Skip Nav Destination
Close Modal
Search Results for
sand mold castings
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 335 Search Results for
sand mold castings
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (7): Al-323.
Published: 01 July 1992
... quality sand and permanent mold casting. Forms Available: Standard Sizes Available: TIG-l/16, 3/32, l/8,5/32, 3/16: MIG-.030, .035,3/64, l/16 Application: Welding sand and permanent mold castings of 356.0 and A356.0 Producer: AIcoTec Wire Company Traverse City, Michigan 49684 616-941-4111 DOI: 10.31399...
Abstract
View article
PDF
Alloys R-A356.0, ER4010 and R4010 include aluminum-silicon-magnesium Almigweld and Altigweld filler wires with low iron content to weld alloys 356.0 (Alloy Digest Al-223, May 1976) and A356.0 (Alloy Digest Al-258, June 1985). This datasheet provides information on composition and physical properties. It also includes information on joining. Filing Code: Al-323. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (9): Al-326.
Published: 01 September 1992
... Mold Castings) Ailoy R&57.0 includes aluminum-silicon-magnesium-beryllium Altigweid filler wire with a low iron content to weld alloys 357.0 and A357.0. (See Alloy Digest alloys Ai-163 and 238) Composition*, Wt. 0% Element R4011, RA357.0 Silicon 6.5-7.5 Iron 0.20 Copper 0.20 Manganese 0.10 Magnesium...
Abstract
View article
PDF
Alloy R-A357.0 includes aluminum-silicon-magnesium-beryllium Altigweld filler wire with a low iron content to weld alloys 357.0 and A357.0. (See Aluminum A357, Alloy Digest Al-163, February 1967, and Aluminum 357.0, Alloy Digest Al-238, May 1982.) This datasheet provides information on composition and physical properties. It also includes information on joining. Filing Code: Al-326. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (10): Al-327.
Published: 01 October 1992
... ALLOY R-C3550 (AI-Si-Cu-Mg Filler Wire for Sand and Permanent Mold Castings) Alloy R-C3550 (R4009) includes aluminum-silicon-magnesium and copper Almigweld and Altigweld filler wire with low iron content to weld alloys 355.0 and A355.0. (See Alloy Digest alloys Al-l 15 and 243) Composition*, Wt...
Abstract
View article
PDF
Alloy R-C355.0 (R4009) includes aluminum-silicon-magnesium and copper Almigweld and Altigweld filler wire with low iron content to weld alloys 355.0 and A355.0. (See also Aluminum C355, Alloy Digest A1-115, June 1962, and Aluminum C355.0, Alloy Digest Al-243, February 1983.) This datasheet provides information on composition and physical properties. It also includes information on joining. Filing Code: Al-327. Producer or source: AlcoTec Wire Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (8): Mg-11.
Published: 01 August 1954
... shear strength tensile properties Filing Code: Mg-11 Magnesium Alloy AUGUST, 1954 B DATA ON WORLD WIDE METALS AND ALLOYS DOMAL AZ91X (Sand casthq, Permanent mould, and die casting alloy) DOMAL Az9lX is a 9% A& 1% Zn, magnesium die casting alloy. It combines good mechanical proPerties, casting...
Abstract
View article
PDF
DOMAL AZ91Z is a 9% Al, 1% Zn, magnesium die casting alloy. It combines good mechanical properties, casting characteristics and resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, and machining. Filing Code: Mg-11. Producer or source: Dominion Magnesium Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (9): Zn-31.
Published: 01 September 1977
... pmd rn1111 m - DATA ON WORLD WIDE METALS AND ALLOYS -- j Pubbhed bu Jb9-ge-bh-& h Upper Mmti, New Jeney ZA-12 (Zinc-Base Sand and Permanent-Mold Casting Alloy) ZA-12 is a zinc-aluminum-copper foundry alloy recommended for general-purpose castings of high strength at moderate cost. Its properties...
Abstract
View article
PDF
ZA-12 is a zinc-aluminum-copper foundry alloy recommended for general-purpose castings of high strength at moderate cost. Its properties are similar to those of cast iron; however, it was designed for use in nonferrous foundries to compete with cast-iron, bronze, brass and aluminum castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion and wear resistance as well as casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-31. Producer or source: Eastern Alloys Inc.. See also Alloy Digest Zn-49, May 1990.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (7): Al-52.
Published: 01 July 1957
... All Q DIcEsT d -DATA ON WORLD WIDE METALS AND ALLOY! JULY 1957 5 ALCAN 350 (Aluminum Sand and Permanent Mold Pvblirbed by Engineering Alloys Digest, Inc upper Monrclair. New Jersey Casting Alloy) AICAN 350 is a lwe magnesium-aluminum casting a&y having high mechanical properties, excellent machina...
Abstract
View article
PDF
ALCAN 350 is a 10% magnesium-aluminum casting alloy having high mechanical properties, excellent machinability, and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-52. Producer or source: Aluminum Company of Canada Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (5): Al-202.
Published: 01 May 1971
... properties shear strength tensile properties Filing Code: Al-202 ALUMINUM 242.0 Aluminum Alloy MAY 1971 DIGESf d - DATA ON WORLD WIDE METALS AND ALLOYS Psblisbui by JIng+&lgAllopsDigcsc,InC Upper MonrcIaIr, New Jersey ALUMINUM 242.0 (Sand and Permanent-Mold Casting Alloy) ALUMINUM 242.0 is an age...
Abstract
View article
PDF
ALUMINUM 242.0 is an age-hardenable casting alloy that has excellent strength at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as creep and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-202. Producer or source: Aluminum Company of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (6): Al-156.
Published: 01 June 1966
... ALUMINUM B214 is an aluminum sand and permanent mold casting alloy recommended where excellent resistance to corrosion and tarnishing are required. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength. It also...
Abstract
View article
PDF
ALUMINUM B214 is an aluminum sand and permanent mold casting alloy recommended where excellent resistance to corrosion and tarnishing are required. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-156. Producer or source: Aluminum Company of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (2): Al-163.
Published: 01 February 1967
... Aluminum A357 is a high strength, pressure tight sand and permanent mold aluminum casting alloy. It is age-hardenable. It is recommended for cast gear cases, cylinder heads, transmission cases and strong structural castings. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Aluminum A357 is a high strength, pressure tight sand and permanent mold aluminum casting alloy. It is age-hardenable. It is recommended for cast gear cases, cylinder heads, transmission cases and strong structural castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-163. Producer or source: Aluminum Company of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1988) 37 (7): Zn-43.
Published: 01 July 1988
... (201) 677-9161 UNS No. 235630 (Zinc-Base Sand and Permanent-Mold Casting Alloy) UNS No. 235630 is a zinc-aluminumcopper foundry alloy recommended for general-purpose castings of high strength at moderate cost. It was designed for use in nonferrous foundries to compete with cast-iron, bronze, brass...
Abstract
View article
PDF
UNS No. Z35630 is a zinc-aluminum-copper foundry alloy recommended for general-purpose castings of high strength at moderate cost. It was designed for use in nonferrous foundries to compete with cast-iron, bronze, brass and aluminum castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion and wear resistance as well as casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-43. Producer or source: Zinc alloy producers.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (10): Al-229.
Published: 01 October 1977
... BELMONT ALLOY 18910 is a general-purpose aluminum casting alloy containing 2.5% silicon which contributes to good casting characteristics for intricate shapes. Sand and permanent-mold castings comprise its main use. It is used widely for bearings and components of intricate shape. Because of its...
Abstract
View article
PDF
BELMONT ALLOY 18910 is a general-purpose aluminum casting alloy containing 2.5% silicon which contributes to good casting characteristics for intricate shapes. Sand and permanent-mold castings comprise its main use. It is used widely for bearings and components of intricate shape. Because of its anti-scuffing properties, low friction and high resistance to wear under conditions of boundary and thin-film lubrication, it is used extensively for large rolling mill bearings. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-229. Producer or source: Belmont Metals Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1988) 37 (5): Mg-73.
Published: 01 May 1988
... AZ91D and AZ91E alloys are magnesium-aluminum-zinc-manganese alloys of closely controlled purity. Ingot is available for use in the production of improved corrosion resistant sand, permanent-mold and die castings. AZ91D is used for die casting and AZ91E for sand and permanent-mold castings...
Abstract
View article
PDF
AZ91D and AZ91E alloys are magnesium-aluminum-zinc-manganese alloys of closely controlled purity. Ingot is available for use in the production of improved corrosion resistant sand, permanent-mold and die castings. AZ91D is used for die casting and AZ91E for sand and permanent-mold castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-73. Producer or source: The Dow Chemical Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1988) 37 (3): Zn-42.
Published: 01 March 1988
... UNS No. Z35635 is a zinc-aluminum-copper-magnesium foundry alloy recommended for castings of moderate strength and low cost. It was designed for use in nonferrous permanent-mold foundries to compete with cast-iron, aluminum and bronze castings. The alloy can be sand cast and die cast. Its many...
Abstract
View article
PDF
UNS No. Z35635 is a zinc-aluminum-copper-magnesium foundry alloy recommended for castings of moderate strength and low cost. It was designed for use in nonferrous permanent-mold foundries to compete with cast-iron, aluminum and bronze castings. The alloy can be sand cast and die cast. Its many uses include hardware, valves, implement components and equipment for liquid fuel transfer because it is non-sparking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion and wear resistance as well as casting, heat treating, machining, and surface treatment. Filing Code: Zn-42. Producer or source: Zinc alloy producers.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (2): Al-243.
Published: 01 February 1983
... ALUMINUM C355.0 is a high-purity casting alloy that responds to an age-hardening heat treatment. It can be cast successfully by the sand and permanent-mold processes. Its castings characteristics are excellent and it is recommended for pressure-tight castings. It has good resistance to corrosion...
Abstract
View article
PDF
ALUMINUM C355.0 is a high-purity casting alloy that responds to an age-hardening heat treatment. It can be cast successfully by the sand and permanent-mold processes. Its castings characteristics are excellent and it is recommended for pressure-tight castings. It has good resistance to corrosion. Its applications include propeller gear boxes, crankcases and stressed structural parts in aircraft. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-243. Producer or source: Various aluminum companies.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (3): Al-474.
Published: 01 March 2021
... Rio Tinto 319.2 is a heat-treatable, Al-Si-Cu casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. Alloy 319.0 exhibits very good castability and pressure tightness, moderate strength, and good high-temperature...
Abstract
View article
PDF
Rio Tinto 319.2 is a heat-treatable, Al-Si-Cu casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. Alloy 319.0 exhibits very good castability and pressure tightness, moderate strength, and good high-temperature properties. It offers good strength in the as-cast condition and is often used that way. However, it is possible to increase strength considerably by heat treatment. In applications that experience high temperatures, as in engine components, it is common to employ a T5, T7, or O treatment. These treatments tend to stabilize the casting and reduced dimensional changes in the component caused by high temperatures in service. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-474. Producer or source: Rio Tinto Limited.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (8): Al-479.
Published: 01 August 2021
... Rio Tinto 354.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting to be used for the production of sand and permanent mold castings. Alloy 354.0 was developed especially for premium engineered casting...
Abstract
View article
PDF
Rio Tinto 354.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting to be used for the production of sand and permanent mold castings. Alloy 354.0 was developed especially for premium engineered casting applications requiring high strength and elongation, and sound castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting and heat treating. Filing Code: Al-479. Producer or source: Rio Tinto Limited.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (12): Al-220.
Published: 01 December 1975
...-silicon sand mold casting alloy recommended for general applications where good corrosion resistance with moderate strength is required. It cannot be hardened and strengthened by any thermal treatment and is used in the as-cast condition (F temper), sometimes with stress relief. It can be machined readily...
Abstract
View article
PDF
ALUMINUM B514.0 is an aluminum sand casting alloy recommended where excellent resistance to corrosion and tarnishing are required. It has moderate strength and pressure tightness. Cooking utensils and marine applications are among its uses. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength. It also includes information on corrosion resistance as well as casting, heat treating, and joining. Filing Code: Al-220. Producer or source: Various aluminum companies.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (8): Al-228.
Published: 01 August 1977
... BELMONT ALLOY 1918 is a general-purpose aluminum casting alloy that can be sand cast and permanent-mold cast. It is used widely for bearings and is particularly suited for heavy-duty bearings such as those used for diesel engine crankshafts. This datasheet provides information on composition...
Abstract
View article
PDF
BELMONT ALLOY 1918 is a general-purpose aluminum casting alloy that can be sand cast and permanent-mold cast. It is used widely for bearings and is particularly suited for heavy-duty bearings such as those used for diesel engine crankshafts. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fatigue. It also includes information on casting, forming, heat treating, and machining. Filing Code: Al-228. Producer or source: Belmont Metals Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (12): Al-231.
Published: 01 December 1977
... ALUMINUM 413.0 is normally classified as a die-casting alloy; however, it also can be used for sand and permanent-mold castings. Its high silicon content (12%) lowers its melting temperature and increases its fluidity, thus improving its castability. It is used for intricate thin-walled castings...
Abstract
View article
PDF
ALUMINUM 413.0 is normally classified as a die-casting alloy; however, it also can be used for sand and permanent-mold castings. Its high silicon content (12%) lowers its melting temperature and increases its fluidity, thus improving its castability. It is used for intricate thin-walled castings requiring pressure tightness, toughness and good resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-231. Producer or source: Various aluminum companies.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (2): Al-213.
Published: 01 February 1975
... FEDERATED F450 is a heat-treatable sand and permanent-mold aluminum casting alloy with good casting characteristics and pressure tightness. It is recommended for general-purpose castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View article
PDF
FEDERATED F450 is a heat-treatable sand and permanent-mold aluminum casting alloy with good casting characteristics and pressure tightness. It is recommended for general-purpose castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-213. Producer or source: Federated Metals Corporation, ASARCO Inc..