Alloy Digest (1976) 25 (3): SS-326.
Published: 01 March 1976
... AQUAMET 17 is a precipitation-hardening stainless steel that provides the best combination of strength, toughness, wear resistance and corrosion resistance available for shafting where extra strength and precision straightness are needed. It is in wide use in various types of boats. This datasheet...
Journal Articles
Alloy Digest (1976) 25 (8): SS-332.
Published: 01 August 1976
... physical properties tensile properties AQUAMET 18 Filing Code: SS-332 Stainless Steer AUGUST 1976 - DATA ON WORLD WIDE METALS AND ALLOYS ACNJAMET* 18 (Shafting Material for Boats, Pumps and Valves) +blisbed by EagkmngAUoysDigut,IIK. Upper Monalair, New Jersey AQUAMET 18 is a low-nickel austenitic...
Journal Articles
Alloy Digest (1977) 26 (4): SS-338.
Published: 01 April 1977
... AQUAMET 22 is an austenitic stainless steel with an outstanding combination of strength, toughness and corrosion resistance. Its corrosion resistance is equal to or better than any other boat shafting material, even better than most high-nickel alloys. It is the best material available...
Journal Articles
Alloy Digest (1979) 28 (5): Cu-373.
Published: 01 May 1979
... BUNTING Alloy 937 is a cast bushing and bearing bronze. It is one of the most satisfactory materials to use where shaft alignments or shaft wear is a problem. It has a good load capacity and excellent anti-friction characteristics. Its many uses include pressure-tight castings, corrosion-resistant...
Journal Articles
Alloy Digest (1980) 29 (3): CS-82.
Published: 01 March 1980
... AISI 1139 is a carbon steel containing 1.35-1.65% manganese and 0.13-0.20% sulfur to furnish free-machining characteristics. It is recommended especially for high-production machined products. Among its many applications are splined shafts, screws, arbors, tool holders and propeller shafts...
Journal Articles
Alloy Digest (1983) 32 (10): CS-97.
Published: 01 October 1983
... ductility and toughness are fairly good but in the transverse direction they tend to be low. Its many uses include spline shafts, mine-car axles and shafts, gears, bolts, tool holders and tie-rods. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1983) 32 (11): CS-98.
Published: 01 November 1983
... in the longitudinal direction, but they tend to be low in the transverse direction. The many uses of AISI 1144 include mine-car axles and shafts, screws, propeller shafts, ball joints, bushings, bolts and gears. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1994) 43 (8): SA-212.
Published: 01 August 1994
... LEDLOY 4140 is a lead and/or tellurized chromium-molybdenum alloy steel having free cutting characteristics. It is recommended for gears, shafts, fasteners and similar machinery parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1995) 44 (5): SS-595.
Published: 01 May 1995
... SOLEIL C5 is a 13% chromium 4% nickel martensitic stainless steel with improved toughness and good corrosion resistance to fresh water. Shafts and compressor impellers for hydraulic applications is the area of primary usage. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1995) 44 (6): Cu-601.
Published: 01 June 1995
... HIDURON alloy 191 was developed for marine applications where both a combination of strength and good corrosion/ impingement resistance is needed. It finds applications in shafts, fasteners and valve stems. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1995) 44 (7): SS-599.
Published: 01 July 1995
... BioDur TrimRite Stainless has a composition that is balanced to be fully martensitic in the hardened condition. The alloy possesses a moderately high level of corrosion resistance and is applied as valve parts, guides, shafting and cutlery, including surgical tools. This datasheet provides...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-495.
Published: 01 January 1996
... Colmonoy No. 635, a Nickel-base hard surfacing Alloy, contains a formulated mixture of both crushed and atomized powders. It achieves a hardness of RC 58-63 with tungsten carbide particles. Typical applications include hardfacing of pump components and shaft sleeves. It is supplied as a powder...
Journal Articles
Alloy Digest (1997) 46 (6): SS-409.
Published: 01 June 1997
... operations where longer tool life results in more productive machining time. Applications include shafts, valve bodies, valves, valve trim, and fittings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1962) 11 (8): SA-133.
Published: 01 August 1962
... Hy-Ten B Temper No. 2 is a low-chromium medium-carbon steel combining strength, toughness and wear resistance. It is recommended for gears, rolls, shafts and other machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1962) 11 (10): SA-136.
Published: 01 October 1962
... AISI 4422 is a carbon-molybdenum type carburizing steel designed as alternate for the AISI 8600 grades of steel for single quench practice. It is recommended for case hardened gears, pinions, shafts and the like. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1963) 12 (1): Cu-124.
Published: 01 January 1963
... Ni-Bral nickel-aluminum bronze is a material having high strength and good corrosion resistance. It is recommended for marine propellers, impellers, valves, gears, and shafting. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1963) 12 (5): Cu-128.
Published: 01 May 1963
... AMPCOLOY 45 is a high strength, extra tough bronze for machine tool parts, gears, shafts, etc. It is heat treatable and has excellent to corrosion, wear and abrasion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1964) 13 (5): SA-164.
Published: 01 May 1964
... Jessop-Saville H.27 is a medium carbon, chromium-molybdenum nitriding steel recommended for components subjected to heavy stresses and severe wear, such as crankshafts and air-screw shafts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1964) 13 (6): SS-156.
Published: 01 June 1964
... AISI No. 630 is a precipitation hardening stainless steel which is used in a variety of applications requiring strength combined with corrosion resistance. It is recommended for chemical process equipment, valve parts, aircraft fittings, pump shafts, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1964) 13 (9): TS-151.
Published: 01 September 1964
... Heppenstall 6H55 is a medium carbon, alloy tool steel recommended for dies, gears, and shafting where toughness and abrasion are factors of performance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...