Alloy Digest (1964) 13 (1): CI-32.
Published: 01 January 1964
... MEEHANITE-GD is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1954) 3 (1): CI-5.
Published: 01 January 1954
... MEEHANITE GA is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, and housings. This datasheet provides information...
Journal Articles
Alloy Digest (1954) 3 (9): CI-8.
Published: 01 September 1954
... MEEHANITE GC is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, permanent molds, lathe beds, bases, pistons...
Journal Articles
Alloy Digest (1955) 4 (10): CI-12.
Published: 01 October 1955
... MEEHANITE GE is a medium strength iron having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, pump bodies, valve bodies, steam cylinders, cylinder...
Journal Articles
Alloy Digest (1958) 7 (9): CI-22.
Published: 01 September 1958
... MEEHANITE GB is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, lathe beds, bases, pistons, crankshafts...
Journal Articles
Alloy Digest (1975) 24 (4): TS-287.
Published: 01 April 1975
... where its self-lubricating quality is advantageous. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code...
Journal Articles
Alloy Digest (1971) 20 (12): Cu-246.
Published: 01 December 1971
... by Engineering Alloys Digest, Inc Upper Montclair, New Jersey COMPO H (Self-lubricated Bearina Allov) COMPO H is an oil-impregnated sintered bronze, produced by powder metallurgy (P/M) techniques, which is widely used in automotive, applicance, farm equipment, and aircraft industry applications. Composition...
Journal Articles
Alloy Digest (2000) 49 (4): TS-576.
Published: 01 April 2000
..., and completely processed in the United States. The alloy is a remarkably tough, long-lasting die steel with excellent high-temperature physical properties and self-lubricating quantities. Cuprodie 2 resists abrasion, heat checking, and washing, and offers excellent machinability. Finkl Cuprodie 2 is forged...
Journal Articles
Alloy Digest (2002) 51 (7): SS-857.
Published: 01 July 2002
... (0) 114 220 1272 (fax) Houston USA Office: (713) 849-0464 (713) 466-0639 (fax) ISSN: 002-614X SS-857B Fig. 3 SCC performance in 32% MgCl at 120 °C (248 °F) Fig. 4 Self-mated test, ASTM G 98, button-on-block. Standard test condi- tions, contact area = 123 mm2, no lubricant, 4.5 in. IF connections...
Journal Articles
Alloy Digest (1971) 20 (4): Pb-7.
Published: 01 April 1971
..., and lead-headed nails. The self-lubricating characteristics result in its use as bearing plates on bridges and as a drawing lubricant for wire and sheet metal. In powder form, it is used in lubricating greases and pipe joint compounds. Pound for pound, lead is a better sound barrier than any other...
Journal Articles
Alloy Digest (1965) 14 (3): TS-161.
Published: 01 March 1965
... Bethlehem O-6 is a graphitic, oil-hardening tool steel recommended where optimum machinability is desired for forming, shaping and drawing tools and dies, and where its inherent self-lubricating effect is advantageous. This datasheet provides information on composition and hardness as well...
Journal Articles
Alloy Digest (1972) 21 (9): Cu-258.
Published: 01 September 1972
... and gritly surroundings, or where a liquid other than oil is used as the lubricant. It is produced in three grades: B-4, B-8 and B-10. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-324.
Published: 01 December 1976
... and gritty surroundings, or where a liquid other than oil is used as the lubricant. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on casting, heat treating...
Journal Articles
Alloy Digest (1992) 41 (3): P-33.
Published: 01 March 1992
... ULTEM 4001 is an unreinforced polyetherimide resin with an internal lubricant. It is wear resistant and it has a reduced coefficient of friction. See also ULTEM 4000 (Alloy Digest CP-21, March 1992) for reinforced resin properties. ULTEM 4001 is available in opaque colors only. This datasheet...
Journal Articles
Alloy Digest (1972) 21 (2): Zn-13.
Published: 01 February 1972
... TITANALOY is a zinc-base alloy containing copper and titanium. It can be readily formed, joined, and finished and is stronger and more dent resistant than the more common zinc alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1992) 41 (3): Cp-21.
Published: 01 March 1992
... ULTEM 4000 is a reinforced polyetherimide resin with an internal lubricant. It is wear resistant and has a reduced coefficient of friction. See also ULTEM 4001 for unreinforced resin properties (Filing code P-33, 3/92). This datasheet provides information on physical properties, hardness, tensile...
Journal Articles
Alloy Digest (1976) 25 (6): Mo-12.
Published: 01 June 1976
... limitation. in. (Flat Surface) Surface roughness, microinches aa As sprayed Ground, 60-grit Sic wheel Ground, 400-grit diamond wheel Lapped Coefficient of friction, against oil- lubricated, hardened steel surface *Using 3MB Plasma Spray Gun. PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES (Plasma Spray...
Journal Articles
Alloy Digest (1976) 25 (4): Ni-225.
Published: 01 April 1976
... properties powder metal products tensile properties wear resistance METCO 447 Filing Code: Ni-225 Nickel Alloy APRIL 1976 - DATA ON WORLD WIDE METALS AND ALLOYS - kkblisbd by Engineering Alloys Digest, Iac. Upper Montclair. New Jew METCO* 447 (Self-Bonding Nickel-Base Powder for Sprayed Coatings) METCO...
Journal Articles
Alloy Digest (1961) 10 (10): Cu-108.
Published: 01 October 1961
... properties, high mechanical properties and good corrosion resistance. It is a free-cutting bearing bronze with self- aligning properties and excellent wear re- sistance. It is superior in many respects to cast materials and has better corrosion re- sistance than phosphor bronze in contact with many corrosive...
Journal Articles
Alloy Digest (1983) 32 (5): Zr-10.
Published: 01 May 1983
..., the excellent corrosion resistance of this metal depends on the specific properties of its self-healing. protective film of zirconium oxide. It can be fabricated readily by machining, grinding, forming and welding. As mentioned above Zircadyne 706 has corrosion resistance similar to that of tircadyne 705...