1-20 of 32 Search Results for

shipbuilding

Sort by
Journal Articles
Alloy Digest (1977) 26 (12): SA-339.
Published: 01 December 1977
... to weld other low-alloy steels and carbon steels; however, the weld metal may differ somewhat from 1/2% molybdenum because of weld-metal dilution. Uniflux V100 is used widely in shipbuilding to weld 1/2% molybdenum steel. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1978) 27 (6): CS-73.
Published: 01 June 1978
... Uniflux V70 is a continuous flux-cored welding electrode (wire) that is used to deposit carbon steel weld metal. Welding is protected by a shielding atmosphere of either 75% argon-25% carbon dioxide or 100% carbon dioxide. Uniflux V70 is used widely in shipbuilding and other fabricating industries...
Journal Articles
Alloy Digest (1979) 28 (2): SA-355.
Published: 01 February 1979
... is protected by a shielding atmosphere of either 75% argon-25% carbon dioxide or 100% carbon dioxide. Uniflux V90 is used widely in shipbuilding and other fabricating industries. It provides around 88,000 psi tensile strength and around 26 food-pounds Charpy V-notch impact at 60 F. This datasheet provides...
Journal Articles
Alloy Digest (1979) 28 (7): SA-362.
Published: 01 July 1979
.... It is used to deposit typically 2.40% nickel steel weld metal with good low-temperature impact properties. Uniflux 90 is used widely in shipbuilding and other fabricating industries. It provides around 85,000 psi tensile strength and around 25 foot-pounds Charpy V-notch impact at -60 F. This datasheet...
Journal Articles
Alloy Digest (1978) 27 (9): CS-74.
Published: 01 September 1978
... UNIFLUX 70 is a continuous flux-cored welding electrode (wire) for welding in carbon dioxide shielding gas in the flat groove and horizontal fillet positions. It is used widely in shipbuilding and other fabricating industries to weld carbon steel and provides around 82,000 psi tensile strength...
Journal Articles
Alloy Digest (1983) 32 (4): SA-389.
Published: 01 April 1983
...-grained steels with low-temperature toughness. Tri-Mark TM-811N2 is used to deposit typically 2.35% nickel steel weld metal with good low-temperature impact properties. It is used for shipbuilding, oil rigs and similar structures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2008) 57 (4): SA-578.
Published: 01 April 2008
... (agricultural and earthmoving equipment, cranes, lift trucks), the oil and gas industry (offshore drilling processing rigs), mining (draglines, continuous miners), transportation (railcars, shipbuilding), and construction (bridges specified by ASTM A709 Grade 50, buildings specified by ASTM A572 Grades 42...
Journal Articles
Alloy Digest (1960) 9 (4): Al-90.
Published: 01 April 1960
... Shipbuilding, structural parts where good strength and hardens rapidly, becoming extremely tough. It was corrosion resistance are required, welded boat hulls, developed qecially to meet the need for high strength guided missile containers, trusses, girders, truck and trailer frames. non-h& treatable alloy...
Journal Articles
Alloy Digest (1989) 38 (8): CS-125.
Published: 01 August 1989
...-7116 36-138 to 600 7/16-l l/4 36-150 to 600 Applications: Machinery designed for cold-weather use, shipbuilding, offshore drill rigs. Producer: Bethlehem Steel Corporation Bethlehem, Pennsylvania 18016 ...
Journal Articles
Alloy Digest (2013) 62 (8): SS-1152.
Published: 01 August 2013
... resistance and high yield strength. This alloy shows excellent weldability. Applications: Castings for severe corrosion service, e.g., in chemical and environmental facilities; offshore industry; shipbuilding; chemical industry; pulp and paper industry; seawater desalination plants with improved corrosion...
Journal Articles
Alloy Digest (2015) 64 (11): Cu-844.
Published: 01 November 2015
... components, defense equipment such as tank turret gearbox gears, periscopes and shipbuilding components, high performance IC engine bearing bushes and shafts, valve and pump trim, shafts, spindles and gears, marine shafts, bearing bushes and fasteners, electrical and hydraulic connectors, fasteners...
Journal Articles
Alloy Digest (2007) 56 (1): SS-983.
Published: 01 January 2007
..., polypropylene production, titanium dioxide production, caustic evaporators, equipment handling organic and fatty acids Marine industry and shipbuilding: rudders, shaft seals, pumps, valves, instrumentation, oil and chemical tankers Oil and gas industry: pumps, valves, pipe, vessels, wellhead equipment...
Journal Articles
Alloy Digest (2007) 56 (7): Ni-653.
Published: 01 July 2007
... heating. Product Forms Available: Bar Applications: In the chemical process industry, applications include processes involving organic acids, caustic soda, and dry chlorine; production of chlorinated plastics; and doctor blades and scrapers. In the marine industry and shipbuilding, applications include...
Journal Articles
Alloy Digest (2008) 57 (9): SS-1018.
Published: 01 September 2008
... Shipbuilding Chemical industry Pulp and paper industry Seawater desalination plants with improved corrosion resistance, e.g., high CPT and CCT resistance also in the as welded condition. Producer: Schmidt & Clemens, Inc. Houston, TX 77046 Tel: 713/629-7770 Fax: 713/629-7373 In Germany Schmidt + Clemens...
Journal Articles
Alloy Digest (2019) 68 (11): Cu-900.
Published: 01 November 2019
... stuffing box nuts. Typical marine uses include shipbuilding, covers for marine hardware, marine applications, and marine hardware. Typical industrial uses include machine parts, glass molds, welding jaws, wear plates, aircraft components, pickling equipment, valve guides/seat/bodies, piston guides, pump...
Journal Articles
Alloy Digest (2012) 61 (12): SS-1129.
Published: 01 December 2012
... utilization of this alloy is for fasteners and actuators in the following industrial applications: Chemical process industry sulfuric acid production, nitric acid processes, polythionic acid resistance, urea production, equipment handling organic and fatty acids Marine industry and shipbuilding pumps...
Journal Articles
Alloy Digest (2002) 51 (5): Al-377.
Published: 01 May 2002
... in the automotive industry include wheels for shear strength, fatigue, and high temperature welding 5454 to 5454, 5454 to 6061, and A356 to 5454, and also frame sections for welding 6061 to 6061. Shipbuilding applications include desalination units for corrosion and high temperature welding 5454 to 5454 and 5052...
Journal Articles
Alloy Digest (2003) 52 (1): Al-384.
Published: 01 January 2003
... 45 179 26 12 DOI: 10.31399/asm.ad.al0384 Applications: Shipbuilding applications include welding 5083 to itself for struc- tural frames, skin, structural plate, and liquid natural gas (LNG) tanks. Recreation applications include welding 7005 to itself and welding 7046 to itself for bicycle frames...
Journal Articles
Alloy Digest (2007) 56 (6): Ni-651.
Published: 01 June 2007
...: Applications include the chemical process industry for sulfuric acid production, hydrochloric acid processes, hydrofluoric and fluorosilicate acid processes, and fatty acid production; marine industry and shipbuilding; propellers and shafts; fasteners; the oil and gas industry for pumps, valves, crude...
Journal Articles
Alloy Digest (2008) 57 (4): SS-1010.
Published: 01 April 2008
... and shipbuilding (rudders, shaft seals, pumps, valves, instrumentation, oil and chemical tankers) Oil and gas industry (pumps, valves, pipe, vessels, wellhead equipment, subset equipment) Pollution control (fans and pumps, wet scrubbers, incinerators) Copper smelting (induced draft, or ID, fans, tuyere bars...