Alloy Digest (1971) 20 (4): SS-253.
Published: 01 April 1971
... USS 18-18-2 Stainless Steel (18% chromium-18% nickel-2% silicon) was developed specifically for superior resistance to stress-corrosion cracking in hot aqueous chloride solutions. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1988) 37 (12): Ni-365.
Published: 01 December 1988
... HASTELLOY alloy H-9M is especially designed for enhanced resistance to pitting and crevice corrosion attack. It is resistant to failure by stress-corrosion cracking in general and to hydrogen/hydrogen sulfide stress cracking in particular. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1965) 14 (3): Cu-149.
Published: 01 March 1965
... Revere Alloy 411 is a bearing bronze alloy having good formability, low coefficient of friction, corrosion resistance, and freedom from stress-cracking. (It was formerly known as Revere No. 325.) This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1961) 10 (7): Cu-103.
Published: 01 July 1961
... RED BRASS, 85% is a copper-zinc alloy having high corrosion resistance to water and high resistance to stress-cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1991) 40 (2): Cu-557.
Published: 01 February 1991
... Copper Alloy No. C70600 is a very resistant alloy in a seawater service. Failure in properly designed systems in such environments by general corrosion, pitting, crevice attack and stress-cracking can be discounted for this copper nickel alloy. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1992) 41 (8): Ni-409.
Published: 01 August 1992
... CARLSON ALLOY C625 has excellent strength and superior resistance to oxidation at temperatures up to 2000 F. Outstanding resistance to general corrosion, pitting, and stress-cracking in many environments. This alloy has exceptional fatigue strength and toughness at cryogenic temperatures...
Journal Articles
Alloy Digest (2014) 63 (4): Ni-666.
Published: 01 April 2014
... Incoloy Alloy 945 is a nickel-base precipitation-strengthened alloy that provides 860 MPa (125 ksi) minimum yield strength and an excellent combination of ductility and impact strength. The nickel content is sufficient to provide protection against chloride-ion stress-corrosion cracking...
Journal Articles
Alloy Digest (1988) 37 (7): Ni-357.
Published: 01 July 1988
... CUSTOM AGE 625 PLUS Alloy offers exceptional resistance to pitting, crevice, attack, general corrosion and to stress-corrosion cracking in the precipitation-hardened condition. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1971) 20 (3): Al-201.
Published: 01 March 1971
... ALUMINUM 7049-T23 is a high-strength alloy having excellent resistance to stress-corrosion cracking. It was developed for use in die and hand forgings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1986) 35 (6): SS-471.
Published: 01 June 1986
... AVESTA STAINLESS 44LN is an austenitic-ferritic stainless steel with good resistance to various types of corrosion. It is highly resistant to stress-corrosion cracking in chloride-containing media. Its yield strength is approximately twice that of austenitic stainless steels. Other properties...
Journal Articles
Alloy Digest (2009) 58 (1): SA-590.
Published: 01 January 2009
... CarElso 70 SOHIC is a steel alloy with special melt practice producing a pressure vessel material with excellent resistance to stress-oriented hydrogen-induced cracking (SOHIC). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1993) 42 (3): SS-541.
Published: 01 March 1993
... displays both higher critical pitting and crevice corrosion temperatures than many of the conven- tional stainless steels and other common duplex stainless steels. Unlike many common cast duplex stainless steels, it exhibits good r&stance to sulfide stress cracking (SSC) in tests conducted according...
Journal Articles
Alloy Digest (2002) 51 (8): SS-860.
Published: 01 August 2002
.... The high pitting potential leads to relatively good fatigue properties in the presence of saline solutions. For example, the endurance limit in 3% NaCl solution for 10.5 in. diam bar (center) at ±215 MPa (±31 ksi) is >107 cycles. See also Table 1. Stress-Corrosion Cracking Resistance. Staballoy 734...
Journal Articles
Alloy Digest (2005) 54 (12): Ni-629.
Published: 01 December 2005
...-ring specimens stressed 100% of yield with carbon steel bolts in NACE solution (5% NaCl + 0.5% CH3COOH + H2S) at room temperature Table 3 Hydrogen Sulfide Stress-Corrosion Cracking Hydrogen sulfide stress-corrosion cracking 050 C-276 NACE solution (5% NaCl + 0.5% CH3COOH + H2S), No cracks No cracks 204...
Journal Articles
Alloy Digest (1978) 27 (5): Ti-70.
Published: 01 May 1978
... of different process histories. The specific strength (strength/density ratio) is superior to that of the Ti-6A1-4V alloy. Resistance to fatigue crack propagation and resistance to chloride-stress-corrosion cracking are comparable to those of Ti-6A1-4V. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-459.
Published: 01 August 1994
... Carlson Alloy C800 AT has superior creep and rupture strengths over long-term exposure to high temperatures and higher ASME boiler and pressure-vessel design stress allowables than C800 H. The alloy resists stress-corrosion cracking, resists sulfur attack, internal oxidation, scaling and corrosion...
Journal Articles
Alloy Digest (1993) 42 (3): SS-472.
Published: 01 March 1993
... AVESTA 2205 is a ferritic-austenitic duplex stainless steel. It resists stress-corrosion cracking very well and has good pitting and general corrosion resistance. Its high strength and stress-corrosion resisting characteristics are a reflection of its duplex microstructure. Its uses include heat...
Journal Articles
Alloy Digest (2000) 49 (1): SS-773.
Published: 01 January 2000
... J and L 2205 is a ferritic-austenitic duplex stainless steel. It resists stress-corrosion cracking very well and has good pitting and general corrosion resistance. Its high strength and stress-corrosion resisting characteristics are a reflection of its duplex microstructure. Its uses include pipe...
Journal Articles
Alloy Digest (2002) 51 (2): SS-844.
Published: 01 February 2002
... Carlson Alloy 904L is a 21Cr-24Ni-4.5Mo-1.5Cu low-carbon austenitic alloy that resists corrosion in a wide range of both oxidizing and reducing environments. It has good pitting and crevice-corrosion resistance and eliminates stress-corrosion cracking in most common chloride environments...
Journal Articles
Alloy Digest (1998) 47 (7): Al-350.
Published: 01 July 1998
... Alcoa 7075 alloy has very high strength and is used for highly stressed structural parts. The T7351 temper offers improved stress-corrosion cracking resistance. The alloy’s strength level equals or exceeds mild steels. This datasheet provides information on composition, physical properties...