Journal Articles
Alloy Digest (1959) 8 (9): Cu-81.
Published: 01 September 1959
... Revere No. 508 is a highly ductile, malleable and corrosion resistant copper-nickel alloy suitable for condenser and heat exchanger tubes and many engineering applications such as salt water piping aboard ship, many components of salt water and fresh water stills, feed water heater tubes and...
Journal Articles
Alloy Digest (1966) 15 (9): Cu-168.
Published: 01 September 1966
... Copper Alloy 720 is a copper-nickel alloy having high corrosion resistance and retention of strength at moderately elevated temperatures. It is recommended for heat exchangers, salt water piping and relays. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-449.
Published: 01 December 1982
.... Its strength and other mechanical properties are similar to the older copper-nickel alloys (90-10 and 70-30). Alloy C72200 is used primarily for condenser and heat-exchanger tubing using seawater and for salt-water piping. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1985) 34 (9): Cu-500.
Published: 01 September 1985
... uses are springs, switches, heat exchangers, salt-water piping and relays. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining...
Journal Articles
Alloy Digest (1991) 40 (9): TS-32.
Published: 01 September 1991
.../ 12500F[649/6770Ccoolslowlytoroomtemperatureforgreater dimensional accuracy in hardening. Finish machine, then harden. Hardening: Place part in furnace or salt bath at 1550 F (843°C) soak 5 min of thickness, quench in 5 to 10% brine. If endother- mic furnace atmosphere is used, dew point should be 45/50 F...
Journal Articles
Alloy Digest (1966) 15 (4): SS-180.
Published: 01 April 1966
...: After annealing or hear creating, scale removal may be effected by pickling in a 10% by volume water solution of sulfuric acid with l/4 pound of rock salt per gallon of solution at 160.180oF. The steel may be passivaced in a 20% by volume water solution of nitric acid ac 70-1200F. Irmnersion times are...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1195.
Published: 01 January 2015
.... Corrosion Resistance: General Corrosion. Pressurfect has good resistance in: Organic acids at moderate temperatures Salt solutions, e.g., sulfates, sulfides, and sulfites Caustic solutions at moderate temperatures SANDVIK PRESSURFECT (Seamless Pipe and Tubing) Filing Code: SS-1195 Stainless Steel...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-391.
Published: 01 March 1980
... Alloy 706 to increase its resistance to corrosion by salt water. Alloy 706 is recommended where good mechanical properties, weldability and corrosion resistance are needed. It is widely used for plates, tubing and piping that must resist seawater. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1986) 35 (4): Cu-503.
Published: 01 April 1986
... Copper Alloy No. C72800 is a copper-nickel-tin spinodal alloy designed for high strength and excellent resistance to corrosion by salt water. It can be fabricated by the commonly-used processes. Among its many uses are springs, electrical contracts and relay elements, especially in marine...
Journal Articles
Alloy Digest (1971) 20 (4): Cu-231.
Published: 01 April 1971
.... Applications: Condenser tubes and plates, distiller tubes, tube sheets for condensers and heat exchangers, evaporator and heat exchanger tubes, ferrules, salt water piping, distillers tubes, hot water tanks for domestic service, tips for welding torches. Manufacturer: Most copper alloy mills. ...
Journal Articles
Alloy Digest (1969) 18 (4): Al-186.
Published: 01 April 1969
... ALUMINUM 6062 is a magnesium silicide type of wrought aluminum alloy having good mechanical properties combined with high resistance to fresh and salt water corrosion. It responds to age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1981) 30 (3): Cu-414.
Published: 01 March 1981
... processes is fair to good. Forms Available: Billets, bars, rods, shapes, plate, sheet, strip, foil, tube, pipe, wire and forgings. Applications: Copper Alloy No. C46400 is used extensively under Naval specifications as a salt-water marine alloy in shafting, propeller hub cones and all types of preci- sion...
Journal Articles
Alloy Digest (1973) 22 (6): Al-39.
Published: 01 June 1973
... ALUMINUM 5052 is nominally an aluminum-magnesium-chromium alloy which cannot be hardened by heat treatment; however, it can be strain hardened by cold working. It combines good workability with good fatigue strength and high corrosion resistance to the atomsphere and to salt water. This datasheet...
Journal Articles
Alloy Digest (1973) 22 (12): Ni-198.
Published: 01 December 1973
... atmospheres. In alkaline, salt water, fresh water, neutral salts and in air, almost no attack occurs. Data for testing in boiling acids are available from the manufacturer. General Characteristics: Pyromet 102 alloy is a nonmagnetic, nickel-chromium base alloy, solid solution strengthened by the refractory...
Journal Articles
Alloy Digest (1987) 36 (10): CS-115.
Published: 01 October 1987
... 5260 300 - 6-9 812 l&18 14-27 2B30 27-35 Corrosion Resistance: This steel will rust when brought into contact with moisture and air at room temperature. If salts are present. the cosroaion rate is increased. The steel is attacked readily by acids, but is somewhat resistant to alkalis at ordinary...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-455.
Published: 01 March 1983
... neutral salts but is attacked by ammonia, particularly in the presence of air. This alloy, in common with other high-copper brasses, is excellent for its resistance to dezincification and season cracking. Resistance to ptting is particularly good. It is frequently specified for underground service lines...
Journal Articles
Alloy Digest (1994) 43 (9): Ni-463.
Published: 01 September 1994
... neutral and alkaline salts. . Marine Components - pumps, valves, piping, shafts and fixtures used in sea and brackish water. l Petroleum Relining - crude distillation towers, accu- mulator tanks, condensers, isomerization units, hydro- fluoric and sulfuric acid alkylation units, vessels, heat exchangers...
Journal Articles
Alloy Digest (1985) 34 (3): Cu-493.
Published: 01 March 1985
...: General Corrosion Behavior: Copper Alloy No. C61300 has good resistance to corrosion by rural. industrial and marine atmospheres, fresh water and salt water. Soft water tends to be more corrosive than hard water. It also resists non-oxidizing mineral acids such as sulfuric. hydrochloric and phosphoric...
Journal Articles
Alloy Digest (1981) 30 (10): Cu-424.
Published: 01 October 1981
... cold dilute sulfuric acid and by cold concentrated sulfuric acid. It is re- sistant to sodium and potassium bydroxides and to neutral salts but is attacked by ammonia, particularly in the presence of air. The relatively low zinc content (15%) of Mueller aRoy 2300 makes it resistant to dezincification...
Journal Articles
Alloy Digest (1975) 24 (3): Co-41.
Published: 01 March 1975
... behavior for UMCo-50 in combined oxidizine and sulfidizine atmospheres. as well as in combustton products contaminate with sulfur and alkali metal salts. UMCo-50 is not corroded by molten copper. but is rapidly attacked by molten zinc and aluminum. It resists attack by molten ferrous oxide slag and slags...