Journal Articles
Alloy Digest (1985) 34 (9): SS-463.
Published: 01 September 1985
... CARPENTER MOLY ASCOLOY is a chromium-nickel-molybdenum-vanadium hardenable martensitic stainless steel designed for service up to 1200 F (649 C). It is utilized in steam turbine buckets and in compressor components in gas turbines and in other high-temperature applications. This datasheet provides...
Journal Articles
Alloy Digest (2004) 53 (9): SA-138.
Published: 01 September 2004
... Durehete 900 is a high-strength steel bolting material often used in steam turbine and other power-plant applications. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on high...
Journal Articles
Alloy Digest (2005) 54 (10): SA-145.
Published: 01 October 2005
... Durehete 950 is a high-strength steel bolting material often used in steam turbine and other power plant applications. It is usually supplied in the heat treated condition. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
... AISI No. 616 is a hardenable martensitic type stainless steel recommended for high temperature applications up to 1200 F. It is used for steam turbine blades and buckets, valves, jet engine components, and high temperature bolting. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1968) 17 (6): SS-210.
Published: 01 June 1968
... Carpenter Stainless No. 404 is recommended for highly stressed parts at temperatures up to 1050 F where joining is a problem. It is both hardenable and weldable. It is used for steam turbine buckets, blades and diaphrams. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (9): Ni-147.
Published: 01 September 1969
... IN-102 is a nickel-chromium-iron alloy designed for long service at temperatures up to 1300 F. It combines high strength and high ductility at the elevated temperatures with a high degree of structural stability. It is used for aerospace, power and steam turbine components. This datasheet provides...
Journal Articles
Alloy Digest (1966) 15 (8): SS-185.
Published: 01 August 1966
... ENDURO S-1 is a chromium type stainless steel providing high strength, toughness and resistance to impact when heat treated. It shows resistance to wet and dry corrosion. It is recommended for steam turbine parts, valves, cutlery, pump components, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1964) 13 (2): SS-152.
Published: 01 February 1964
... Pyromet X-12 is a martensitic stainless steel offering high strength at both room temperature and high heat. It is recommended for use in jet engines, steam turbines and aircraft structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1965) 14 (3): SS-166.
Published: 01 March 1965
... F.V.520B is an improved martensitic stainless steel which has good corrosion resistance, weldability, and capacity of being hardened by low temperature heat treatment. It is recommended for steam turbine blades and aircraft components. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1981) 30 (12): SS-398.
Published: 01 December 1981
... CRUCIBLE 403 is a hardenable steel containing 11.50-13.00% chromium. Its composition and mill processing are controlled carefully to produce a product capable of meeting the severe requirements of steam turbine blading and other high-requirement uses. Crucible 403 is magnetic at all times...
Journal Articles
Alloy Digest (1972) 21 (12): SS-284.
Published: 01 December 1972
... tensile strength and good ductility. This alloy is recommended for applications such as steam turbine buckets, blades and bucket covers, as well as for casting in assemblies such as turbine diaphragms. Forms Available: Forging billets, forgings, bars, strip, wire and wire rods. Applications: Steam...
Journal Articles
Alloy Digest (1975) 24 (7): SS-313.
Published: 01 July 1975
... to corrosion in exhaust gases. It is used for sodium-filled aircraft valves. aircraft valve inserts. aircraft and steam turbine bolts. and various other automotive parts requiring high- temperature properties. Forms Available: Bars in the following conditions: hot rolled. rou& turned, cold drawn and centerless...
Journal Articles
Alloy Digest (1973) 22 (12): Ni-198.
Published: 01 December 1973
... is solid solution strengthened by the refractory metals niobium, tungsten and molybdenum. It possesses excellent corrosion properties, strength, ductility, toughness and structural stability. It is used as tubing and piping for steam and gas turbines, rocket engines, heat shields, furnace hardware...
Journal Articles
Alloy Digest (1964) 13 (6): Co-37.
Published: 01 June 1964
..., the high internal damping capacity of NIVCO can be used to advantage. Forms Available: Forgings, bar, sheet and wire, strip and place. Forged, rough turned billets up to 10 diameter. Round, center less ground bars. Applications: Steam turbine blades and uses where vibratory stresses are critical...
Journal Articles
Alloy Digest (2005) 54 (5): SS-928.
Published: 01 May 2005
... Resistance: NIROSTA 4120 is resistant to water with a low chlorine concen- tration in the precision machined or, better still, in the polished condition. The resistance to corrosion is a result of the addition of molybdenum, and due to that resistance the alloy is used in water and steam turbines. It also...
Journal Articles
Alloy Digest (1997) 46 (5): Fe-56.
Published: 01 May 1997
... components; in hot-work die applications. (such as extrusion dies). punches and mandrels; and in high-pressure hydrogen environments. Pyromet ClX- I also has excellent characteristics for applications such as ordnance hardware, steam turbine blades, gage blocks, springs, rocket thrust chambers and die...
Journal Articles
Alloy Digest (2006) 55 (5): Ti-138.
Published: 01 May 2006
... components. The alloy is also suitable for general engineering applications such as steam-turbine blades, axial and radial compressor parts, connecting rods, and other high-speed rotating and reciprocating components. Timetal 551 is not normally regarded as weldable. Producer: Timet Denver, CO 80202 (303...
Journal Articles
Alloy Digest (1964) 13 (6): SS-157.
Published: 01 June 1964
...: Uniloy 1409TB is turbine blade quality 12% chromium stainless steel developed for applications in turbine construction and is used extensively for steam turbine buckets and blades and gas turbine compressor wheels and blading. This alloy can be fabricated by practically all production methods...
Journal Articles
Alloy Digest (1966) 15 (9): Ni-117.
Published: 01 September 1966
... properties Pyromet 860 steam turbines tensile properties workability Filing Code: Ni-117 I 3 Nickel Alloy SEPTEMBER 1966 -DATA ON WORLD WIDE METALS AND ALLOYS PYROMET 860 (High Temperature Alloy) Pyromet 860 is a high temperature alloy with an unusual combination of strength and ductility...
Journal Articles
Alloy Digest (2007) 56 (12): SS-1004.
Published: 01 December 2007
... applications include compressor and turbine blades (aircraft, gas or steam turbines), compressor and turbine wheels, rotors, high- temperature bolting, valve trim, and other valve applications, and structural components for aircraft and missile applications. Producer: Crucible Service Centers Divisional...