Journal Articles
Alloy Digest (2007) 56 (5): TS-648.
Published: 01 May 2007
... Toughtec SF is a spray-formed cold-work tool steel offering a combination of high wear resistance and very good ductility. Toughtec SF is suitable for the production of hot shearing dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive...
Journal Articles
Alloy Digest (1981) 30 (8): TS-385.
Published: 01 August 1981
... many applications include blanking dies, coining, cold shears and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-385. Producer or source: Jessop Steel...
Journal Articles
Alloy Digest (1981) 30 (4): TS-381.
Published: 01 April 1981
... be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information...
Journal Articles
Alloy Digest (1969) 18 (4): TS-217.
Published: 01 April 1969
... EB alloy is a high-carbon chromium alloy steel for general hot-work applications. It possesses good compressive strength and hot mechanical properties. It is recommended for hot header and gripper dies, shear blades, hot rivet sets, forging dies, cold forming and embossing dies. This datasheet...
Journal Articles
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... without fear of cracking. Among its many applications are forging dies, hot-extrusion mandrels, hot-shear blades, die-casting dies and hot punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1986) 35 (1): TS-453.
Published: 01 January 1986
... checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides...
Journal Articles
Alloy Digest (1986) 35 (3): TS-455.
Published: 01 March 1986
... will withstand repeated heating to 700-800 F, when used in lower temperature hot-work applications. Among its many uses are shear blades, hand chisels, pneumatic tools, coining dies, hot-heading dies, forging dies and machine parts. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1986) 35 (11): TS-465.
Published: 01 November 1986
...-work applications. Another feature of this versatile die steel is its outstanding secondary hardness associated with remarkable tempering resistance up to 900 F. Typical applications comprise blanking dies, swaging dies, hot and cold-piercing punches, forming rolls, shear blades and coining dies...
Journal Articles
Alloy Digest (1981) 30 (9): TS-386.
Published: 01 September 1981
... are blanking dies, cold-forming dies, punches and cold and hot shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-386. Producer or source...
Journal Articles
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
... HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements...
Journal Articles
Alloy Digest (1969) 18 (6): TS-220.
Published: 01 June 1969
... AISI Type A10 is a high-carbon graphitic tool steel capable of developing high hardness and wear resistance. It is recommended for shear blades, blanking and forming dies, drawing dies and wear plates. This datasheet provides information on composition and hardness as well as fracture toughness...
Journal Articles
Alloy Digest (1985) 34 (2): TS-435.
Published: 01 February 1985
... excellent non-deforming characteristics. It is well suited for applications requiring toughness and fairly high resistance to abrasion. Typical applications for AIRKOOL include blanking dies, forming dies, punches and shear blades. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1985) 34 (3): TS-437.
Published: 01 March 1985
... of chromium and molybdenum. It is used for both cold and hot tooling applications. Its many uses include shear blades, swaging dies, chisels and dies for molding plastics below 1000 F (538 C). This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1986) 35 (9): TS-462.
Published: 01 September 1986
...), hot-heading dies, forging dies, hot punches and heavy shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-462. Producer or source: Columbia Tool Steel...
Journal Articles
Alloy Digest (2010) 59 (11): TS-694.
Published: 01 November 2010
... Thermodur 2714 is a tough die steel with high tempering resistance and good through hardening. Typical applications include forging dies, mandrels, die holders, armored trim dies, and hot-shear blades. This datasheet provides information on composition, physical properties, and hardness. It also...
Journal Articles
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... shear strength tensile strength workability - DATA ON WORLD WIDE METALS AND ALLOY! I Filing Code: Zn-3 DI - METAL 3 Zinc Alloy JUNE 1956 DI-METAL 3 (Zinc-Base Die Casting Alloy) DI-METAI. 3 is a zinc-base alk of hiah fluidity camable of producing fine detail in die casting alloys, die -dogs...
Journal Articles
Alloy Digest (1957) 6 (4): Zn-4.
Published: 01 April 1957
... No. 2 DIE METAL is a zinc-base alloy recommended primarily for die castings and sand castings (stamping and drop-hammer dies). This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness and fatigue...
Journal Articles
Alloy Digest (1978) 27 (8): TS-336.
Published: 01 August 1978
... tool and die steel of the high-carbon, high-chromium type. It is characterized by high resistance to abrasion, fair toughness, minimum distortion in hardening and high compressive strength. Its many uses include a wide range of cutting and forming dies, rolls, reamers, plug gages and shear blades...
Journal Articles
Alloy Digest (1978) 27 (11): TS-341.
Published: 01 November 1978
... UNS No. T30402 is an air-hardening high-carbon, high-chromium cold-work die steel that offers excellent wear resistance. It is a deep-hardening steel but hardens with a minimum change in size and volume. Typical uses are cold-work dies, slitting cutters, shear blades and wood-working tools...
Journal Articles
Alloy Digest (1979) 28 (3): TS-346.
Published: 01 March 1979
... CYCLOPS SCK is a cold-work tool steel with a balanced composition to provide air hardening and an optimum combination of toughness, wear resistance and minimum distortion during heat treatment. Typical applications are shear blades, trimming dies and forming rolls, including grade rolls...