1-16 of 16 Search Results for

steam turbine buckets

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (9): SS-463.
Published: 01 September 1985
... CARPENTER MOLY ASCOLOY is a chromium-nickel-molybdenum-vanadium hardenable martensitic stainless steel designed for service up to 1200 F (649 C). It is utilized in steam turbine buckets and in compressor components in gas turbines and in other high-temperature applications. This datasheet provides...
Journal Articles
Alloy Digest (1968) 17 (6): SS-210.
Published: 01 June 1968
... Carpenter Stainless No. 404 is recommended for highly stressed parts at temperatures up to 1050 F where joining is a problem. It is both hardenable and weldable. It is used for steam turbine buckets, blades and diaphrams. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1972) 21 (12): SS-284.
Published: 01 December 1972
... tensile strength and good ductility. This alloy is recommended for applications such as steam turbine buckets, blades and bucket covers, as well as for casting in assemblies such as turbine diaphragms. Forms Available: Forging billets, forgings, bars, strip, wire and wire rods. Applications: Steam...
Journal Articles
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
... AISI No. 616 is a hardenable martensitic type stainless steel recommended for high temperature applications up to 1200 F. It is used for steam turbine blades and buckets, valves, jet engine components, and high temperature bolting. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1958) 7 (3): SS-72.
Published: 01 March 1958
... to scaling and oxidation at temperatures up to 1400 deg F. Forms Available: Billets, hot rolled and cold finished bars special shapes, wire and cold rolled strip. Applications: High temperature bolting, steam turbine buckets and blades, bucket bands, locking pins, compressor blades, valve stems, etc. Feed...
Journal Articles
Alloy Digest (2022) 71 (12): SS-1354.
Published: 01 December 2022
...; wire rod; wire; strip Applications CarTech 410 is used for blades; bucket covers; fasteners; gas turbine compressor blades; machine parts; nuclear reactor control rod mechanisms; petrochemical equipment; pump parts; shafting; steam turbine buckets; valves. Supplier Carpenter Technology Corporation 1735...
Journal Articles
Alloy Digest (1988) 37 (8): SS-70.
Published: 01 August 1988
... and oxidizing acids. It has best resistance in the hardened and tempered condi- tion Specification Equivalents: AMS 5616 AISI No. 615 uNsNo.S418Oo Forms Available: Billets, hot rolled and cold fished bars, wire, cold rolled strip, special shapes. Applications: Steam turbine buckets and blades, gas turbine...
Journal Articles
Alloy Digest (1958) 7 (11): SS-81.
Published: 01 November 1958
... turbine buckets and blades, budtet bands, locking pins, compressor blades, valve stems, compressor wheels, turbine shafts. Manufacturer: Carpenter Steel Company Reading, Pennsylvania ...
Journal Articles
Alloy Digest (1964) 13 (6): SS-157.
Published: 01 June 1964
...: Uniloy 1409TB is turbine blade quality 12% chromium stainless steel developed for applications in turbine construction and is used extensively for steam turbine buckets and blades and gas turbine compressor wheels and blading. This alloy can be fabricated by practically all production methods...
Journal Articles
Alloy Digest (1955) 4 (6): SS-31.
Published: 01 June 1955
... not need to be protected against corrosion or oxida- tion throughout its range of saviccabiky. This ahoy is similar to Crucible s AIIoy 422. Forms Available: Bars, forging bilks, wire, sheet, strip, pIate, forgings, and special shapes Applications: Steam and gas turbine buckets, compressor and tur- bine...
Journal Articles
Alloy Digest (1992) 41 (2): SS-294.
Published: 01 February 1992
.../1400 F (649/77O C). Steam turbine compressor buckets and blades, high-tem- perature bolting, compressor and turbine wheels, valve trim and valves, aircraft components. Producers: Carpenter Technology Corporation Carpenter Steel Division Reading, Pennsylvania 19603 ...
Journal Articles
Alloy Digest (1992) 41 (2): SS-139.
Published: 01 February 1992
... (1038/ 1137 C). Avoid prolonged heating which can result in decarbtuization. Cool slowly after forging then anneal or temper, 1200/1400 F (649/77O C). Steam turbine compressor buckets and blades, high-tem- perature bolting, compressor and turbine wheels, valve trim and valves, aircraft components...
Journal Articles
Alloy Digest (1975) 24 (11): SS-319.
Published: 01 November 1975
.... Applications: Gas turbine and jet engine heat-resisting components such as rotor forgrngs. buckets, tail cones and bolts; aircraft exhaust manifolds and collector rings; components for steam service in- cluding valves and autoclaves; oil-refining and chemical-process equipment. Manufacturer: Universal Cyclops...
Journal Articles
Alloy Digest (1967) 16 (7): SS-196.
Published: 01 July 1967
... be used to improve the wear resistance of 419 alloy used in parts such as valve stems and bushings. The usual depth of nicriding is about 0.006- 0.008 inches; even thinner films will increase rhe notched-fatigue strength. Forms Available: Bars and sheet. Applications: Steam turbine blades and buckets...
Journal Articles
Alloy Digest (1958) 7 (9): SS-78.
Published: 01 September 1958
..., forgings, bars, special shapes. Applications: Jet engine and supercharger parts; compressor wheels and blades; bolts, nuts, and other fasteners; buckets and blades in steam turbines. Manufacturer: Firtb Sterling, Inc. Pittsburgh 30, Pennsylvania ...
Journal Articles
Alloy Digest (1976) 25 (6): SS-329.
Published: 01 June 1976
... corrosion throughout its application temperature range. Forms Available: Wets, bars, sheet, srrip. plate and Lvire. Applications: Components for jet engines; buckets for steam and gas turbines; discs; bolts; wheels. blades and structural components for aircraft and missiles; valves and valve trim...