Journal Articles
Alloy Digest (1990) 39 (3): Ni-380.
Published: 01 March 1990
... ALLVAC 500 ZB is an austenitic precipitation hardening alloy which develops outstanding tensile, fatigue and stress-rupture properties. It is suited to longtime service requirements up to 1800 F (982 C). It is produced by vacuum induction melting plus vacuum arc remelting. This datasheet provides...
Journal Articles
Alloy Digest (1975) 24 (3): SS-307.
Published: 01 March 1975
... Type HP is an iron-chromium-nickel alloy with a combination of elements that makes it resistant to both oxidizing and carburizing atmospheres at high temperatures. The alloy has good creep-rupture properties in the 1800-2000 F temperature range. It has an austenitic structure at all temperatures...
Journal Articles
Alloy Digest (1976) 25 (6): SS-329.
Published: 01 June 1976
... UNITEMP 1420WM is a hardenable 12% chromium stainless steel containing nickel, molybdenum, tungsten and vanadium additions to attain high strength up to 1200 F. Its good creep-rupture properties and resistance to stress-corrosion cracking make this steel well suited for jet engines and many other...
Journal Articles
Alloy Digest (2021) 70 (4): Ni-769.
Published: 01 April 2021
... VDM 601 (Nicrofer 6023 H) is a nickel-chromium-iron alloy with additions of aluminum and titanium. This alloy is specifically recommended for service above 550 °C (1020 °F) because of its superior creep-rupture properties resulting from its controlled carbon content and coarse grain size...
Journal Articles
Alloy Digest (2010) 59 (4): Ni-678.
Published: 01 April 2010
... Electralloy ECHX is a solution-strengthened, nickel-base, high-performance alloy providing excellent resistance to high-temperature gaseous corrosion, coupled with good strength and stress rupture properties up to 1205 deg C (2200 deg F). This datasheet provides information on composition...
Journal Articles
Alloy Digest (1967) 16 (2): Ni-121.
Published: 01 February 1967
... INCONEL alloy 625 is a nickel-base alloy having excellent stress-rupture properties and good oxidation resistance to 1200 F. It is recommended for jet engine components, aerospace applications and chemical processing equipment. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (10): SS-201.
Published: 01 October 1967
... INCOLOY nickel-iron-chromium alloy 801 is a modification of INCOLOY alloy 800. Its nominally 1% titanium content gives it improved tensile and rupture properties. It has excellent oxidation resistance up to 1600-1700 F and can be readily formed and welded. This datasheet provides information...
Journal Articles
Alloy Digest (2006) 55 (7): Ni-640.
Published: 01 July 2006
... Electralloy EC625 is a solution-strengthened, nickel-base, high-performance alloy providing excellent resistance to both high-temperature gaseous corrosion and to aqueous corrosion, coupled with good strength and stress rupture properties up to 982 deg C (1800 deg F). This datasheet provides...
Journal Articles
Alloy Digest (2010) 59 (4): SS-1060.
Published: 01 April 2010
... Kubota alloy HN is an austenitic Fe-Ni-Cr alloy with long-term creep-rupture properties that are intermediate between those of HK40 and HP40 alloys. Carburization resistance is better than that of HK40, but oxidation resistance is generally lower, making the alloy suitable for long service at 1095...
Journal Articles
Alloy Digest (1995) 44 (5): Ni-481.
Published: 01 May 1995
... The Microcast-X process produces a substantially finer grain size that improves mechanical properties in MAR-M-247 with modest negative impact on rupture properties above 1600 F (871 C). This datasheet provides information on composition, microstructureand tensile properties as well as creep...
Journal Articles
Alloy Digest (1995) 44 (6): Ni-482.
Published: 01 June 1995
... The Microcast-X process produces a finer grain size than earlier produced castings which improves mechanical properties in IN-718 without negative impact on rupture properties in temperatures of interest for applications in the aerospace market. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1996) 45 (9): SS-654.
Published: 01 September 1996
... Wiscalloy 25-35Nb is a high-temperature cast heat-resistant stainless steel with good creep-rupture properties. The alloy is centrifugally cast and is often used as petrochemical furnace tubing. This datasheet provides information on composition, physical properties, and tensile properties as well...
Journal Articles
Alloy Digest (1996) 45 (11): SS-656.
Published: 01 November 1996
... Wiscalloy 25-35NB MA is a high-temperature cast heat-resistant microalloyed stainless steel with good creep-rupture properties. The alloy is centrifugally cast and is often used as petrochemical furnace tubing. This datasheet provides information on composition, physical properties, and tensile...
Journal Articles
Alloy Digest (1993) 42 (5): SS-543.
Published: 01 May 1993
... Märker G4859 is a cast austenitic iron-base alloy with good additions of chromium and nickel to develop good stress-rupture properties with good thermal shock resistance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1957) 6 (5): Ti-12.
Published: 01 May 1957
... REM-CRU C-120AV is an alpha-beta titanium-base alloy having good high temperature strength, low temperature impact and notch rupture properties, and good creep resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1980) 29 (7): SS-373.
Published: 01 July 1980
... RA 800H is an austenitic iron-base, heat-resistant alloy with excellent high-temperature strength and good resistance to oxidation in air up to 2000 F (1090 C). High creep-rupture properties are obtained by a solution-anneal treatment followed by a rapid cool; grain size is controlled in the range...
Journal Articles
Alloy Digest (1965) 14 (4): Mo-6.
Published: 01 April 1965
... FANSTEEL 42 Metal is a molybdenum-base alloy recommended for high temperature applications. It has high recrystallization temperature and good stress-rupture properties. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep...
Journal Articles
Alloy Digest (1970) 19 (5): Cu-215.
Published: 01 May 1970
... CDA 710 is a cupro-nickel alloy having high resistance to seawater corrosion and good stress-rupture properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on low...
Journal Articles
Alloy Digest (1970) 19 (11): SS-246.
Published: 01 November 1970
... IN-519 was developed primarily for application as centrifugally cast tubes in steam-hydrocarbon reformer furnaces. It has significantly higher stress-rupture properties than HK-40 (25Cr-20Ni), which is most commonly used for such components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1961) 10 (5): Mo-2.
Published: 01 May 1961
... Climelt Molybdenum-0.5% Ti is a molybdenum alloy having high strength at elevated temperatures, high modulus of elasticity, low coefficient of expansion, and high thermal conductivity. It has exceptionally high rupture properties above 1600 F. This datasheet provides information on composition...