Alloy Digest (1989) 38 (10): P-10.
Published: 01 October 1989
... ISOPLAST 101, unreinforced, is a rigid, amorphous polyurethane thermoplastic polymer. It is opaque and impact modified. It is injection moldable and extrudable. It is characterized by its high impact strength, high abrasion resistance, excellent chemical and solvent resistance and low moisture...
Journal Articles
Alloy Digest (1990) 39 (1): P-14.
Published: 01 January 1990
... and solvent resistance and high abrasion resistance. This datasheet provides information on physical properties, hardness, and tensile properties as well as fracture toughness. Filing Code: P-14. Producer or source: The Dow Chemical Company, Dow Plastics. Producer or Source: The Dow Chemical Company, Dow...
Journal Articles
Alloy Digest (1991) 40 (6): P-27.
Published: 01 June 1991
... chemical corrosion re- sistance. ULTEM 6000 resin has enhanced resistance to partiahy halogenated solvents. Machinability: ULTEM resins have excellent machining and Finishing characteristics. Processability: The combination of outstanding thermal, mechanical and electrical properties of ULTEM resin...
Journal Articles
Alloy Digest (1989) 38 (11): P-12.
Published: 01 November 1989
... for further particulars. lmo 2mo 3mo - - - ii: 92 - t; 84 104 90 90 :Fi 104 6mo 9mo 12 mo 72 100 62 63 101 97 fi i; 65 100 ;: 9 ; 91 87 SewiceinComsiveEnvimnments: Demkane 470-36 and 47045 vinyl ester resins have supe- rior resistance to a wide variety of chemicals and organic solvents and perform...
Journal Articles
Alloy Digest (2017) 66 (5): SS-1263.
Published: 01 May 2017
... containing sulfuric acid, chlorides, and nitric and phosphoric acid. The combination of high strength with good corrosion resistance in acidic environments makes Sanicro 32Cu a suitable grade for the production of gases, solvents, and organic and inorganic chemicals. Typical applications include flanges...
Journal Articles
Alloy Digest (1986) 35 (11): Cu-517.
Published: 01 November 1986
... industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-517. Producer or source: Copper and copper alloy...
Journal Articles
Alloy Digest (1989) 38 (10): P-11.
Published: 01 October 1989
... at temperatures not exceeding 70°C. General Characteristics: GRILON ELX23NZ has excellent strength, toughness and duc- tility; outstanding abrasion resistance and bearing characteris- tics; very good resistance to a wide range of chemicals, solvents, oils and greases. It can be easily processed using conventional...
Journal Articles
Alloy Digest (1980) 29 (4): Cu-393.
Published: 01 April 1980
... and seam resistance welding. Corrosion Resistance: Mueller alloy 3470 has good resistance to corrosion by most industrial, rural and marine atmospheres. It with- stands attack from dry gases, fresh water and seawater, petroleum products, organic solvents and sulfides. Prolonged contact with oxidizing acids...
Journal Articles
Alloy Digest (1986) 35 (4): Cu-503.
Published: 01 April 1986
... issimilar to that of the above family of spinodal alloys and the following four paragraphs are based on this assumptton. Copper Alloy No. C72800 shares with other copper-base alloys a high degree of corrosion resistance to a wide variety of compounds and solvents. atmospheres. fresh and salt waters. many...
Journal Articles
Alloy Digest (1979) 28 (9): Cu-379.
Published: 01 September 1979
...: Mueller alloy 3406 has good resistance to corrosion by most industrial, rural and marine atmospheres. It with- stands attack from dry gases, fresh water, seawater, petroleum products, organic solvents and sulphides. Prolonged contact with oxidizing acids, mercury com- pounds, moist ammonia, cyanides...
Journal Articles
Alloy Digest (1982) 31 (3): Cu-433.
Published: 01 March 1982
...- working properties but they are good enough to produce it readily. This alloy has excellent resistance to corrosion by most rural, industrial and marine atmospheres. It withstands attack from dry gases, fresh and seawater, petroleum products, organic solvents and sulphides. Copper Alloy No. C35300 has...
Journal Articles
Alloy Digest (1981) 30 (4): Cu-415.
Published: 01 April 1981
... by any thermal treatment but it can be hardened by cold working. It resists cor- rosive attack by most industrial, rural and marine at- mospheres. It also withstands attack by a number of materials such as organic solvents, seawater, petroleum products and dry gases. Its uses include a wide range...
Journal Articles
Alloy Digest (1975) 24 (9): Ni-221.
Published: 01 September 1975
... and corrosion resistance over a wide temperature range. The results of some wear and wear-corrosion tests are given in Tables 2 and 3. The Alpha wear tests (Table 2) were conducted in naphtha (Stoddard Solvent), a poor lubricant. Rider/ drum test data (Table 3) indicate that TRIBALOY T-700 has good resistance...
Journal Articles
Alloy Digest (1975) 24 (10): Co-73.
Published: 01 October 1975
... in Tables 2 and 3. The Alpha wear tests (Table 2) were conducted in naphtha (Stoddard Solvent), a poor lubricant. Rider/ drum test data (Table 3) indicate that TRIBALLY T-800 has superior resistance to wearcorrosion in 5% hydrochloric acid. Other experimental data show that the corrosion resis- tance of T...
Journal Articles
Alloy Digest (1980) 29 (7): Cu-398.
Published: 01 July 1980
... resistance to corrosion by most rural, industrial and marine atmospheres. It withstands attack from dry gases, fresh and seawater, petroleum products, organic solvents and sulphides. As mentioned in the introduction, Mueller alloy 3530 has excellent thread-rolling and knurling properties. It is used on screw...
Journal Articles
Alloy Digest (1980) 29 (7): SS-373.
Published: 01 July 1980
... RA 800H is an austenitic iron-base, heat-resistant alloy with excellent high-temperature strength and good resistance to oxidation in air up to 2000 F (1090 C). High creep-rupture properties are obtained by a solution-anneal treatment followed by a rapid cool; grain size is controlled in the range...
Journal Articles
Alloy Digest (1984) 33 (5): Cu-476.
Published: 01 May 1984
... excellent resistance to corrosion by most industrial, rural and marine atmospheres. It withstands attack from dry gases, fresh and seawater, petroleum products, organic solvents and sulphides. Prolonged contact with oxidizing acids, mercury compounds, moist ammonia, cyanides and strong bases should...
Journal Articles
Alloy Digest (1991) 40 (3): Cp-14.
Published: 01 March 1991
... heat aging. Chemical Resistance: Solvent exposure tests (14 day exposure) at 23 and 71°C in hydraulic fluid showed excellenr resistance in the as-consoli- dated condition. Specimens with machined surfaces lost 36% of their flexural strength under the same exposure conditions. For other solvents...
Journal Articles
Alloy Digest (1992) 41 (10): SS-535.
Published: 01 October 1992
... CARLSON C20 PLUS alloy is an austenitic stainless steel designed for improved resistance to reducing acids, particularly sulfuric acid. It finds wide use in all phases of the chemical industry and has good strength and fabricability for case in making process equipment and piping. This datasheet...
Journal Articles
Alloy Digest (1962) 11 (11): Ni-76.
Published: 01 November 1962
... satisfactory resistance under most conditions to acetate solvents, all strengths of acetic acid, alum, ammonium hydroxide, aniline dyes, boric acid, brine, calcium chloride, carbonic acid, chlorinated water, chromic and citric acids, fatty acids, mixed acids, phenol, concentrated phosphoric acid, potassium...