1-20 of 1463 Search Results for

scaling resistance

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1963) 12 (6): SS-144.
Published: 01 June 1963
... Carpenter No. 1-JR is a low cost oxidation-resistant steel which offers an excellent combination of electrical resistance and scale resistance. It is primarily used as an electrical resistant material, but is also used as a magnetic core material where resistance to oxidation and corrosion...
Journal Articles
Alloy Digest (1995) 44 (9): SS-613.
Published: 01 September 1995
... REMANIT 4509 was developed specially for silencers and exhaust gas purification plants. Due to its composition, this steel exhibits scale resistance up to 950 C and a high degree of corrosion resistance to the gases occurring in the exhaust system. This datasheet provides information...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-496.
Published: 01 January 1996
... Nicrofer 7520 is a high temperature creep resistant nickel-base alloy with good scaling resistance to 2000 deg F (1100 deg C). Many applications are in the aerospace industry. The alloy is sometimes called alloy 75. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1996) 45 (11): Co-102.
Published: 01 November 1996
... Conicro 4023 W is a high-temperature, heat-resistant, cobalt-base alloy with equal contents of nickel and chromium, a high tungsten content, and a controlled lanthanum addition. The alloy has excellent mechanincal properties and scaling resistance to 1150 deg C (2100 deg F). This datasheet...
Journal Articles
Alloy Digest (1992) 41 (7): SS-532.
Published: 01 July 1992
... AVESTA 353 MA is a high-temperature austenitic stainless steel with excellent scaling resistance, creep strength at elevated temperatures, with carburization and nitriding resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2015) 64 (5): SS-1210.
Published: 01 May 2015
... Böhler (or Boehler) T240 Extra is a high temperature creep resistant austenitic steel. Scaling resistance in air up to approximately 750 C (1380 F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep...
Journal Articles
Alloy Digest (1966) 15 (11): SA-204.
Published: 01 November 1966
... HECLA EM, 20 is an iron-nickel-cobalt-chromium austenitic alloy steel having high oxidation and scaling resistance. It is recommended for high temperature service and medium loads up to 2000 F, such as turbine blading, jet engine exhaust stacks and combustion chambers. This datasheet provides...
Journal Articles
Alloy Digest (1961) 10 (12): SS-28.
Published: 01 December 1961
... MULTIMET alloy is cobalt-nickel-chromium-iron austenitic alloy having high oxidation and scaling resistance along with good high-temperature properties. It tends to work harden but does not respond significantly to age-hardening. It is made in a wrought grade (0.08-0.16% carbon) and a casting...
Journal Articles
Alloy Digest (2007) 56 (5): Ni-650.
Published: 01 May 2007
... Boehler L311 VMR is a nickel alloy having high creep and rupture strength up to 760 deg C (1400 deg F) and scaling resistance in air to 850 deg C (1560 deg F). It is used in the aircraft and gas turbine industries as shafts, blades, and discs. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1971) 20 (9): SS-259.
Published: 01 September 1971
... Armco 18 SR is a ferritic stainless steel that provides excellent resistance to high temperature scaling. It is readily welded by conventional methods and is not subject to troublesome embrittlement or loss of corrosion resistance in the heat-affected zones that affect many other straight chromium...
Journal Articles
Alloy Digest (1981) 30 (9): SS-391.
Published: 01 September 1981
... CARPENTER STAINLESS TYPE 443 is a heat-resisting chromium steel which stands up very well under destructive scaling conditions up to 1600 F (871 C). It is not subject to intergranular corrosion as a result of hot working, welding or continuous operation at elevated temperatures. Type 443...
Journal Articles
Alloy Digest (1962) 11 (6): SS-132.
Published: 01 June 1962
... AISI Type 302B is an austenitic chromium nickel stainless steel which has a resistance to scaling at elevated temperatures superior to Type 302. It is used exclusively for parts which are exposed to high temperatures in service. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1972) 21 (4): Ni-171.
Published: 01 April 1972
... UDIMET 75 is a nickel-base high-temperature alloy developed for good resistance to oxidation and scaling to 2000 F. It can be fabricated and welded readily. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also...
Journal Articles
Alloy Digest (1992) 41 (2): SS-139.
Published: 01 February 1992
... CARPENTER 636 is a hardenable stainless steel designed for service up to 1200 F (649 C). It exhibits good resistance to scaling and oxidation in continuous service up to 1400 F (760 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1973) 22 (6): Ni-192.
Published: 01 June 1973
... PYROMET 90 is a precipitation-hardenable nickel-base alloy with high strength at high temperatures. It is highly resistant to oxidation, scaling, heat and corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep...
Journal Articles
Alloy Digest (1975) 24 (4): SS-309.
Published: 01 April 1975
... CRUTEMP 25 is a fully austenitic stainless steel with outstanding resistance to scaling at elevated temperatures. It also has high strength at elevated temperatures and its weldability is excellent. It is used in such applications as automotive emission control systems and gas turbines...
Journal Articles
Alloy Digest (1979) 28 (10): SS-368.
Published: 01 October 1979
... result in grain-boundary carbide ureciuitation. which will result in reduced corrosion-resistance. in such cases; annealing will restore the 0riginaI corrosion resistance. For best results, surfaces must be entirely free of scale and foreign particles. Finished parts should be passivated for 20 to 30...
Journal Articles
Alloy Digest (1961) 10 (12): Ni-6.
Published: 01 December 1961
... NIMONIC 90 is a nickel-base alloy containing high percentages of chromium and cobalt with aluminum and titanium as hardening agents. It has strength at high temperature levels, and is highly resistant to scaling, oxidation, heat and corrosion. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1959) 8 (7): SS-91.
Published: 01 July 1959
...- sistance and scale resistance. It is a ferritic alloy that does not respond to any thermal treaamnt for harden- ing or strengthening. Its maximum temperature for continuous service (scale resistance) is 1600 F. For intermittent service it is good to 18OO F. It has ex- cellent resistance to intergranular...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-392.
Published: 01 March 1980
..., corrosion and scaling-resistant parts, and parts requiring high thermal conductivity. MaIUlfactU~r: Atnpco Metal Division of Ampco-Pittsburgh Corporation Milwaukee, Wisconsin 53201. Castability and Casting Characteristics: Ampcoloy 570 presents no unusual problems in making good castings. Sound, pore-free...