Alloy Digest (2016) 65 (12): Pd-2.
Published: 01 December 2016
... Paliney H3C is a palladium, copper and silver based alloy designed for applications such as semiconductor test probes where extreme hardness and higher levels of electrical conductivity are required. This datasheet provides information on physical properties, hardness, elasticity, and tensile...