Alloy Digest (1971) 20 (4): SS-253.
Published: 01 April 1971
... USS 18-18-2 Stainless Steel (18% chromium-18% nickel-2% silicon) was developed specifically for superior resistance to stress-corrosion cracking in hot aqueous chloride solutions. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1988) 37 (12): Ni-365.
Published: 01 December 1988
... HASTELLOY alloy H-9M is especially designed for enhanced resistance to pitting and crevice corrosion attack. It is resistant to failure by stress-corrosion cracking in general and to hydrogen/hydrogen sulfide stress cracking in particular. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1993) 42 (3): SS-472.
Published: 01 March 1993
... AVESTA 2205 is a ferritic-austenitic duplex stainless steel. It resists stress-corrosion cracking very well and has good pitting and general corrosion resistance. Its high strength and stress-corrosion resisting characteristics are a reflection of its duplex microstructure. Its uses include heat...
Journal Articles
Alloy Digest (2002) 51 (2): SS-844.
Published: 01 February 2002
... Carlson Alloy 904L is a 21Cr-24Ni-4.5Mo-1.5Cu low-carbon austenitic alloy that resists corrosion in a wide range of both oxidizing and reducing environments. It has good pitting and crevice-corrosion resistance and eliminates stress-corrosion cracking in most common chloride environments...
Journal Articles
Alloy Digest (2000) 49 (1): SS-773.
Published: 01 January 2000
... J and L 2205 is a ferritic-austenitic duplex stainless steel. It resists stress-corrosion cracking very well and has good pitting and general corrosion resistance. Its high strength and stress-corrosion resisting characteristics are a reflection of its duplex microstructure. Its uses include pipe...
Journal Articles
Alloy Digest (1987) 36 (2): Ni-344.
Published: 01 February 1987
... to both high-temperature gaseouscorrosion and aqueous corrosion coupled with good strength and stressrupture properties to 18OO F.The alloy has good resistance to stress-corrosion cracking. *UNITEMP is a registered trademark of Cyclops Corporation. Composition: Carbon Manganese Silicon Chromium Molybdenum...
Journal Articles
Alloy Digest (1978) 27 (5): Ti-70.
Published: 01 May 1978
... of different process histories. The specific strength (strength/density ratio) is superior to that of the Ti-6A1-4V alloy. Resistance to fatigue crack propagation and resistance to chloride-stress-corrosion cracking are comparable to those of Ti-6A1-4V. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-459.
Published: 01 August 1994
... Carlson Alloy C800 AT has superior creep and rupture strengths over long-term exposure to high temperatures and higher ASME boiler and pressure-vessel design stress allowables than C800 H. The alloy resists stress-corrosion cracking, resists sulfur attack, internal oxidation, scaling and corrosion...
Journal Articles
Alloy Digest (1998) 47 (7): Al-350.
Published: 01 July 1998
... Alcoa 7075 alloy has very high strength and is used for highly stressed structural parts. The T7351 temper offers improved stress-corrosion cracking resistance. The alloy’s strength level equals or exceeds mild steels. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-600.
Published: 01 January 2003
... Allcorr (UNS N06110) is a single-phase, non-age-hardenable, nickel-base alloy for service in highly corrosive environments. It is characterized by outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress-corrosion cracking. The alloy...
Journal Articles
Alloy Digest (2021) 70 (8): Ni-774.
Published: 01 August 2021
... to oxidizing chemicals and atmospheres. It is also resistant to reducing chemicals because of its nickel and copper contents. The nickel content also provides the alloy with exceptional stress-corrosion-cracking resistance in chloride-containing environments. The high molybdenum content provides very good...
Journal Articles
Alloy Digest (1979) 28 (1): SS-360.
Published: 01 January 1979
... ALLEGHENY LUDLUM E-BRITE 26-1 ALLOY is a low-carbon, low-nitrogen ferritic stainless steel made by a vacuum refining process. It provides: (1) Excellent resistance to pitting and crevice corrosion in chloride-containing environments, (2) Excellent resistance to chloride stress-corrosion cracking...
Journal Articles
Alloy Digest (1974) 23 (7): SS-298.
Published: 01 July 1974
... CARPENTER STAINLESS No. 7-Mo is a two-phase alloy consisting of a ferritic matrix with pools of austenite. It has high resistance to stress-corrosion cracking and pitting, and good general corrosion resistance in many environments. Its principal use is for tubing and pipe in heat exchangers...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-318.
Published: 01 July 1985
..., pitting and stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-318. Producer...
Journal Articles
Alloy Digest (1979) 28 (3): SS-362.
Published: 01 March 1979
... ALLEGHENY LUDLUM Type 29-4 is a low-interstitial ferritic stainless steel. It contains approximately 29% chromium and 4% molybdenum. The alloy provides excellent resistance to pitting, crevice corrosion, and stress-corrosion cracking in chloride-containing environments. Type 29-4 is used widely...
Journal Articles
Alloy Digest (1980) 29 (11): SS-377.
Published: 01 November 1980
... resistance to stress-corrosion cracking and to intergranular corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining...
Journal Articles
Alloy Digest (1983) 32 (2): Ni-283.
Published: 01 February 1983
... NICROFER 4221 is a fully austenitic nickel-chromium-iron-molybdenum-copper alloy that is stabilized (against intergranular corrosion) by an addition of titanium. It is resistant to stress-corrosion cracking, pitting corrosion and oxidizing and non-oxidizing hot acids. It has good mechanical...
Journal Articles
Alloy Digest (1983) 32 (8): Ni-289.
Published: 01 August 1983
... resistance to a wide variety of corrosive conditions. It resists corrosion in both oxidizing and reducing environments, and can handle both acid and alkaline solutions. JS Alloy G resists pitting and stress-corrosion cracking extremely well. Among its many uses are equipment for chemical processing...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... CARPENTER 20Mo-6 is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. Its good resistance to corrosion has been...
Journal Articles
Alloy Digest (1984) 33 (6): SS-446.
Published: 01 June 1984
... to pitting. crevice and inter- granular corrosion and to stress-corrosion cracking. and (3) Good mechanical properties. Its many uses include equipment for pro- ducing phosphoric acid by the wet method. equipment for handling sulfuric acid contaminated with chlorides. handling seawater and use in deep sour...