Alloy Digest (2018) 67 (4): Cu-870.
Published: 01 April 2018
... Alloy CuSn4 is a high-performance copper alloy. It finds use in applications where high strength and good formability combined with good stress relaxation resistance and moderate conductivity are required. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2021) 70 (11): Cu-926.
Published: 01 November 2021
... the strength, and improve the softening characteristics. Wieland B31 possesses the right combination of formability, conductivity, strength, and stress relaxation resistance to be used for automotive applications at relatively high ambient temperatures. In addition, its strength is similar to that of a 4% tin...
Journal Articles
Alloy Digest (2005) 54 (12): Cu-738.
Published: 01 December 2005
... Wieland K-88 is a copper alloy with very high electrical and thermal conductivity, good strength, and excellent stress relaxation resistance at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2008) 57 (10): Cu-760.
Published: 01 October 2008
... Luvata C1921 is a copper alloy with high electrical and thermal conductivity, good softening resistance, good stress-relaxation resistance, and good formability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2000) 49 (2): Cu-647.
Published: 01 February 2000
... Olin C654 is a 95.4Cu-3.0Si-1.5Sn-0.1Cr bronze alloy with high strength, good formability, and stress-relaxation resistance. Uses include springs and connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2017) 66 (8): Cu-863.
Published: 01 August 2017
... strength, good bend formability and good stress relaxation resistance. Producer: Gebr. Kemper GmbH + Co. KG Metallwerke D-57462 Olpe, Germany Tel: +49 (0) 27 61 8 91-0 Fax +49 (0) 27 61 8 91-2 02 www.kemper-olpe.de ISSN: 002-614X Cu-863B Table 1 Mechanical properties Temper Tensile strength, Rm, MPa (ksi...
Journal Articles
Alloy Digest (2017) 66 (11): Cu-866.
Published: 01 November 2017
... Alloy KAD 442 (UNS C44250) is a high-performance copper alloy. Typical uses are applications where high strength and good formability combined with good stress relaxation resistance and moderate conductivity are required. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1999) 48 (3): Cu-631.
Published: 01 March 1999
... Alloy C7025 is a second generation, high performance alloy whose strength comes from an age hardening heat treatment similar to that used for the beryllium coppers. With stress relaxation resistance comparable to Be-Cu alloys C170/C172 (see Olin 170, Alloy Digest Cu-615, July 1998, and Olin 172...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-645.
Published: 01 January 2000
... Olin C688 is a brass enriched with both aluminum and cobalt for added strength and stress relaxation resistance. The alloy is ideal for springs. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes...
Journal Articles
Alloy Digest (2004) 53 (3): Cu-712.
Published: 01 March 2004
... to thermal management. Higher power requirements create harsh environments and higher operating temperatures. Alloy 390 provides excellent stress-relaxation resistance at elevated temperatures, which increases electrical contact reliability. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1987) 36 (1): Cu-520.
Published: 01 January 1987
... ZHC COPPER is a high-electrical-conductivity alloy developed to satisfy the requirements of high-power electronic circuits. It has high strength compared to other metals of equivalent conductivity, good bend formability, excellent stress-relaxation resistance and is readily soldered. It also...
Journal Articles
Alloy Digest (2023) 72 (12): Cu-943.
Published: 01 December 2023
... formability and ductility. This alloy features good stress relaxation resistance and high fatigue strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1999) 48 (8): Cu-638.
Published: 01 August 1999
... WRM alloy 5058 is a phosphor-bronze alloy with a good combination of electrical conductivity, tensile strength, and stress-relaxation resistance. Typical applications include lead frames, contact springs, and fuse clips. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-640.
Published: 01 October 1999
... WRM alloy 5248 is a phosphor bronze alloy with higher strength and better stress relaxation resistance than 10% tin alloys. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. Filing Code: CU-640. Producer or source: Waterbury...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-634.
Published: 01 October 1999
... WRM Alloy C19400 has one of the best combinations of electrical conductivity, mechanical strength, forming properties, and stress-relaxation resistance characteristics of high-performance copper alloys for electronic applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-644.
Published: 01 January 2000
... WRM alloy 4260 is a modified tin-brass alloy with strength and formability similar to C52100 but possessing a significantly higher electrical conductivity and improved stress relaxation resistance. The alloy can be used for connectors and contact springs. This datasheet provides information...
Journal Articles
Alloy Digest (2003) 52 (4): Cu-699.
Published: 01 April 2003
... Outokumpu 5119, or KLF-7, is a high performance copper tin alloy with excellent combination of strength and stress relaxation resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. Filing Code: CU-699...
Journal Articles
Alloy Digest (1999) 48 (5): Cu-635.
Published: 01 May 1999
... Olin alloy 186 provides high thermal stability for elevated-temperature connector applications. This alloy provides exceptional resistance to loss in contact because of its excellent resistance to stress relaxation. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1981) 30 (5): Cu-417.
Published: 01 May 1981
... previously only attainable with more expensive materials. The new alloy has superior stress-relaxation characteristics, good bend performance and excellent corrosion resistance. Among its typical uses are elec- trical connectors, fuse clips and relay springs. *ULTRONZE is a registeredtrademark of the Olin...
Journal Articles
Alloy Digest (2020) 69 (1): Cu-904.
Published: 01 January 2020
... Olin Brass Alloy C42200 (Tradename: Lubronze) is a copper-zinc-tin alloy (tin brass). The mechanical properties and performance of C42200 are very similar to those of high-zinc brass alloys with the added benefit of improved resistance to stress relaxation. It is also a cost-effective alternative...