Alloy Digest (1983) 32 (1): Cu-451.
Published: 01 January 1983
... MUELLER Alloy 3140 is a high-copper alloy with moderate strength, a rich bronze color and excellent corrosion resistance. Its lead content gives it excellent machinability which makes it suitable for screw-machine applications. Its uses include many screw-machine products, decorative hardware...
Journal Articles
Alloy Digest (1985) 34 (1): Cu-489.
Published: 01 January 1985
... MUELLER Alloy 3602 is a leaded brass of moderate strength and ductility. It is suitable for moderate thread rolling. Also, because of its free-cutting characteristics, it is suitable for high-speed screw-machine products. Among its many applications are hardware, unions, bolts, screws and nuts...
Journal Articles
Alloy Digest (1994) 43 (6): SA-176.
Published: 01 June 1994
... LEDLOY-A is a leaded, low-carbon free-machining steel recommended for high production automatic screw machine products. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (1981) 30 (6): SS-387.
Published: 01 June 1981
... a uniquely soft and machinable sulfide inclusion. This grade is non-magnetic in the annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides...
Journal Articles
Alloy Digest (1981) 30 (2): SS-380.
Published: 01 February 1981
... conditions. Typical applications are screw-machine products and all machined parts requiring good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (1982) 31 (11): Cu-447.
Published: 01 November 1982
.... It has medium strength and ductility. Alloy 360 is used for hardware such as gears and pinions where excellent machinability is of prime importance and for all types of automatic high-speed screw-machine products. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1980) 29 (2): Cu-389.
Published: 01 February 1980
... widely for electrical or thermal conductors requiring extensive machining and for screw-machine products requiring a color that matches pure copper. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high...
Journal Articles
Alloy Digest (1980) 29 (12): SS-378.
Published: 01 December 1980
...-magnetic in the annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1980) 29 (12): Al-182.
Published: 01 December 1980
... ALUMINUM 6262 is an alloy with an excellent combination of machinability, strength and resistance to corrosion. Lead and bismuth are added to provide free-machining characteristics. Its many applications include screw-machine products, housewares, marine parts. aerospace fittings and general...
Journal Articles
Alloy Digest (1981) 30 (1): SS-379.
Published: 01 January 1981
... CARPENTER STAINLESS TYPE 303Se is a free-machining modification of the 18% chromium-8% nickel stainless steel. Type 303Se is used for all types of screw-machine products. This alloy is frequently used for machined parts which will be subjected to some cold forming in assembly operations...
Journal Articles
Alloy Digest (1986) 35 (7): Cu-513.
Published: 01 July 1986
... Copper Alloy No. C33200 is a free-machining brass containing nominally 1.6% lead. Its machinability rating is 80% of that of Free-Cutting Brass. It has good resistance to corrosion in many environments. Alloy No. C33200 is used widely for general-purpose screw-machine products. This datasheet...
Journal Articles
Alloy Digest (1974) 23 (7): Cu-281.
Published: 01 July 1974
... COPPER ALLOY No. 544 is a leaded phosphor bronze with a machinability rating of 80% of free-cutting brass. It is suitable for screw machine products and has many uses such as valve parts, shafts, bearings and gears. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2011) 60 (7): Cu-800.
Published: 01 July 2011
... Ansonia alloy C48500 is a highly machinable brass for applications in screw-machine products. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (1994) 43 (7): SA-227.
Published: 01 July 1994
... LEDLOY-AX is a lead and tellurium-bearing steel, having superior free-machining characteristics. It is recommended for screw machine products, fasteners, hardware, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1978) 27 (12): Al-32.
Published: 01 December 1978
... ALUMINUM 2011 is an age-hardenable aluminum-copper alloy to which lead and bismuth are added to make it a free-machining alloy. It has good mechanical properties and was designed primarily for the manufacture of screw-machine products. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1981) 30 (4): SS-385.
Published: 01 April 1981
... applications include-screw-machine products and bar and fountain accessories. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1969) 18 (6): SS-226.
Published: 01 June 1969
... Allegheny 203EZ is a free-machining chromium-nickel-manganese austenitic stainless steel recommended for high-speed automatic screw machine products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1970) 19 (6): Cu-217.
Published: 01 June 1970
... BRUSH alloy M25 is a free-machining beryllium-copper alloy having good response to age-hardening for high strength, hardness, fatigue and corrosion resistance. It is recommended for screw machine products, gears, shafts, hardware, fasteners, connectors, electronic and electrical components...
Journal Articles
Alloy Digest (1970) 19 (12): Cu-223.
Published: 01 December 1970
... parts, screw machine products, and electrical parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-223...
Journal Articles
Alloy Digest (1981) 30 (9): SS-392.
Published: 01 September 1981
... condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...