Alloy Digest (1987) 36 (9): Ni-351.
Published: 01 September 1987
... NIMONIC alloy 86 is a nickel-base high-temperature alloy with exceptionally good cyclic oxidation resistance at 1050 C (1922 F). The alloy has good workability, ductility and weldability. It is intended principally for use in sheet form. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (10): TS-198.
Published: 01 October 1967
... International chemical composition compressive strength elasticity fracture toughness hardness heat treatability Huron joinability machinability physical properties sheet workability workability Filing Code: TS-198 Tool Steel OCTOBER 1967 -DATA ON WORLD WIDE METALS AND AL- - _ - HURON Pdlisbd...
Journal Articles
Alloy Digest (1957) 6 (12): Ni-38.
Published: 01 December 1957
... to permit the two materials to be joined without special provision for thermal expansion. Forms Available: Bars, forgings, and sheets. Workability: Applications: Incoloy 901 is workable, both hot and cold. The major part of forging should be done between 2050 deg F. and 1850 deg F. metal temperarure. Light...
Journal Articles
Alloy Digest (1987) 36 (2): TS-470.
Published: 01 February 1987
... treatability machinability physical properties plates sheets workability UNS T30402 DOI: 10.31399/asm.ad.ts0470 Copyright © ASM International® 1996 All QI6BSTOr - ATMODIE DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: TS-470 Tool Steel FEBRUARY 1987 Puhlishrd hr 4lloy Digest. Inc. 27 Canfield...
Journal Articles
Alloy Digest (1981) 30 (12): SS-398.
Published: 01 December 1981
... information is given in the CRUCIBLE MACHINABILITY DATA SHEET. Workability: Hot Working: CRUCIBLE 403 should be forged at 2050 to 2150°F and fished not lower than 1400°F. Reheating should be used if necessary. When CRUCIBLE 403 is to be upset, temperatures should be such that the work is completed be- tween...
Journal Articles
Alloy Digest (1988) 37 (6): Al-289.
Published: 01 June 1988
... on laboratory tests of specimens exposed to the 3.5Y~ NaCl alternate immersion test and on service experience is excellent. There are no known instances of failure. Specification Equivalents: ASTM B 209 General Characteristics: AA 3 I05 is a non-heat treatable aluminum sheet alloy. It has good workability...
Journal Articles
Alloy Digest (2015) 64 (2): SS-1201.
Published: 01 February 2015
... treatment is solution treatment 1100 1150 °C (2012 2102 °F) then rapid cooling. Workability: Workability and formability is basically equal to that of Type 304. LDR (Limiting Draw Ratio), sheet thickness 0.7 mm (0.03 in.) NAS NM17, Erichsen value 11.5 mm (0.45 in.) 2.0 NAS 302, Erichsen value 12.0 mm (0.47...
Journal Articles
Alloy Digest (1974) 23 (4): Al-51.
Published: 01 April 1974
... ALUMINUM 3004 is nominally an aluminum-manganese-magnesium alloy which cannot be hardened by heat treatment; however, it can be strain hardened by cold working. It has higher strength than Aluminum 3003 and good workability, weldability and resistance to corrosion. This datasheet provides...
Journal Articles
Alloy Digest (1990) 39 (11): Al-309.
Published: 01 November 1990
... resistance weldability is good in both the annealed and hardened tempers. Fusion weldability is diffi- cult Cold workability is limited. Forms Available: Sheet & plate, tubing, extrusions, rolled or cold finishedrod/bar/ wire, rivers. forgings and forging stock. Applications: Aircraft and other structures...
Journal Articles
Alloy Digest (1991) 40 (5): Al-316.
Published: 01 May 1991
... Copyright © ASM International® 1996 1996 ASM International Aluminum alloys 5456 chemical composition elasticity hardness heat treatability joinability low-temperature alloys machinability physical properties shear strength tensile properties workability wrought aluminum alloys UNS A95456...
Journal Articles
Alloy Digest (1996) 45 (6): SS-647.
Published: 01 June 1996
...°C At 200°C At 300 C At 400°C 7.7 55 460 0.60 Present 10.5 11 il.5 12 II 220 215 210 205 200 Heat Treatment: -w T 750-850 Workability: The cold workability (e.g.. bending, flanging, deep drawing) of Remanit 4589 largely depends on the thickness of the material. With cold-rolled strip and sheet...
Journal Articles
Alloy Digest (2005) 54 (1): Fe-135.
Published: 01 January 2005
... nonoriented silicon steel sheet. The suitable frequency range is 5 40 kHz. The mate- rial has a high saturation induction and good workability. Ability to stamp, ability to bend, and ability to weld are all good. JNHF-Core is one of two types of JFE Super-Core material used for the core materials...
Journal Articles
Alloy Digest (1972) 21 (8): Be-2.
Published: 01 August 1972
... by climb milling with spiral cutters. Workability: Workability is a function of sheet width and thickness. Beryllium is usuallv formed in the range 1250-135OoF and in this range easily takes a ST bend. If the part is formed at 13OOoF or above, it is usually not necessary to apply a stress relief treatment...
Journal Articles
Alloy Digest (1991) 40 (6): Al-317.
Published: 01 June 1991
... is rated D. Workability: Cold workability of AA 5657 rates B for II25 temper and C for H28 temper on a scale of A through D. Rec- ommended minimum bend radii for 90 cold forming of sheet (l/32 thick) is 0 for II25 temper and 1 1/2t for H23 temper. For sheet l/16 thick, the minimum bend radius for II25...
Journal Articles
Alloy Digest (2008) 57 (5): Al-413.
Published: 01 May 2008
... Kaiser aluminum alloy 2124 is a high-purity version of 2024 with tighter controls on the iron and silicon for an increase in strength and toughness. It is primarily used as plate in the aircraft industry. This data sheet applies to sheet, coil, and plate in the T851 temper. This datasheet provides...
Journal Articles
Alloy Digest (1990) 39 (8): Al-306.
Published: 01 August 1990
... or fusion welding of M7178. Corrosion resistance is average in light sec- tions but decreases in heavy sections. Cold workability of M 7178 is limited. Forn~s Available: Sheet and plate, extruded wire, rod, bar and shapes; rolled or cold finished rod and wire. Applications: Aircraft and other structures...
Journal Articles
Alloy Digest (1970) 19 (5): Al-196.
Published: 01 May 1970
... Aluminum 3105 is a non-heat treatable aluminum alloy sheet material having excellent weldability, formability and corrosion resistance. It is recommended for appliances, trim and containers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1995) 44 (10): SS-615.
Published: 01 October 1995
... REMANIT 4003 possesses good workability, weldability and is mainly used in the transportation industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat...
Journal Articles
Alloy Digest (1997) 46 (9): SS-697.
Published: 01 September 1997
.... saucnue is ferritic. Workability: Cold workability (bending, flanging, spinning. and deep draw- ing) largely depends on the ma&al thic&zss. Fiie grain smtc- tnre and accompanying toughness makes is easy to cold work cold-rolled sheet and strip up to 3 mm thick However. sharp-an- gled flanges parallel...
Journal Articles
Alloy Digest (2014) 63 (6): Ti-156.
Published: 01 June 2014
... 20 Sheet, typical 30 Bend radius Annealed, minimum 4T Sheet, typical < 2T Typical mechanical properties are shown in Table 1 and Fig. 1. Workability: See Table 2 for typical cold forming properties of sheet. Corrosion Resistance: Corrosion rate, mm/y (mpy) Hydrochloric acid, 1%, boiling 2.05 (80.6...