Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (1): SS-579.
Published: 01 January 1995
...-579. Producer or source: Carpenter Technology Corporation. Producer or Source: Carpenter Technology Corporation Copyright ┬ę ASM International┬« 1996 1996 ASM International chemical composition elasticity physical properties stainless steel 304 SCQ thermal properties TYPE 304 SCQTM...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (2): SS-875.
Published: 01 February 2003
... applications in corrosive service in the as-welded condition. A special consumable remelted, non-free-machining version of Type 304 stainless is available as Type 304-SCQ. This special grade is advanta- geous for use in thin sections under high pressure or vacuum or to achieve optimal surface quality after...