy has outstanding localized corrosion resistance, excellent stress-corrosion cracking...
Journal Articles
Alloy Digest (2023) 72 (1): SS-1355.
Published: 01 January 2023
... corrosion environments and has a lower coefficient of expansion and better thermal conductivity. Cleveland- Cliffs 444 has superior chloride stress-corrosion cracking resistance to Type 304 and Type 316 austenitic stainless steels. It is oxidation and creep resistant at elevated temperatures, making...
Journal Articles
Alloy Digest (2013) 62 (3): SS-1138.
Published: 01 March 2013
... AK Steel Nitronic 30 has good wet abrasion resistance, good resistance to aqueous and atmospheric corrosion, high strength, economy, and improved stress-corrosion cracking resistance over common 18-8 stainless steels. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1986) 35 (10): Ni-341.
Published: 01 October 1986
... INCO Alloy G-3 is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to provide increased resistance to weld heat-affected zone corrosion. The alloy has exceptional stress-corrosion cracking resistance in chloride-containing environments...
Journal Articles
Alloy Digest (1989) 38 (1): Ni-366.
Published: 01 January 1989
... Allegheny Ludlum AL 825 alloy is a nickel-iron-chromium-molybdenum-copper alloy with superior corrosion resistance including stress-corrosion cracking resistance. It is highly ductile from cryogenic to well over 1000 F(538 C) temperatures. It is readily weldable. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (1): SS-842.
Published: 01 January 2002
... Carlson alloy 926 Mo is a superaustenitic 6% Mo stainless steel that resists highly corrosive environments and has excellent chloride pitting, crevice, and stress-corrosion cracking resistance. It can be utilized where the performance of conventional austenitic stainless steels is bor-derline...
Journal Articles
Alloy Digest (1994) 43 (3): SS-564.
Published: 01 March 1994
... URANUS 47N is a nitrogen-alloyed duplex stainless steel improved in stress-corrosion cracking resistance with pitting and crevice corrosion resistance better than AISI Type 317L. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1994) 43 (5): SS-566.
Published: 01 May 1994
... URANUS 52N is a nitrogen-alloyed duplex stainless steel improved in stress-corrosion cracking resistance and with pitting and crevice corrosion resistance better than AISI Type 317L. Applications include handling phosphoric acid contaminated with chlorides and in flue gas desulfurization scrubbers...
Journal Articles
Alloy Digest (1995) 44 (9): SS-608.
Published: 01 September 1995
... CARPENTER 7-Mo PLUS is a duplex stainless steel of austenite in a ferrite matrix. It is superior to 300 series stainless steels like types 304 and 316 in strength, corrosion, pitting and stress-corrosion cracking resistance (to chlorides). Typical applications are heat exchangers in the chemical...
Journal Articles
Alloy Digest (1989) 38 (3): SS-503.
Published: 01 March 1989
... JS Alloy 2205 has a microstructure of approximately 50% austenite and 50% ferrite. This duplex structure provides excellent stress-corrosion cracking resistance in chloride and hydrogen sulfide environments. The alloy has about twice the yield strength of standard austenitic stainless steels...
Journal Articles
Alloy Digest (1974) 23 (12): Ni-212.
Published: 01 December 1974
... PYROMET 625 is a nonmagnetic alloy with outstanding strength and toughness from cryogenic temperatures to 2000 F. It has excellent fatigue strength and stress-corrosion-cracking resistance to chloride ions. Some typical applications are heat shields, chemical plant hardware and special seawater...
Journal Articles
Alloy Digest (1993) 42 (9): Ni-441.
Published: 01 September 1993
... P/M 625 is a nonmagnetic alloy with outstanding strength and toughness from cryogenic temperatures to 2000 F. It has excellent fatigue strength and stress-corrosion-cracking resistance to chloride ions. This datasheet provides information on composition, microstructureand elasticity as well...
Journal Articles
Alloy Digest (1990) 39 (1): Al-233.
Published: 01 January 1990
... ALCOA ALUMINUM ALLOY 7050 is an aluminum-zinc-copper-magnesium alloy with a superior combination of strength, stress-corrosion cracking resistance and toughness, particularly in thick sections. In thin sections it also possesses an excellent combination of properties that are important...
Journal Articles
Alloy Digest (1991) 40 (9): SS-523.
Published: 01 September 1991
... LESCALLOY 13-8Mo VIM-VAR is a precipitation hardening martensitic stainless steel with excellent fracture toughness, transverse mechanical properties and stress-corrosion cracking resistance. It is produced by vacuum induction melting plus vacuum arc remelting. This datasheet provides information...
Journal Articles
Alloy Digest (2009) 58 (10): Ni-673.
Published: 01 October 2009
... Sandvik Sanicro 67 is a composite tube for various boiler applications. The outer tube layer is of Sanicro 67, an austenitic nickel-base alloy with excellent corrosion and stress-corrosion cracking resistance. This datasheet provides information on composition and physical properties. It also...
Journal Articles
Alloy Digest (1997) 46 (3): SS-674.
Published: 01 March 1997
... RA2205 is an austenitic/ferritic duplex stainless steel containing about 40 to 50% ferrite in the annealed condition. The alloy provides superior service when compared to Type 316L or 317L in most environments, especially considering pitting, chloride-ion stress-corrosion cracking resistance...