Journal Articles
Alloy Digest (2008) 57 (11): SA-587.
Published: 01 November 2008
... Domex 420 MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 1.80-15.00 mm. The alloy meets or exceeds the requirements of S420MC in EN 10149-2. Applications include a wide range of fabricated components and steel structures...
Journal Articles
Alloy Digest (2009) 58 (1): SA-591.
Published: 01 January 2009
... Domex 460 MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-13.00 mm. The alloy meets or exceeds the requirements of S460MC in EN 10149-2. Applications include a wide range of fabricated components and steel structures...
Journal Articles
Alloy Digest (2006) 55 (2): SA-555.
Published: 01 February 2006
... HPS 100W is specified in ASTM A 709 (Standard Specification for Carbon and High-Strength Low-Alloy Structural Steel Shapes, Plates, and Bars and Quenched-and-Tempered Alloy Structural Steel Plates for Bridges) and is being added to AASHTO M270. Initial applications were planned to be those...
Journal Articles
Alloy Digest (2019) 68 (5): SA-844.
Published: 01 May 2019
... Bisalloy Structural 80 Pressure Vessel Steel (80 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel for pressure vessel applications. It exhibits excellent cold formability and low-temperature fracture toughness. This datasheet provides information...
Journal Articles
Alloy Digest (2004) 53 (4): SA-533.
Published: 01 April 2004
... DUAL-TEN 600 is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional high-strength low-alloy (HSLA) steels. Applications include front and rear rails, crush cans, rocker reinforcements, pillar...
Journal Articles
Alloy Digest (2004) 53 (5): SA-535.
Published: 01 May 2004
... DUAL-TEN 780 (UTS 780 MPa, or 113 ksi) is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional high-strength low-alloy (HSLA) steels. Applications include front and rear rails, crush cans...
Journal Articles
Alloy Digest (2004) 53 (2): SA-530.
Published: 01 February 2004
... DUAL-TEN 500 (UTS 500 MPa, or 73 ksi) is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional HSLA steels. They offer a great opportunity for part weight reduction. The improved formability...
Journal Articles
Alloy Digest (2004) 53 (3): SA-532.
Published: 01 March 2004
... DUAL-TEN 590 (UTS 590 MPa, or 86 ksi) is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional HSLA steels. They offer a great opportunity for part weight reduction. The improved formability...
Journal Articles
Alloy Digest (1979) 28 (6): SA-360.
Published: 01 June 1979
...-Alloy OII JUNE 1979 DICBST - DATA ON WORLD WIDO MRTALS AND ALLOYS w-ggzJuP&k Inc. Upper Mmtckir. New Jersey CREUSABRO*M (Abrasion-Resistant 12% Manganese Steel) CREUSABRO M has special properties obtained by annealing and quenching, resulting in an austenitic structure which has the ability to rapidly...
Journal Articles
Alloy Digest (1983) 32 (8): CS-96.
Published: 01 August 1983
... steel is required. Its manganese content (nominally 1.15%) provides some increase in hardenability in all applications and increased hardness and strength in uncarburized uses and in the core of carburized parts. Its applications include a wide range of components and parts for machinery and structures...
Journal Articles
Alloy Digest (2003) 52 (11): SA-524.
Published: 01 November 2003
... International Steel Group (ISG) produces seven grades of steel in the ASTM A 514 (structural applications) and ASTM A 517 (pressure vessel applications) families. These are grades A, B, E, F, H, P, and Q. They are chemically identical between A 514 and A 517 This datasheet provides information...
Journal Articles
Alloy Digest (2018) 67 (9): SA-821.
Published: 01 September 2018
... Strenx 900 is a structural steel that guarantees a minimum yield strength of up to 900 MPa (131 ksi) depending on thickness. Strenx 900 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low...
Journal Articles
Alloy Digest (2018) 67 (10): SA-826.
Published: 01 October 2018
... Strenx 900 Plus is a structural steel with a minimum yield strength of 900 MPa (131 ksi). Strenx 900 Plus provides a good combination of strength and toughness together with good workshop properties. Typical applications include load-bearing structures, where low weight is needed. This datasheet...
Journal Articles
Alloy Digest (1977) 26 (7): SA-335.
Published: 01 July 1977
... LESCALLOY D6AC VAC ARC is a high-hardenability low-alloy steel for high-strength structural applications requiring tensile strengths up to 280,000 psi. It provides a high ratio of yield strength to tensile strength, good ductility and excellent notch toughness with a tough, fibrous fracture as low...
Journal Articles
Alloy Digest (2019) 68 (1): SA-834.
Published: 01 January 2019
... Strenx 1100 is a structural steel that guarantees a minimum yield strength of 1100 MPa (160 ksi). Strenx 1100 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low weight is needed. Despite...
Journal Articles
Alloy Digest (2017) 66 (2): SA-779.
Published: 01 February 2017
... Strenx 700 is a high-strength structural steel with a minimum yield strength of 650–700 MPa (94–102 ksi) depending on thickness. Strenx 700 meets the requirements of EN 10 025-6 for the S690 grade and thicknesses. Typical applications include demanding load-bearing structures. This datasheet...
Journal Articles
Alloy Digest (2017) 66 (5): SA-783.
Published: 01 May 2017
... Strenx 1300 is a very high-strength structural steel with a minimum yield strength of 1300 MPa (189 ksi). Typical applications include load-carrying structures that place very high demands on low weight. S5188 This datasheet provides information on composition, physical properties, tensile...
Journal Articles
Alloy Digest (1972) 21 (7): SA-277.
Published: 01 July 1972
... USS COR-TEN B is an atmospheric corrosion-resistant steel with a minimum yield point of 50,000 psi in plates, bars and structural shapes through 4-in. thick. It is suited for many structural applications. This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (1963) 12 (7): SA-149.
Published: 01 July 1963
... Republic-M is a low carbon, manganese type structural steel having high notch-impact resistance and high ductility at subzero temperatures. It is recommended for structural applications where weight reduction is important. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1968) 17 (5): SS-209.
Published: 01 May 1968
... temperature structural applications as well as hot work applications such as extrusion tooling, die casting dies and glass molds. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information...