Alloy Digest (1997) 46 (12): Ni-532.
Published: 01 December 1997
... MAT 21 is a nickel-20 chromium-20 molybdenum-2 tantalum alloy. The very high molybdenum and tantalum content gives excellent general, pitting, and crevice corrosion resistance. The alloy was developed to be resistant to sulfuric acid dew point corrosion. Applications include scrubbers for flue gas...
Journal Articles
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
... 304, 316, and 317L stainless steels. Its many uses include marine scrubbers, desalination equipment, sulfuric acid production, wet phosphoric acid production, mild sour gas wells, urea production, and applications in the pulp and paper industry. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1982) 31 (3): SS-403.
Published: 01 March 1982
... higher than that of the common austenitic stainless steels. CRONIFER 1925 HMo has good strength and ductility, high impact values and good weldability. Its applications include heat exchangers for use with salt water, bleaching-plant equipment and flue-gas scrubbers. This datasheet provides information...
Journal Articles
Alloy Digest (1982) 31 (3): SS-404.
Published: 01 March 1982
... carbon content for good resistance to intergranular corrosion after welding or stress relieving. Typical applications include pulp and paper plants and flue gas desulfurication scrubbers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1983) 32 (12): Ni-295.
Published: 01 December 1983
... and sulfuric acids. It is used for flue-gas scrubbers. In various acidic and alkaline environments, alloy G is used for its high level of resistance to pitting and stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1982) 31 (12): SS-417.
Published: 01 December 1982
... has good strength, toughness, and weldability; it also tough at sub-zero temperatures after welding. Its uses include scrubbers, condensers and heat exchangers in plants that use seawater or other chloride-containing solutions This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1983) 32 (4): Ni-285.
Published: 01 April 1983
... scrubbers. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-285. Producer or source: Jessop Steel Company. Producer...
Journal Articles
Alloy Digest (1984) 33 (5): SS-445.
Published: 01 May 1984
.... In addition, its high nitrogen content results in superior strength when compared with other austenitic stainless steels. Typical applications for Avesta 254 SMO involve seawater contact, scrubbers and high-halide level tanks and piping. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1994) 43 (5): SS-566.
Published: 01 May 1994
... URANUS 52N is a nitrogen-alloyed duplex stainless steel improved in stress-corrosion cracking resistance and with pitting and crevice corrosion resistance better than AISI Type 317L. Applications include handling phosphoric acid contaminated with chlorides and in flue gas desulfurization scrubbers...
Journal Articles
Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
... and 317L stainless steels. Its many uses include marine scrubbers, desalination equipment, sulfuric acid production, wet phosphoric acid production, mild sour gas wells, urea production and pulp and paper industry. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1992) 41 (12): Ni-419.
Published: 01 December 1992
..., evaporators, pumps, piping, valves, vessels, expansion bellows, tank trucks, scrubbers, condensers, tank and vessel linings; and for processing and handling sulfuric acid, phospho- ric acid, hydrofluoric acid, nitric acid, nitrates and oxi- dizing salts. 9 Pulp and Paper - wet scrubber linings in systems...
Journal Articles
Alloy Digest (1985) 34 (3): Ni-311.
Published: 01 March 1985
.... Table 4 - CORROSION IN SCRUBBER SLURRY, MAXIMUM PITTING OR CREVICE ATTACK* [Units are mpy (mm/yr)] Scrubber Under Spray Scrubber Hold Material Bottom Nozzles Outlet Tank AlSl 316 5 (.13) 7 (.18) Alloy 825 <2 (< .03) 49 (1.25 2 (05) 1.2 (.03) 49 (1.25 nil Alloy 625 nil nil 26 (.65) nil Alloy C-276 nil...
Journal Articles
Alloy Digest (1992) 41 (9): Ni-411.
Published: 01 September 1992
..., phenol, styrene, vinyl chloride, chlorine and other chemicals. Pulp and Paper - bleaching, head boxes, and waster-gas scrubbers. Air Pollution Control - power plant scrubbers and re- lated equipment, elastrostatic precipitators, reheaters, waster-heat recovery systems, industrial boiler scrubbers, marine...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... good resistance to commercial fume scrubber and wet process phosphoric acid environments. based on field tests. Pitting and Crevice Corrosion Resistance: Both laboratory and field tests have demonstrated the high level of pitting and crevice corrosion resistance possessed by Carpenter 20Mo-6stainless...
Journal Articles
Alloy Digest (2008) 57 (4): SS-1010.
Published: 01 April 2008
... and shipbuilding (rudders, shaft seals, pumps, valves, instrumentation, oil and chemical tankers) Oil and gas industry (pumps, valves, pipe, vessels, wellhead equipment, subset equipment) Pollution control (fans and pumps, wet scrubbers, incinerators) Copper smelting (induced draft, or ID, fans, tuyere bars...
Journal Articles
Alloy Digest (2013) 62 (1): SS-1133.
Published: 01 January 2013
... control fans and pumps, wet scrubbers, incinerators Copper smelting ID fans, tuyere bars, wet scrubbers, leaching area precipitators Pulp and paper industry digester blow valves, rotary feed valves, ID fans, brownstock washers, precipitators, bleaching components Food industry sugar cane...
Journal Articles
Alloy Digest (1995) 44 (4): SS-592.
Published: 01 April 1995
... be- haves particularly well in abrasion-corrosion conditions. Mixed acids associated with chloride and flour&. additions are encountered in pollution control equipment. Due to high chro- mium and molybdenum levels associated with copper addi- tions, URANUS 52N+ behaves well in scrubber systems. In the pulp...
Journal Articles
Alloy Digest (2021) 70 (8): Ni-774.
Published: 01 August 2021
... Inconel G-3 is particularly suitable for handling chloride (as NaCl), pH 5.0, 58 °C (135 °F), simulated SO2 scrubber reducing acids such as phosphoric and sulfuric. It is used in environment for 30 days. flue gas desulfurization systems (scrubbers), especially in quencher, damper, and outlet ducting areas...
Journal Articles
Alloy Digest (2001) 50 (7): SS-465.
Published: 01 July 2001
... in the bodies, struc- tural members, and internals for scrubbers for flue-gas desulfurization. It is also a versatile and cost-effective material in a wide range of chemical processing applications requiring a stainless steel with corrosion resistance better than that of 316L and 317L. The corrosion resistance...
Journal Articles
Alloy Digest (1989) 38 (1): SS-502.
Published: 01 January 1989
... on life-cost basis in a variety of highly corrosive environments. They have been used in flue gas desulfuri- ration scrubber systems; in chemical and petrochemical processing equipmenS and in pulp and paper mills. Manufacturer: Jessop Steel Company Washington, Pennsylvania 15301. ...